| 小尺度材料的疲劳研究进展 |
| 张广平 王中光 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳110016 |
|
| Progress in Fatigue of Small Dimensional Materials |
| ZHANG Guangping; WANG Zhongguang |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The Chinese |
引用本文:
张广平; 王中光 . 小尺度材料的疲劳研究进展[J]. 金属学报, 2005, 41(1): 1-8 .
,
.
Progress in Fatigue of Small Dimensional Materials[J]. Acta Metall Sin, 2005, 41(1): 1-8 .
[1] Menz W, Mohr J, Paul O. Microsystem Technology. Wein-heim: WILEY-VCH, 2001: 1 [2] Spearing S M. Acta Mater, 2000; 48: 179 [3] Ohring M. Reliability and Failure of Electronic Materialsand Devices. Academic Press, 1998: 4 [4] Nix W D. Metall Trans, 1989; 20A: 2217 [5] Arzt E. Acta Mater, 1998; 46: 5611 [6] Keller R M, Baker S P, Arzt E. J Mater Res, 1998; 13:1307 [7] Hommel M, Kraft O. Acta Mater, 2001; 49: 3935 [8]Suresh S,Translated by Wang Z G.Fatigue of Materials. Beijing:National Defense Industry Press,1999:37 (Suresh S著,王中光译.材料的疲劳(第二版).北京:国防 工业出版社,1999:37) [9] Grosskreutz J C, Mughrabi H. In: Argon A S ed, Constitutive Equations in Plasticity Cambridge, MA: The MIT Press, 1975: 251 [10] Sharpe Jr W N, Yuan B, Edwards R L. J Microelec-tromechan Syst, 1997; 6: 193 [11] Tsuchiya T, Tabata O, Sakata J, Taga Y. In: Proceedings of IEEE Tenth Annual International Workshop on Micro Electro Mechanical Systems. 1997: 529 [12] Kapels H, Aigner R, Binder J. IEEE Trans Electron Devices, 2000; 47: 1522 [13] Judelewicz M. Scr Metall Mater, 1993; 29: 1463 [14] Hommel M, Kraft O, Arzt E. J Mater Res, 1999; 14: 2373 [15] Brown S B, van Arsdell W, Muhlstein C L. In: Transducers-97: Int Conf on Solid State Sensors and Actuators, Chicage, Illinois: Digest of Technical Papers, 1997: 591 [16] Kahn H, Ballarini R, Mullen R L, Heuer A H. Proc RoyalSoc London, 1999; 455: 3807 [17] Schwaiger R, Kraft O. Scr Mater, 1999; 41: 823 [18] Takashima K, Maekawa S, Shimojo M, Higo Y, SugiuraS, Pfister B, Swain M V. In: Wu X R, Wang Z G eds,Proceedings of the 7th International Fatigue Congress,Cradley Heath, UK: High Education Press, 1999; 3: 1871 [19] Zhang G P, Takashima K, Shimojo M, Higo Y. Mater Lett,2003; 57(1): 1555 [20] Connally J A, Brown S B. Exp Mechan, 1992; 32: 81 [21] Muhlstein C L, Stach E A, Ritchie R O. Appl Phy Lett,2002; 80: 1532 [22] Muhlstein C L, Brown H B, Ritchie R O. Sens Actuators,2001; 94: 177 [23] Allameh S M, Gaily B, Brown S, Soboyejo W O. ASTMSTP 1413, West Conshohocken, 2000 [24] Hofbeck R, Hausmann K, Ilschner B, Kuenzi H U. ScrMetall, 1986; 20: 1601 [25] Judelewicz M, Kunzi H U, Merk N, Ilschner B. Mater SciEng, 1994; A186: 135 [26] Hong S, Weil R. Thin Solid Films, 1996; 283: 175 [27] Read D T. Int J Fatigue, 1998; 20: 203 [28] Merchant H D, Minor M G, Liu Y L. J Electron Mater,1999; 28: 998 [29] Hadrboletz A, Kathibi G, Weiss B, Stickler R. In: Wu XR, Wang Z G eds, Proceedings of the 7th InternationalFatigue Congress, Cradley Heath, UK: High EducationPress, 1999: 1865 [30] Schwaiger R, Dehm G, Kraft O. Philos Mag, 2003; 83: 693 [31] Kraft O, Schwaiger R, Wellner P. Mater Sci Eng, 2001; A319-321: 919 [32] Kraft O, Wellner P, Hommel M, Schwaiger R, Arzt E. ZMetallkd, 2002; 93(5): 392 [33] Schwaiger R, Kraft O. Acta Mater, 2003; 51(1): 195 [34] Zhang G P, Schwaiger R, Volkert C A, Kraft O. PhilosMag Lett, 2003; 83: 477 [35] Maekawa S, Takashima K, Shimojo M, Higo Y. Jpn J ApplPhys, 1999; 38: 7194 [36] Takashima K, Higo Y, Sugiura S, Shimojo M. MaterTrans, 2001; 42: 68 [37] Zhang G P, Volkert C A, Schwaiger R, Arzt E, Kraft O.Accepted by J Mater Res, 2005; 20(1): 201 [38] Zhang G P, Takashima K, Higo Y. Acta Metall Sin , inpress(张广平,高岛和希,肥後失吉.金属学报,待发表) [39] Mughrabi M, Wang R, Differt K, Essmann U. ASTM STP811, 1983: 5 [40] Zhang G P, Volkert C A, Schwaiger R, Wellner P, Arzt E,Kraft O. to be published [41] Freund L B. J Appl Mech, 1987; 54: 553 [42] Thiele E, Holste C, Klemm R. Z Metallkd, 2002; 93: 730 [43] Tang M J, Xu J S, Cai W, Bulatov V. Mater Res SocSymp Proc, 2003; 795: U2.4.1 [44] Gao H, Huang Y, Nix W D, Hutchinson J W. J Mech PhysSolids, 2000; 48: 99. [45] Hwang K C, Jiang H, Huang Y, Gao H, Hu N. J MechPhys Solids, 2002; 50: 81. [46] Chen S H, Wang Z Q. Adv Mech, 2003; 33: 407(陈少华,王自强.力学进展, 2003;33:407) [47] Stoken J S, Evans A G. Acta Mater, 1998; 46: 5109 [48] Liu Y, Ngan A H W. Scr Mater, 2001; 44: 237 [49] Ashby M F. Philos Mag, 1970; 21: 399 [50] Zhang G P, Moenig R, Park Y B, Arzt E, Volkert C A. tobe published, 2005 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|