综述:SiC/Al界面反应与界面结构演变规律及机制 |
邱丰, 佟昊天, 沈平, 丛晓霜, 王轶, 姜启川( ) |
吉林大学材料科学与工程学院 长春 130025 |
|
Overview: SiC/Al Interface Reaction and Interface Structure Evolution Mechanism |
Feng QIU, Haotian TONG, Ping SHEN, Xiaoshuang CONG, Yi WANG, Qichuan JIANG( ) |
Department of Materials Science and Engineering, Jilin University, Changchun 130025, China |
引用本文:
邱丰, 佟昊天, 沈平, 丛晓霜, 王轶, 姜启川. 综述:SiC/Al界面反应与界面结构演变规律及机制[J]. 金属学报, 2019, 55(1): 87-100.
Feng QIU,
Haotian TONG,
Ping SHEN,
Xiaoshuang CONG,
Yi WANG,
Qichuan JIANG.
Overview: SiC/Al Interface Reaction and Interface Structure Evolution Mechanism[J]. Acta Metall Sin, 2019, 55(1): 87-100.
[1] | Taya M, Arsenault R J.A comparison between a shear lag type model and an eshelby type model in predicting the mechanical properties of a short fiber composite[J]. Scr. Metall., 1987, 21: 349 | [2] | Luo C P, Sui X D, Ouyang L Z, et al.Crvstallographic orientation relationship between SiC and Al in SiCp/Al-Si composites[J]. Acta Metall. Sin., 1999, 35: 343(罗承萍, 隋贤栋, 欧阳柳章等. SiCp/Al-Si复合材料中SiC/Al的晶体学位向关系[J]. 金属学报, 1999, 35: 343) | [3] | Lü W J, Bian Y J, Zhang D, et al.Growth mechanism of reinforcement in in situ processed TiC/Ti composites[J]. Acta Metall. Sin., 1999, 35: 536(吕维洁, 卞玉君,张荻等. 原位合成TiC/Ti基复合材料增强体的生长机制[J]. 金属学报, 1999, 35: 536) | [4] | Fan G L, Yu Z Y, Tan Z Q, et al.Evolution, control, and effects of interface in CNT/Al composites: A review[J]. Acta Metall. Sin.(Engl. Lett.), 2014, 27: 839 | [5] | Qian F.An investigation on fabrication of SiCp/Al composite materials with pressureless infiltration techniques [D]. Nanjing: Nanjing University of Science and Technology, 2008(钱凤. 无压浸渗法制备SiCp/Al复合材料的研究 [D]. 南京: 南京理工大学, 2008) | [6] | Nie J H, Fan J Z, Zhang S M, et al.Tensile and fracture properties of 15 vol% SiCp/2009Al composites fabricated by hot isostatic pressing and hot extrusion processes[J]. Acta Metall. Sin.(Engl. Lett.), 2014, 27: 875 | [7] | Shi Z L, Ochiai S, Gu M Y, et al.Interfacial microstructure evolution in aluminium matrix composites reinforced with unoxidized and oxidized SiC particles[J]. Surf. Interface Anal., 2001, 31: 375 | [8] | Gupta M, Surappa M K, Qin S.Effect of interfacial characteristics on the failure-mechanism mode of a SiC reinforced A1 based metal-matrix composite[J]. J. Mater. Process. Technol., 1997, 67: 94 | [9] | Rado C, Kalogeropoulou S, Eustathopoulos N.Bonding and wetting in non-reactive metal/SiC systems: Weak or strong interfaces[J]. Mater. Sci. Eng., 2000, A276: 195 | [10] | Luo Z P, Song Y G, Zhang S Q.A TEM study of the microstructure of SiCP/Al composite prepared by pressureless infiltration method[J]. Scr. Mater., 2001, 45: 1183 | [11] | Shi Z L, Gu M Y, Liu J Y, et al.Interfacial reaction between the oxidized SiC particles and Al-Mg alloy[J]. Chin. Sci. Bull., 2001, 46: 1161(施忠良, 顾明元, 刘俊友等. 氧化的碳化硅与铝镁合金之间的界面反应[J]. 