| 固溶时效对激光沉积修复ZM6合金组织及力学性能的影响 |
钦兰云1, 张健1, 伊俊振2,3( ), 崔岩峰4, 杨光1( ), 王超3 |
1 沈阳航空航天大学 机电工程学院 沈阳 110136 2 沈阳航空航天大学 材料科学与工程学院 沈阳 110136 3 沈阳航空航天大学 航空制造工艺数字化国防重点学科实验室 沈阳 110136 4 中国航发哈尔滨东安发动机有限公司 哈尔滨 150066 |
|
| Effects of Solution Aging on Microstructural Evolution and Mechanical Properties of Laser Deposition Repairing ZM6 Alloy |
QIN Lanyun1, ZHANG Jian1, YI Junzhen2,3( ), CUI Yanfeng4, YANG Guang1( ), WANG Chao3 |
1 School of Mechatronics Engineering, Shenyang Aerospace University, Shenyang 110136, China 2 School of Materials Science and Engineering, Shenyang Aerospace University, Shenyang 110136, China 3 Key Laboratory of Fundamental Science for National Defense of Aeronautical Digital Manufacturing Process, Shenyang Aerospace University, Shenyang 110136, China 4 AECC Harbin Dongan Engine Co. Ltd., Harbin 150066, China |
引用本文:
钦兰云, 张健, 伊俊振, 崔岩峰, 杨光, 王超. 固溶时效对激光沉积修复ZM6合金组织及力学性能的影响[J]. 金属学报, 2025, 61(6): 875-886.
Lanyun QIN,
Jian ZHANG,
Junzhen YI,
Yanfeng CUI,
Guang YANG,
Chao WANG.
Effects of Solution Aging on Microstructural Evolution and Mechanical Properties of Laser Deposition Repairing ZM6 Alloy[J]. Acta Metall Sin, 2025, 61(6): 875-886.
| 1 |
Song J F, She J, Chen D L, et al. Latest research advances on magnesium and magnesium alloys worldwide [J]. J. Magnes. Alloy., 2020, 8: 1
|
| 2 |
Xu T C, Yang Y, Peng X D, et al. Overview of advancement and development trend on magnesium alloy [J]. J. Magnes. Alloy., 2019, 7: 536
doi: 10.1016/j.jma.2019.08.001
|
| 3 |
Yang Y, Xiong X M, Chen J, et al. Research advances in magnesium and magnesium alloys worldwide in 2020 [J]. J. Magnes. Alloy., 2021, 9: 705
doi: 10.1016/j.jma.2021.04.001
|
| 4 |
Song B, Zhang J L, Zhang Y J, et al. Research progress of materials design for metal laser additive manufacturing [J]. Acta Metall. Sin., 2023, 59: 1
doi: 10.11900/0412.1961.2022.00026
|
| 4 |
宋 波, 张金良, 章媛洁 等. 金属激光增材制造材料设计研究进展 [J]. 金属学报, 2023, 59: 1
|
| 5 |
Wu G H, Wang C L, Sun M, et al. Recent developments and applications on high-performance cast magnesium rare-earth alloys [J]. J. Magnes. Alloy., 2021, 9: 1
|
| 6 |
Tang W N, Mo N, Hou J, et al. Research progress of additively manufactured magnesium alloys: A review [J]. Acta Metall. Sin., 2023, 59: 205
doi: 10.11900/0412.1961.2022.00063
|
| 6 |
唐伟能, 莫 宁, 侯 娟. 增材制造镁合金技术现状与研究进展 [J]. 金属学报, 2023, 59: 205
doi: 10.11900/0412.1961.2022.00063
|
| 7 |
Cheng B, Mao C, Zhang M J, et al. Comparative study on microstructure and properties of laser welding and argon arc welding Hastelloy C-276/SS304 with filler wire [J]. Opt. Laser Technol., 2023, 164: 109565
|
| 8 |
Ci S W, Liang J J, Li J G, et al. Microstructure and tensile properties of DD32 single crystal Ni-base superalloy repaired by laser metal forming [J]. J. Mater. Sci. Technol., 2020, 45: 23
doi: 10.1016/j.jmst.2020.01.003
|
| 9 |
Lin X, Cao Y Q, Wu X Y, et al. Microstructure and mechanical properties of laser forming repaired 17-4PH stainless steel [J]. Mater. Sci. Eng., 2012, A553: 80
|
| 10 |
Smail B S, Cailloux T, Quinsat Y, et al. Integrated approach to stainless steel 316L parts repair for pitting corrosion using laser metal deposition [J]. J. Manuf. Processes, 2023, 95: 1
|
| 11 |
Yan W G, Zeng W, Man J X, et al. Microstructure and mechanical properties of a directionally solidified superalloy DZ411 plate sample repaired by laser melting deposition [J]. Mater. Sci. Eng., 2023, A876: 145141
|
| 12 |
Wang Z D, Yang K, Chen M Z, et al. Investigation of the microstructure and mechanical properties of Ti-6Al-4V repaired by the powder-blown underwater directed energy deposition technique [J]. Mater. Sci. Eng., 2022, A831: 142
|
| 13 |
Qin L Y, Pang S, Yang G, et al. Microstructure and micro-hardness of laser deposition repair ZL114A aluminum alloy [J]. Infrared Laser Eng., 2017, 46: 0506004
|
| 13 |
钦兰云, 庞 爽, 杨 光 等. 激光沉积修复ZL114A铝合金的显微组织及显微硬度研究 [J]. 红外与激光工程, 2017, 46: 0506004
|
| 14 |
Peng L M, Deng Q C, Wu Y J, et al. Additive manufacturing of magnesium alloys by selective laser melting technology: A review [J]. Acta Metall. Sin., 2023, 59: 31
doi: 10.11900/0412.1961.2022.00166
|
| 14 |
彭立明, 邓庆琛, 吴玉娟 等. 镁合金选区激光熔化增材制造技术研究现状与展望 [J]. 金属学报, 2023, 59: 31
