| 31%B4Cp/6061Al复合材料的热变形及加工图的研究 |
周丽1, 李明1, 王全兆2( ), 崔超3, 肖伯律2, 马宗义2 |
1 烟台大学机电汽车工程学院 烟台 264005 2 中国科学院金属研究所沈阳材料科学国家研究中心 沈阳 110016 3 哈尔滨工业大学(威海)材料科学与工程学院 威海 264209 |
|
| Study of the Hot Deformation and Processing Map of 31%B4Cp/6061Al Composites |
ZHOU Li1, LI Ming1, WANG Quanzhao2( ), CUI Chao3, XIAO Bolv2, MA Zongyi2 |
1 School of Electromechanical and Vehicle Engineering, Yantai University, Yantai 264005, China 2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 3 School of Materials Science and Engineering, Harbin Institute of Technology Weihai, Weihai 264209, China |
引用本文:
周丽, 李明, 王全兆, 崔超, 肖伯律, 马宗义. 31%B4Cp/6061Al复合材料的热变形及加工图的研究[J]. 金属学报, 2020, 56(8): 1155-1164.
Li ZHOU,
Ming LI,
Quanzhao WANG,
Chao CUI,
Bolv XIAO,
Zongyi MA.
Study of the Hot Deformation and Processing Map of 31%B4Cp/6061Al Composites[J]. Acta Metall Sin, 2020, 56(8): 1155-1164.
| [1] |
Liu B, Huang W M, Huang L, et al. Size-dependent compression deformation behaviors of high particle content B4C/Al composites [J]. Mater. Sci. Eng., 2012, A534: 530
|
| [2] |
Bie B X, Huang J Y, Su B, et al. Dynamic tensile deformation and damage of B4C-reinforced Al composites: Time-resolved imaging with synchrotron X-rays [J]. Mater. Sci. Eng., 2016, A664: 86
|
| [3] |
Zhou L, Zhang P F, Wang Q Z, et al. Multi-scale study on the fracture behavior of hot compression B4C/6061Al composite [J]. Acta Metall. Sin., 2019, 55: 911
doi: 10.11900/0412.1961.2018.00453
|
| [3] |
(周 丽, 张鹏飞, 王全兆等. B4C/6061Al复合材料热压缩断裂行为的多尺度研究 [J]. 金属学报, 2019, 55: 911)
doi: 10.11900/0412.1961.2018.00453
|
| [4] |
Xiao B L, Huang Z Y, Ma K, et al. Research on hot deformation behaviors of discontinuously reinforced aluminum composites [J]. Acta Metall. Sin., 2019, 55: 59
doi: 10.11900/0412.1961.2018.00461
|
| [4] |
(肖伯律, 黄治冶, 马 凯等. 非连续增强铝基复合材料的热变形行为研究进展 [J]. 金属学报, 2019, 55: 59)
doi: 10.11900/0412.1961.2018.00461
|
| [5] |
Shi W C, Shan D B. Effect of whisker breakage on the forgeability and the tensile properties of the forged 2024Al/Al18B4O33w composite [J]. Mater. Charact., 2018, 135: 303
|
| [6] |
El-Sabbagh A M, Soliman M, Taha M A, et al. Effect of rolling and heat treatment on tensile behaviour of wrought Al-SiCp composites prepared by stir-casting [J]. J. Mater. Process. Technol., 2013, 213: 1669
|
| [7] |
Raj R. Development of a processing map for use in warm-forming and hot-forming processes [J]. Metall. Trans., 1981, 12A: 1089
|
| [8] |
Rajamuthamilselvan M, Ramanathan S, Karthikeyan R. Processing map for hot working of SiCp/7075 Al composites [J]. Trans. Nonferrous Met. Soc. China, 2010, 20: 668
|
| [9] |
Hao S M, Xie J P, Wang A Q, et al. Hot deformation behavior and processing map of SiCp/2024Al composite [J]. Rare Met. Mater. Eng., 2014, 43: 2912
|
| [10] |
Ramanathan S, Karthikeyan R, Ganasen G. Development of processing maps for 2124Al/SiCp composites [J]. Mater. Sci. Eng., 2006, A441: 321
|
| [11] |
