| Co对Fe--B--Y--Nb块体非晶合金玻璃形成能力及软磁性能的影响 |
| 吴泽宇;郭胜锋;李宁;柳林 |
| (华中科技大学材料科学与工程学院材料成形与模具技术国家重点实验室; 武汉 430074) |
|
| INFLUENCE OF Co ON THE GLASS FORMING ABILITY AND SOFT MAGNETIC PROPERTY OF Fe–B–Y–Nb BULK AMORPHOUS ALLOY |
| WU Zeyu; GUO Shengfeng; LI Ning; LIU Lin |
| State Key Laboratory of Material Processing and Die&Mould Technology; College of Materials Science and Engineering; Huazhong University of Science and Technology; Wuhan 430074 |
引用本文:
吴泽宇 郭胜锋 李宁 柳林. Co对Fe--B--Y--Nb块体非晶合金玻璃形成能力及软磁性能的影响[J]. 金属学报, 2009, 45(2): 249-252.
,
,
,
.
INFLUENCE OF Co ON THE GLASS FORMING ABILITY AND SOFT MAGNETIC PROPERTY OF Fe–B–Y–Nb BULK AMORPHOUS ALLOY[J]. Acta Metall Sin, 2009, 45(2): 249-252.
| [1] Duwez P, Lin S C H. J Appl Phys, 1967; 38: 4096
[2] Inoue A, Shinohara Y, Gook J S. Mater Trans JIM, 1995; 36: 1427
[3] Inoue A, Zhang T, Takeuchi A. Appl Phys Lett, 1997; 71: 464
[4] Inoue A, Zhang W. J Appl Phys, 1999; 85: 4491
[5] Inoue A, Shen B L. Mater Trans JIM, 2002; 43: 766
[6] Shen T D, Schwarza R B. Appl Phys Lett, 1999; 75: 49
[7] Lin C Y, Tien H Y, Chin T S. Appl Phys Lett, 2005; 86: 162501
[8] Hu Y, Pan M X, Liu L, Zhao Y H, Zhao D Q, Wang W H. Mater Lett, 2003; 57: 2698
[9] Kim D H, Park J M, Kim D H, Kim W T. J Mater Res, 2007; 22: 471
[10] Han Z, Zhang J, Li Y. Intermetallics, 2007; 15: 1447
[11] Shen B L, Inoue A, Chang C T. Appl Phys Lett, 2004; 85: 4911
[12] Park J M, Park J S, Kim D H, Kim J H, Fleury E. J Mater Res, 2006; 21: 1019
[13] Li F S, Shen B L, MakinoA, Inoue A. Appl Phys Lett, 2007; 91: 234101
[14] Greer A L. Nature, 1993; 366: 303
[15] Slater J C. J Appl Phys, 1937; 8: 385
[16] Um C Y, McHenry M E. IEEE Trans Magn, 2004; 40: 2724
[17] Egami T. Rep Prog Phys, 1984; 47: 1601
[18] He S L, He K Y, Shen B G, Zhang H W, Zhang S Y, Guo H Q. J Appl Phys, 1999; 86: 6301 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|