doi: 10.11900/0412.1961.2022.00166
|
| 15 |
Dai J, Huang J, Li M, et al. Effects of heat treatments on laser welded Mg-rare earth alloy NZ30K [J]. Mater. Sci. Eng., 2011, A529: 401
|
| 16 |
Singh K. Effect of post-welding heat treatment on mechanical and microstructural properties of friction stir welded dissimilar magnesium alloys [J]. Mater. Today Proc., 2023, doi: 10.1016/j.matpr.2023.02.133
|
| 17 |
Tong X, Zhang G, Wu G H, et al. Addressing the abnormal grain coarsening during post-weld heat treatment of TIG repair welded joint of sand-cast Mg-Y-RE-Zr alloy [J]. Mater. Charact., 2021, 176: 111125
|
| 18 |
Zhang G Q, Tong X, Wu G H, et al. Research on the post-weld heat treatment of TIG repair welded joint of sand-cast Mg-Y-RE-Zr alloy [J]. Mater. Sci. Eng., 2021, A821: 141577
|
| 19 |
Yang G, Zhang W Q, Zhang J, et al. Evolution of microstructure of WE43 magnesium alloys fabricated by laser deposition manufacturing with subsequent friction stir processing [J]. Mater. Lett., 2023, 330: 133218
|
| 20 |
Jiao X Y, Li X J, Zhan L Q, et al. The Microstructural evolution and grain growth kinetics of fine-grained extruded Mg-Nd-Zn-Zr alloy [J]. Materials (Basel), 2022, 15: 3556
|
| 21 |
Ning Z L, Cao F Y, Liu H H, et al. Microstructure analysis of Mg-2.54Nd-0.26Zn-0.32Zr alloy [J]. Rare. Met. Mater. Eng., 2009, 38: 1997
|
| 21 |
宁志良, 曹福洋, 刘洪汇 等. Mg-2.54Nd-0.26Zn-0.32Zr合金组织分析 [J]. 稀有金属材料与工程, 2009, 38: 1997
|
| 22 |
Ning Z L, Liu H H, Cao F Y, et al. The effect of grain size on the tensile and creep properties of Mg-2.6Nd-0.35Zn-xZr alloys at 250 °C [J]. Mater. Sci. Eng., 2013, A560: 163
|
| 23 |
Gao M, Wang H K, Hao K D, et al. Evolutions in microstructure and mechanical properties of laser lap welded AZ31 magnesium alloy via beam oscillation [J]. J. Manuf. Processes, 2019, 45: 92
|
| 24 |
Lei Z L, Bi J, Li P, et al. Analysis on welding characteristics of ultrasonic assisted laser welding of AZ31B magnesium alloy [J]. Opt. Laser Technol., 2018, 105: 15
|
| 25 |
Harooni M, Carlson B, Strohmeier B R, et al. Pore formation mechanism and its mitigation in laser welding of AZ31B magnesium alloy in lap joint configuration [J]. Mater. Des., 2014, 58: 265
|
| 26 |
Fu P H, Peng L M, Jiang H Yet al. Effects of heat treatments on the microstructures and mechanical properties of Mg-3Nd-0.2Zn-0.4Zr (wt.%) alloy [J]. Mater. Sci. Eng., 2008, A486: 183
|
| 27 |
Chen R N, Chen Q H, Peng P, et al. Abnormal grain growth induced by <1120> orientation of AZ31 magnesium alloy [J]. Mater. Sci. Technol., 2023, 39: 1337
|
| 28 |
Pei R S, Korte-Kerzel S, Al-Samman T. Normal and abnormal grain growth in magnesium: Experimental observations and simulations [J]. J. Mater. Sci. Technol., 2020, 50: 257
doi: 10.1016/j.jmst.2020.01.014
|
| 29 |
Tang J W, Chen L, Li Z G, et al. Formation of abnormal coarse grains and its effects on corrosion behaviors of solution treated ZK60 Mg alloy [J]. Corros. Sci., 2021, 180: 109201
|
| 30 |
Kim H J, Jin S C, Jung J G, et al. Influence of undissolved second-phase particles on dynamic recrystallization behavior of Mg-7Sn-1Al-1Zn alloy during low- and high-temperature extrusions [J]. J. Mater. Sci. Technol., 2021, 71: 87
doi: 10.1016/j.jmst.2020.08.056
|
| 31 |
Lezaack M B, Simar A. Avoiding abnormal grain growth in thick 7XXX aluminium alloy friction stir welds during T6 post heat treatments [J]. Mater. Sci. Eng., 2021, A807: 140901
|
| 32 |
Zheng D D, Li Z, Jiang Y L, et al. Effect of multiple thermal cycles on the microstructure evolution of GA151K alloy fabricated by laser-directed energy deposition [J]. Addit. Manuf., 2022, 57: 102957
|
| 33 |
Qin L Y, Pang S, Yang G, et al. Microstructure and mechanical property analysis of ZL114A aluminum alloy repaired by laser deposition [J]. Infrared Laser Eng., 2016, 43: 108
|
| 33 |
钦兰云, 庞 爽, 杨 光 等. 激光沉积修复ZL114A铝合金组织和力学性能分析 [J]. 中国激光, 2016, 43: 108
|
| 34 |
Zheng R X, Du J P, Gao S, et al. Transition of dominant deformation mode in bulk polycrystalline pure Mg by ultra-grain refinement down to sub-micrometer [J]. Acta Mater., 2020, 198: 35
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|