Hao S M, Xie J P, Wang A Q, et al. Hot deformation behaviors of 35%SiCp/2024Al metal matrix composites [J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 2468
doi: 10.1016/S1003-6326(14)63372-0
|
| [12] |
Gangolu S, Rao A G, Sabirov I, et al. Development of constitutive relationship and processing map for Al-6.65Si-0.44Mg alloy and its composite with B4C particulates [J]. Mater. Sci. Eng., 2016, A655: 256
|
| [13] |
Li Y L, Wang W X, Zhou J, et al. Hot deformation behaviors and processing maps of B4C/Al6061 neutron absorber composites [J]. Mater. Charact., 2017, 124: 107
|
| [14] |
Shao J C, Xiao B L, Wang Q Z, et al. Constitutive flow behavior and hot workability of powder metallurgy processed 20 vol.%SiCp/2024Al composite [J]. Mater. Sci. Eng., 2010, A527: 7865
|
| [15] |
Galiyev A, Kaibyshev R, Gottstein G. Correlation of plastic deformation and dynamic recrystallization in magnesium alloy ZK60 [J]. Acta. Mater., 2001, 49: 1199
|
| [16] |
Zhu Y P, Jin P P, Zhao P T, et al. Hot deformation behavior of Mg2B2O5 whiskers reinforced AZ31B magnesium composite fabricated by stir-casting [J]. Mater. Sci. Eng., 2013, A573: 148
|
| [17] |
Murty S V S N, Sarma M S, Rao B N. On the evaluation of efficiency parameters in processing maps [J]. Metall. Mater. Trans., 1997, 28A: 1581
|
| [18] |
Huang Z Y, Zhang X X, Xiao B L, et al. Hot deformation mechanisms and microstructure evolution of SiCp/2014Al composite [J]. J. Alloys Compd., 2017, 722: 145
|
| [19] |
Yang Q Y, Deng Z H, Zhang Z Q, et al. Effects of strain rate on flow stress behavior and dynamic recrystallization mechanism of Al-Zn-Mg-Cu aluminum alloy during hot deformation [J]. Mater. Sci. Eng., 2016, A662: 204
|
| [20] |
Peng W W, Zeng W D, Wang Q J, et al. Effect of processing parameters on hot deformation behavior and microstructural evolution during hot compression of as-cast Ti60 titanium alloy [J]. Mater. Sci. Eng., 2014, A593: 16
|
| [21] |
Prasad Y V R K. Dynamic materials model: Basis and principles [J]. Metall. Mater. Trans., 1996, 27A: 235
|
| [22] |
Prasad Y V R K, Gegel H L, Doraivelu S M, et al. Modeling of dynamic material behavior in hot deformation: Forging of Ti-6242 [J]. Metall. Trans., 1984, 15A: 1883
|
| [23] |
Chakravartty J K, Prasad Y V R K, Asundi M K. Processing map for hot working of alpha-zirconium [J]. Metall. Trans., 1991, 22A: 829
|
| [24] |
Prasad Y V R K. Recent advances in the science of mechanical processing [J]. Indian J. Technol., 1990, 28: 435
|
| [25] |
Wang C X, Yu F X, Zhao D Z, et al. Hot deformation and processing maps of DC cast Al-15%Si alloy [J]. Mater. Sci. Eng., 2013, A577: 73
|
| [26] |
Xiao B L, Fan J Z, Tian X F, et al. Hot deformation and processing map of 15%SiCp/2009 Al composite [J]. J. Mater. Sci., 2005, 40: 5757
|
| [27] |
Zhou L, Cui C, Wang Q Z, et al. Constitutive equation and model validation for a 31 vol.% B4Cp/6061Al composite during hot compression [J]. J. Mater. Sci. Technol., 2018, 34: 1730
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|