| 单晶Cu纳米加工机理及其热效应的分子动力学模拟 |
| 郭永博;梁迎春;陈明君;卢礼华 |
| 哈尔滨工业大学精密工程研究所; 哈尔滨 150001 |
|
| MOLECULAR DYNAMICS SIMULATIONS OF NANOMACHINING MECHANISM AND THERMAL EFFECTS OF SINGLE CRYSTAL Cu |
| GUO Yongbo; LIANG Yingchun; CHEN Mingjun; LU Lihua |
| Precision Engineering Research Institute; Harbin Institute of Technology; Harbin 150001 |
引用本文:
郭永博 梁迎春 陈明君 卢礼华. 单晶Cu纳米加工机理及其热效应的分子动力学模拟[J]. 金属学报, 2009, 45(10): 1199-1204.
,
,
,
.
MOLECULAR DYNAMICS SIMULATIONS OF NANOMACHINING MECHANISM AND THERMAL EFFECTS OF SINGLE CRYSTAL Cu[J]. Acta Metall Sin, 2009, 45(10): 1199-1204.
| [1] Liang H Y, Ni X G, Wang X X. Acta Metall Sin, 2001; 37: 833
(梁海弋, 倪向贵, 王秀喜. 金属学报, 2001; 37: 833)
[2] Wu H A, Wang X X, Liang H Y, Liu G Y. Acta Metall Sin, 2002; 38: 903
(吴恒安, 王秀喜, 梁海弋, 刘光勇. 金属学报, 2002; 38: 903)
[3] Inamura T, Takezawa N. CIRP Ann, 1992; 41: 121
[4] Fang T H, Weng C I. Nanotechnology, 2000; 11: 148
[5] Kim J D, Moon C H. J Mater Process Technol, 1996; 59: 309
[6] Liang Y C, Guo Y B, Chen M J. Tribology, 2008; 3: 282
(梁迎春, 郭永博, 陈明君. 摩擦学学报, 2008; 3: 282)
[7] Cheng K, Luo X, Ward R. Wear, 2003; 255: 1427
[8] Lin B, Wu H, Yu S Y, Xu Y S. Nanotech Precis Eng, 2004;2: 136
(林滨, 吴辉, 于思远, 徐燕申. 纳米技术与精密工程, 2004; 2: 136)
[9] Guo X G, Guo D M, Kang R K, Jin Z J. J Dalian Univ Technol, 2008; 48: 205
(郭晓光, 郭东明, 康仁科, 金洙吉. 大连理工大学学报, 2008; 48: 205)
[10] Ikawa N, Shimada S, Tanaka H. CIRP Ann, 1991; 40: 551
[11] Shimada S, Ikawa N, Tanaka H, Uchikoshi J. CIRP Ann, 1994; 43: 51
[12] Komanduri R, Chandrasekaran N, Raff L M. Wear, 2000; 242: 60
[13] Pei Q X, Lu C, Fang F Z, Wu H. Comput Mater Sci, 2006; 37: 434
[14] Maekawa K, Itoh A. Wear, 1995; 188: 115
[15] Cheong W C D, Zhang L C. Nanotechnology, 2000; 11: 173
[16] Tersoff J. Phys Rev, 1989; 39B: 5566
[17] Daw M S, Baskes M I. Phys Rev, 1984; 29B: 6443
[18] Ye Y, Biswas R, Morris J R, Bastawros A, Chandra A. Nanotechnology, 2003; 14: 390
[19] Fuente O R, Zimmerman J A, Gonz´alez M A, Figuera J, Hamilton J C, Pai W, Rojo J M. Phys Rev Lett, 2002; 88: 036101 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|