蒸发—气体—聚集制备的Co-Ag颗粒膜微观结构与巨磁电阻特性 |
王浩 S.P.Wong |
五邑大学数学物理系; 江门 529020 |
|
引用本文:
王浩; S.P.Wong . 蒸发—气体—聚集制备的Co-Ag颗粒膜微观结构与巨磁电阻特性[J]. 金属学报, 1999, 35(6): 569-572 .
[1]Berkowitz A E, Mitchellj R, Carey M J, Young A P, Zhang S, Spada F E, Parker P T, Hutten A, Thomas G. Phys Rev L:tt,1992; 68:3745 [2]Wang J Q, Xiao G. Phpo Re。,1994; B49: 3982 [3]Gester M, Ounadjela K, Gregg J F.J Magn Magn Mater,1997i 165:323 [4]Zhany W, BordlW, Elliott M.J Mag。Magn Maten 1997 165:330 [5]Haberland H, Insepov Z, Karrals.Mate,Set Eny。1993; B19:31 [6]wang H.J Mate, Set; 1998; 33: 4643 [7]Zhu L B.Physics of Surface and Interface.Tianjin:Tianjin Science Technology Press, 1997: 165,526 (朱履冰.表面与界面物理.天津:天津科学技术出版社,1997: 165,526) [8]Honda S, Okada T, Nawate M.J Mop Magn Mater, 1997;165:326 |
|