| 热轧变形量对高钛耐磨钢组织与力学性能的影响 |
许帅1, 孙新军1( ), 梁小凯1, 刘俊2, 雍岐龙1 |
1 钢铁研究总院工程用钢研究所 北京 100081 2 江阴兴澄特种钢铁有限公司 江阴 214400 |
|
| Effect of Hot Rolling Deformation on Microstructure and Mechanical Properties of a High-Ti Wear-Resistant Steel |
XU Shuai1, SUN Xinjun1( ), LIANG Xiaokai1, LIU Jun2, YONG Qilong1 |
1 Department of Structural Steels, Central Iron & Steel Research Institute, Beijing 100081, China 2 Jiangyin Xingcheng Special Steel Co., Ltd., Jiangyin 214400, China |
引用本文:
许帅, 孙新军, 梁小凯, 刘俊, 雍岐龙. 热轧变形量对高钛耐磨钢组织与力学性能的影响[J]. 金属学报, 2020, 56(12): 1581-1591.
Shuai XU,
Xinjun SUN,
Xiaokai LIANG,
Jun LIU,
Qilong YONG.
Effect of Hot Rolling Deformation on Microstructure and Mechanical Properties of a High-Ti Wear-Resistant Steel[J]. Acta Metall Sin, 2020, 56(12): 1581-1591.
| [1] |
Deng X T, Wang Z D, Han Y, et al. Microstructure and abrasive wear behavior of medium carbon low alloy martensitic abrasion resistant steel [J]. J. Iron Steel Res. Int., 2014, 21: 98
doi: 10.1016/S1006-706X(14)60015-7
|
| [2] |
Zhang K, Yong Q L, Sun X J, et al. Effect of tempering temperature on microstructure and mechanical properties of high Ti microalloyed directly quenched high strength steel [J]. Acta Metall. Sin., 2014, 50: 913
|
| [2] |
(张 可, 雍岐龙, 孙新军等. 回火温度对高Ti微合金直接淬火高强钢组织及性能的影响 [J]. 金属学报, 2014, 50: 913)
|
| [3] |
Lindroos M, Valtonen K, Kemppainen A, et al. Wear behavior and work hardening of high strength steels in high stress abrasion [J]. Wear, 2015, 322-323: 32
doi: 10.1016/j.wear.2014.10.018
|
| [4] |
Bressan J D, Daros D P, Sokolowski A, et al. Influence of hardness on the wear resistance of 17-4 PH stainless steel evaluated by the pin-on-disc testing [J]. J. Mater. Process. Technol., 2008, 205: 353
doi: 10.1016/j.jmatprotec.2007.11.251
|
| [5] |
Ojala N, Valtonen K, Heino V, et al. Effects of composition and microstructure on the abrasive wear performance of quenched wear resistant steels [J]. Wear, 2014, 317: 225
doi: 10.1016/j.wear.2014.06.003
|
| [6] |
Srivastava A K, Das K. Microstructure and abrasive wear study of (Ti,W)C-reinforced high-manganese austenitic steel matrix composite [J]. Mater. Lett., 2008, 62: 3947
doi: 10.1016/j.matlet.2008.05.049
|
| [7] |
Ni Z F, Sun Y S, Xue F, et al. Evaluation of electroslag remelting in TiC particle reinforced 304 stainless steel [J]. Mater. Sci. Eng., 2011, A528: 5664
|
| [8] |
Xu L J, Xing J D, Wei S Z, et al. Study on relative wear resistance and wear stability of high-speed steel with high vanadium content [J]. Wear, 2007, 262: 253
doi: 10.1016/j.wear.2006.05.016
|
| [9] |
Liu L J. TiC precipitation behavior and its effect on properties in high titanium and high wear-resistant steels [D]. Beijing: Central Iron & Steel Research Institute, 2019
|
| [9] |
(刘罗锦. 高钛高耐磨钢中TiC析出行为及对性能的影响 [D]. 北京: 钢铁研究总院, 2019)
|
| [10] |
Sun X J, Liu L J, Liang X K, et al. TiC precipitation behavior and its effect on abrasion resistance of high titanium wear-resistant steel [J]. Acta Metall. Sin., 2020, 56: 661
|
| [10] |
(孙新军, 刘罗锦, 梁小凯等. 高钛耐磨钢中TiC析出行为及其对耐磨粒磨损性能的影响 [J]. 金属学报, 2020, 56: 661)
|
| [11] |
Liu L J, Liang X K, Liu J, et al. Precipitation process of TiC in low alloy martensitic steel and its effect on wear resistance [J]. ISIJ Int., 2020, 60: 168
