铜单晶循环变形饱和阶段疲劳裂纹萌生及表面区域内应力分布的模拟 |
杨继红 张新平 Y. W. Mai 李勇 |
沈阳师范大学物理科学与技术学院; 沈阳110034 |
|
Simulation Of Internal~ Stresses~ Near The Surface And Fatigue Crack Nucleation For A Copper Single Crystal In Cyclic Deformation Saturation Stage |
YANG Jihong; ZHANG Xinping; Y. W. MAI; LI Yong |
College of Physics and Technology; Shenyang Normal University; Shenyang 110034 |
引用本文:
杨继红; 张新平; Y.W.Mai; 李勇 . 铜单晶循环变形饱和阶段疲劳裂纹萌生及表面区域内应力分布的模拟[J]. 金属学报, 2005, 41(1): 9-.
,
,
,
.
Simulation Of Internal~ Stresses~ Near The Surface And Fatigue Crack Nucleation For A Copper Single Crystal In Cyclic Deformation Saturation Stage[J]. Acta Metall Sin, 2005, 41(1): 9-.
[1] Suresh S. Fatigue of Materials. UK, Cambridge: Cambridge University Press, 1998: 132 [2] Miller K J, de Los Rios E R. Short Fatigue Crack. London: European Structural Integrity Society Publication,1992: 55 [3] Zhang X P, Wang C H, Chen W, Ye L, Mai Y W. ScrMater, 2001; 44: 2443 [4] Lukas P, Kunz L. Mater Sci Eng, 2001; A 314: 7 [5] Forsyth P J E. Nature, 1953; 171: 172 [6] Katigirl K, Omura A, Koyanagi K, Awatani J, ShiraishiT, Kaneshiro H. Metall Trans, 1977; 8 A: 1769 [7] Basinski Z S, Pascual R, Basinski S J. Ada Metall, 1983;31: 591 [8] Hunsche A, Neumann P. Acta Metall, 1986; 34: 207 [9] Ma B T, Laird C. Acta Metall, 1989; 37: 325 [10] Antonopoulos J G, Brown L M, Winter A T. Philos Mag,1976; 34: 549 [11] Essmann U, Gosele U, Mughrabi H. Philos Mag, 1981; 44A: 405 [12] Tanaka K, Mura T. J Appl Mech, 1981; 48: 97 [13] Sauzay M, Gilormini P. Fati Frac Eng Mater Struct, 2000;23: 573 [14] Repetto E A, Ortiz M. Acta Mater, 1997; 45: 2577 [15] Yang J H, Li Y, Li S X, Ma C X, Li G Y. Mater Sci Eng,2001; 299 A: 51 [16] Yang J H, Li Y, Cai Z, Li S X, Ma C X, Han E H, Ke W.Mater Sci Eng, 2003; 345 A: 164 [17] Li S X, Li Y, Li G Y, Yang J H. Philos Mag, 2002; 82A:867 [18] Yang S H. Principle of Dislocation Theory in Crystals. 2nd ed, Beijing: Science Press, 1998: 81(杨顺华.晶体位错理论基础(第一卷).第2版,北京:科学出版社,1998:81) [19] Mughrabi H. Mater Sci Eng, 2001; 309-310 A: 237 [20] Holzwarth U, Essmann U. Appl Phys, 1993; 57 A: 1319 |
|