| 非等温时效对7B50铝合金组织及性能的影响 |
李吉臣1, 冯迪1,2( ), 夏卫生2, 林高用3, 张新明3, 任敏文1 |
1 江苏科技大学材料科学与工程学院 镇江 212003 2 华中科技大学材料科学与工程学院 武汉 430074 3 中南大学材料科学与工程学院 长沙 410083 |
|
| Effect of Non-Isothermal Ageing on Microstructure and Properties of 7B50 Aluminum Alloy |
LI Jichen1, FENG Di1,2( ), XIA Weisheng2, LIN Gaoyong3, ZHANG Xinming3, REN Minwen1 |
1 School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China 2 School of Materials Science and Engineering, Huazhong University of Science and Technology, Wuhan 430074, China 3 School of Materials Science and Engineering, Central South University, Changsha 410083, China |
引用本文:
李吉臣, 冯迪, 夏卫生, 林高用, 张新明, 任敏文. 非等温时效对7B50铝合金组织及性能的影响[J]. 金属学报, 2020, 56(9): 1255-1264.
Jichen LI,
Di FENG,
Weisheng XIA,
Gaoyong LIN,
Xinming ZHANG,
Minwen REN.
Effect of Non-Isothermal Ageing on Microstructure and Properties of 7B50 Aluminum Alloy[J]. Acta Metall Sin, 2020, 56(9): 1255-1264.
| [1] |
Feng D, Zhang X M, Chen H M, et al. Effect of non-isothermal retrogression and re-ageing on microstructure and properties of Al-8Zn-2Mg-2Cu alloy thick plate [J]. Acta Metall. Sin., 2018, 54: 100
|
| [1] |
(冯 迪, 张新明, 陈洪美等. 非等温回归再时效对Al-8Zn-2Mg-2Cu合金厚板组织及性能的影响 [J]. 金属学报, 2018, 54: 100)
|
| [2] |
Rometsch P A, Zhang Y, Knight S. Heat treatment of 7xxx series aluminium alloys—Some recent developments [J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 2003
|
| [3] |
Zhang X M, Deng Y L, Zhang Y. Development of high strength aluminum alloys and processing techniques for the materials [J]. Acta Metall. Sin., 2015, 51: 257
|
| [3] |
(张新明, 邓运来, 张 勇. 高强铝合金的发展及其材料的制备加工技术 [J]. 金属学报, 2015, 51: 257)
|
| [4] |
Cina B M. Reducing the susceptibility of alloys, particularly aluminium alloys, to stress corrosion cracking [P]. US Pat, 3856584, 1974
|
| [5] |
Ø Grong, Shercliff H R. Microstructural modelling in metals processing [J]. Prog. Mater. Sci., 2002, 47: 163
|
| [6] |
Hutchinson C R, Gouné M, Redjaïmia A. Selecting non-isothermal heat treatment schedules for precipitation hardening systems: An example of coupled process-property optimization [J]. Acta Mater., 2007, 55: 213
|
| [7] |
Feng D, Zhang X M, Liu S D, et al. The effect of pre-ageing temperature and retrogression heating rate on the microstructure and properties of AA7055 [J]. Mater. Sci. Eng., 2013, A588: 34
|
| [8] |
Li K, Zhang K, Yang L, et al. Investigation of non-isothermal aging process of 7085 aluminum alloy [A]. Proceedings of the 12th International Conference on Aluminium Alloys [C]. Yokohama, Japan: The Japan Institute of Light Metals, 2010: 2120
|
| [9] |
Tang Q J. Study on cooling ageing process of 7A85 aluminum alloy [D]. Harbin: Harbin Institute of Technology, 2010
|
| [9] |
(唐秋菊. 7A85铝合金降温时效工艺的研究 [D]. 哈尔滨: 哈尔滨工业大学, 2010)
|
| [10] |
Jiang J T, Tang Q J, Yang L, et al. Non-isothermal ageing of an Al-8Zn-2Mg-2Cu alloy for enhanced properties [J]. J. Mater. Process. Technol., 2016, 48: 110
|
| [11] |
Liu Y, Jiang D M, Li B Q, et al. Heating aging behavior of Al-8.35Zn-2.5Mg-2.25Cu alloy [J]. Mater. Des., 2014, 60: 116
|
| [12] |
