| 稀土Gd掺杂对锆基块体非晶合金玻璃形成能力及力学性能的影响 |
| 孙亚娟; 魏先顺; 黄永江; 沈军 |
| (哈尔滨工业大学材料科学与工程学院; 哈尔滨 150001) |
|
| EFFECT OF Gd ADDITION ON THE GLASS FORMING ABILITY AND MECHANICAL PROPERTIES IN A Zr–BASED BULK AMORPHOUS ALLOY |
| SUN Yajuan; WEI Xianshun; HUANG Yongjiang; SHEN Jun |
| School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001 |
引用本文:
孙亚娟 魏先顺 黄永江 沈 军. 稀土Gd掺杂对锆基块体非晶合金玻璃形成能力及力学性能的影响[J]. 金属学报, 2009, 45(2): 243-248.
.
EFFECT OF Gd ADDITION ON THE GLASS FORMING ABILITY AND MECHANICAL PROPERTIES IN A Zr–BASED BULK AMORPHOUS ALLOY[J]. Acta Metall Sin, 2009, 45(2): 243-248.
| [1] Johnson W L. MRS Bull, 1999; 24: 42
[2] Wang W H, Dong C, Shek C H. Mater Sci Eng, 2004; R44: 45
[3] Telford M. Mater Today, 2004; 7: 36
[4] Ashby M F, Greer A L. Scr Mater, 2006; 54: 321
[5] Peker A, Johnson W L. Appl Phys Lett, 1993; 63: 2342
[6] Inoue A, Zhang T, Nishiyama N, Ohba K, Masumoto T. Mater Trans JIM, 1993; 34: 1234
[7] Inoue A, Zhang T. Mater Trans JIM, 1996; 37: 185
[8] Xing L Q, Ochin P, HarmelinM, Faudot F, Bigot J, Chevalier J P. Mater Sci Eng, 1996; A220: 155
[9] Jiang Q K, Wang X D, Nie X P, Zhang G Q, Ma H, Fecht H J, Bendnarcik J, Franz H, Liu Y G, Cao Q P, Jiang J Z. Acta Mater, 2008; 56: 1785
[10] Gebert A, Eckert J, Sculzt L. Acta Mater, 1998; 46: 5475
[11] Wang W H, Bian Z, Wen P, Zhang Y, Pana M X, Zhao D Q. Intermetallics, 2002; 10: 1249
[12] Yan M, Zou J, Shen J. Acta Mater, 2006; 54: 3627
[13] Iqbal M, Hu Z Q, Zhang H F, Sun W S, Akhter J I. J Non–Cryst Solids, 2006; 352: 3290
[14] Iqbal M, Akhter J I, Zhang H F, Hu Z Q. J Non–Cryst Solids, 2008; 354: 3291
[15] Wang W H. Prog Mater Sci, 2007; 52: 540
[16] Turnbull D. Contemp Phys, 1969; 10: 473
[17] Lu Z P, Liu C T. Phys Rev Lett, 2003; 91: 115505
[18] Fu H M, ang H, Zhang H F, Hu Z Q. Scr Mater, 2006; 55: 147
[19] Sun Y Y, Liu B, Chen Q, Liu L. Acta Metall Sin, 2007; 43: 177
(孙阳阳, 刘 兵, 谌祺, 柳林. 金属学报, 2007; 43: 177)
[20] Ma L Q, Wang L M, Zhang T, Inoue A. Acta Metall Sin, 1999; 35: 631
(马立群, 王立民, 张涛, 井上明久. 金属学报, 1999; 35: 631)
[21] Li R, Pang S J, Ma C L, Zhang T. Acta Mater, 2007; 55: 3719
[22] Poon S J, Shiflet G J, Guo F Q, Ponnambalam V. J Non–Cryst Solids, 2003; 317: 1
[23] Kanibolotsky D S, Lisnyak V V. J Non–Cryst Solids, 2004; 333: 194
[24] Battezzati L, Garrone E. Z Metallkd, 1984; 75: 305
[25] Guo F Q, Poon S J, Shiflet G J. Appl Phys Lett, 2003; 83: 2575
[26] Yang B, Liu C T, Nieh T G. Appl Phys Lett, 2006; 88: 221911
[27] Shen J, Liang W Z, Sun J F. Appl Phys Lett, 2006; 89: 121908
[28] Xi X K, Zhao D Q, Pan M X, Wang W H, Wu Y, Lewandowski J J. Phys Rev Lett, 2005; 94: 125510
[29] Pan D G, Zhang H F, Wang A M, Wang Z G, Hu Z Q. J Alloy Compd, 2007; 438: 145
[30] Wang G, Wang Y T, Liu Y H, Pan M X, Zhao D Q, Wang W H. Appl Phys Lett, 2006; 89: 121909
[31] Zhang Z F, Wu F F, Gao W, Tan J, Wang Z G, Stoica M, Das J, Eckert J, Shen B L, Inoue A. Appl Phys Lett, 2006; 89: 251917
[32] Wang G, Zhao D Q, Bai H Y, Pan M X, Xia A L, Han B S, Xi X K, Wu Y, Wang W H. Phys Rev Lett, 2007; 98: 235501
[33] Zhang Z F, Zhang H, Shen B L, Inoue A, Eckert J. Philos Mag Lett, 2006; 86: 643
[34] Zhang Z F, Wu F F, Fan J T, Zhang H. Sci China, 2008; 38G: 349
(张哲峰, 伍复发, 范吉堂, 张辉.中国科学, 2008; 38G: 349)
[35] Zhang Z F, Wu F F, He G, Eckert J. J Mater Sci Technol, 2007; 23: 747
[36] Donovan P E, Stobbs W M. Acta Metall, 1981; 29: 1419
[37] Spaepen F. Acta Metall, 1977; 25: 407
[38] Argon A S. Acta Metall, 1979; 27: 47
[39] Liu L F, Dai L H, Bai Y L, Wei B C. J Non–Cryst Solids, 2005; 351: 3259
[40] Wright W J, Hufnagel T C, Nix W D. J Appl Phys, 2003; 93: 1432
[41] Meng J X, Ling Z, Jiang M Q, Zhang H S, Dai L H. Appl Phys Lett, 2008; 92: 171909 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|