doi: 10.2355/isijinternational.ISIJINT-2019-151
|
| [12] |
Jang J H, Lee C H, Heo Y U, et al. Stability of (Ti, M)C (M=Nb, V, Mo and W) carbide in steels using first-principles calculations [J]. Acta Mater., 2012, 60: 208
doi: 10.1016/j.actamat.2011.09.051
|
| [13] |
Yu H L. Evolution behavior of cracks and inclusions in slab during rolling [D]. Shenyang: Northeastern University, 2008
|
| [13] |
(喻海良. 轧制过程中轧件裂纹和夹杂物演变行为研究 [D]. 沈阳: 东北大学, 2008)
|
| [14] |
Weng Y Q. Ultra-Fine Grained Steels [M]. Beijing: Metallurgical Industry Press, 2003: 1
|
| [14] |
(翁宇庆. 超细晶钢 [M]. 北京: 冶金工业出版社, 2003: 1)
|
| [15] |
Liang X K, Sun X J, Yong Q L, et al. Precipitation of TiC in high Ti steel [J]. J. Iron Steel Res., 2016, 28(9): 71
|
| [15] |
(梁小凯, 孙新军, 雍岐龙等. 高钛钢中TiC析出机制 [J]. 钢铁研究学报, 2016, 28(9): 71)
|
| [16] |
Yong Q L. Secondary Phases in Steels [M]. Beijing: Metallurgical Industry Press, 2006: 1
|
| [16] |
(雍岐龙. 钢铁材料中的第二相 [M]. 北京: 冶金工业出版社, 2006: 1)
|
| [17] |
Gladman T. Precipitation hardening in metals [J]. Mater. Sci. Technol., 1999, 15: 30
doi: 10.1179/026708399773002782
|
| [18] |
Cooman B C, Speer J G. Strengthening Mechanisms [M]. Warrendale: Fundamentals of Steel Product Metallurgy, 2011: 270
|
| [19] |
Kennett S C, Krauss G, Findley K O. Prior austenite grain size and tempering effects on the dislocation density of low-C Nb-Ti microalloyed lath martensite [J]. Scr. Mater., 2015, 107: 123
doi: 10.1016/j.scriptamat.2015.05.036
|
| [20] |
Klemm-Toole J, Benz J, Thompson S W, et al. A quantitative evaluation of microalloy precipitation strengthening in martensite and bainite [J]. Mater. Sci. Eng., 2019, A763: 138145
|
| [21] |
Akbary F H, Sietsma J, Böttger A J, et al. An improved X-ray diffraction analysis method to characterize dislocation density in lath martensitic structures [J]. Mater. Sci. Eng., 2015, A639: 208
|
| [22] |
Morito S, Nishikawa J, Maki T. Dislocation density within lath martensite in Fe-C and Fe-Ni alloys [J]. ISIJ Int., 2003, 43: 1475
doi: 10.2355/isijinternational.43.1475
|
| [23] |
Kehoe M, Kelly P M. The role of carbon in the strength of ferrous martensite [J]. Scr. Metall., 1970, 4: 473
doi: 10.1016/0036-9748(70)90088-8
|
| [24] |
Kobayashi Y, Takahashi J, Kawakami K. Experimental evaluation of the particle size dependence of the dislocation-particle interaction force in TiC-precipitation-strengthened steel [J]. Scr. Mater., 2012, 67: 854
doi: 10.1016/j.scriptamat.2012.08.005
|
| [25] |
Petch N J. The cleavage strength of polycrystals [J]. J. Iron Steel Inst., 1953, 174: 25
|
| [26] |
Petch N J. The ductile-brittle transition in the fracture of α-iron: I [J]. Philos. Mag., 1958, 34: 1089
|
| [27] |
Wang C F. Study on structure control unit of strength and toughness of low alloy martensitic steel [D]. Beijing: Central Iron & Steel Research Institute, 2008
|
| [27] |
(王春芳. 低合金马氏体钢强韧性组织控制单元的研究 [D]. 北京: 钢铁研究总院, 2008)
|
| [28] |
Kocks U F. Superposition of alloy hardening, hardening strain, and dynamic recovery [A]. Proc. 5th Int. Conf. Strength of Metals and Alloys [C]. Oxford: Peramon Press, 1979: 1661
|
| [29] |
Ashby M F. The deformation of plastically non-homogeneous materials [J]. Philos. Mag., 1970, 21: 399
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|