Peng X Y, Guo Q, Liang X P, et al. Mechanical properties, corrosion behavior and microstructures of a non-isothermal ageing treated Al-Zn-Mg-Cu alloy [J]. Mater. Sci. Eng., 2017, A688: 146
|
| [13] |
Liu Y, Liang S, Jiang D M. Influence of repetitious non-isothermal aging on microstructure and strength of Al-Zn-Mg-Cu alloy [J]. J. Alloys Compd., 2016, 689: 632
doi: 10.1016/j.jallcom.2016.08.017
|
| [14] |
AMS 4252B-2005 Aluminum alloy, plate 6.4Zn-2.4Mg-2.2Cu-0.12Zr (7150-T7751) solution heat treated, stress relieved, and overaged [S]. 2005
|
| [15] |
Feng D, Zhang X M, Liu S D, et al. Effect of pre-aging temperature and retrogression heating rate on microstructure and properties of 7150 alloy [J]. Chin. J. Nonferrous Met., 2013, 23: 1173
|
| [15] |
(冯 迪, 张新明, 刘胜胆等. 预时效温度及回归加热速率对7150铝合金显微组织及性能的影响 [J]. 中国有色金属学报, 2013, 23: 1173)
|
| [16] |
Xu D, Li Z H, Wang G J, et al. Phase transformation and microstructure evolution of an ultra-high strength Al-Zn-Mg-Cu alloy during homogenization [J]. Mater. Charact., 2017, 131: 285
doi: 10.1016/j.matchar.2017.07.011
|
| [17] |
Azarniya A, Taheri A K, Taheri K K. Recent advances in ageing of 7xxx series aluminum alloys: A physical metallurgy perspective [J]. J. Alloys Compd., 2019, 781: 945
doi: 10.1016/j.jallcom.2018.11.286
|
| [18] |
Jiang D M, Liu Y, Liang S, et al. The effects of non-isothermal aging on the strength and corrosion behavior of Al-Zn-Mg-Cu alloy [J]. J. Alloys Compd., 2016, 681: 57
doi: 10.1016/j.jallcom.2016.04.208
|
| [19] |
Liu L L, Pan Q L, Wang X D, et al. The effects of aging treatments on mechanical property and corrosion behavior of spray formed 7055 aluminium alloy [J]. J. Alloys Compd., 2018, 735: 261
doi: 10.1016/j.jallcom.2017.11.070
|
| [20] |
BjØrneklett B I, Ø Grong, Myhr O R, et al. Additivity and isokinetic behaviour in relation to particle dissolution [J]. Acta Mater., 1998, 46: 6257
doi: 10.1016/S1359-6454(98)00260-2
|
| [21] |
Ø Grong, Myhr O R. Additivity and isokinetic behaviour in relation to diffusion controlled growth [J]. Acta Mater., 2000, 48: 445
doi: 10.1016/S1359-6454(99)00360-2
|
| [22] |
Myhr O R, Ø Grong. Modelling of non-isothermal transformations in alloys containing a particle distribution [J]. Acta Mater., 2000, 48: 1605
doi: 10.1016/S1359-6454(99)00435-8
|
| [23] |
Khalfallah A, Raho A A, Amzert S, et al. Precipitation kinetics of GP zones, metastable η′ phase and equilibrium η phase in Al-5.46wt.%Zn-1.67wt.%Mg alloy [J]. Trans. Nonferrous Met. Soc. China, 2019, 29: 233
|
| [24] |
Su R M, Qu Y D, Li R D. Pre-aging of retrogression and re-aging of spray formed 7075 alloy [J]. Acta Metall. Sin., 2014, 50: 863
|
| [24] |
(苏睿明, 曲迎东, 李荣德. 喷射态7075合金回归再时效中预时效的研究 [J]. 金属学报, 2014, 50: 863)
|
| [25] |
Panigrahi S K, Jayaganthan R. Influence of solutes and second phase particles on work hardening behavior of Al 6063 alloy processed by cryorolling [J]. Mater. Sci. Eng., 2011, A528: 3147
|
| [26] |
Han N M, Zhang X M, Liu S D, et al. Effects of pre-stretching and ageing on the strength and fracture toughness of aluminum alloy 7050 [J]. Mater. Sci. Eng., 2011, A528: 3714
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|