科学通报, 2001, 46: 1161) | [12] | Wu G H, Su J, Gou H S, et al.Study on graphite fiber and Ti particle reinforced Al composite[J]. J. Mater. Sci., 2009, 44: 4776 | [13] | Song M H, Wu G H, Yang W S, et al.Mechanical properties of Cf/Mg composites fabricated by pressure infiltration method[J]. J. Mater. Sci. Technol., 2010, 26: 931 | [14] | Cong X S.Wettability of silicon carbide by molten aluminum or aluminum alloys and their interfacial microstructures [D]. Changchun: Jilin University, 2014(丛晓霜. Al及其合金与多晶α-SiC陶瓷的润湿及界面结构 [D]. 长春: 吉林大学, 2014) | [15] | Wang W M, Pan F S, Sun X W, et al.Advance in research on interfacial reaction in SiCp/Al composites[J]. J. Chongqing Univ.: Nat. Sci. Ed., 2004, 27: 108(王文明, 潘复生, 孙旭炜等. SiCp/Al复合材料界面反应研究现状[J]. 重庆大学学报: 自然科学版, 2004, 27: 108) | [16] | Viala J C, Fortier P, Bouix J.Stable and metastable phase equilibria in the chemical interaction between aluminium and silicon carbide[J]. J. Mater. Sci., 1990, 25: 1842 | [17] | Viala J C, Bosselet F, Laurent F, et al.Mechanism and kinetics of the chemical interaction between liquid aluminium and silicon-carbide single crystals[J]. J. Mater. Sci., 1993, 28: 5301 | [18] | Peteves S D, Tambuyser P, Helbach P, et al.Microstructure and microchemistry of the Al/SiC interface[J]. J. Mater. Sci., 1990, 25: 3765 | [19] | Iseki T, Kameda T, Maruyama T.Interfacial reactions between SiC and aluminium during joining[J]. J. Mater. Sci., 1984, 19: 1692 | [20] | Cong X S, Shen P, Wang Y, et al.Wetting of polycrystalline SiC by molten Al and Al-Si alloys[J]. Appl. Surf. Sci., 2014, 317: 140 | [21] | Shen P, Wang Y, Ren L H, et al.Influence of SiC surface polarity on the wettability and reactivity in an Al/SiC system[J]. Appl. Surf. Sci., 2015, 355: 930 | [22] | Laurent V, Chatain D, Eustathopoulos N.Wettability of SiC by aluminium and Al-Si alloys[J]. J. Mater. Sci., 1987, 22: 244 | [23] | Laurent V, Rado C, Eustathopoulos N.Wetting kinetics and bonding of Al and Al alloys on α-SiC[J]. Mater. Sci. Eng., 1996, A205: 1 | [24] | Ferro A C, Derby B.Wetting behaviour in the Al-Si/SiC System: Interface reactions and solubility effects[J]. Acta Metall. Mater., 1995, 43: 3061 | [25] | Hashim J, Looney L, Hashmi M S J. The wettability of SiC particles by molten aluminium alloy[J]. J. Mater. Process. Technol., 2001, 119: 324 | [26] | Landry K, Rado C, Eustathopoulos N.Influence of interfacial reaction rates on the wetting driving force in metal/ceramic systems[J]. Metall. Mater. Trans., 1996, 27A: 3181 | [27] | Wang Y.Wettability of SiC single crystal and carbon nanotubes by molten aluminum and their interfacial microstructures [D]. Changchun: Jilin University, 2015(王轶. Al在单晶SiC和碳纳米管上的润湿性及界面结构 [D]. 长春: 吉林大学, 2015) | [28] | Liu J S.Wettability of silicon carbide and silica by molten aluminum alloys and their interfacial microstructures [D]. Changchun: Jilin University, 2016(刘精深. Al合金与SiC和SiO2的润湿性及界面结构 [D]. 长春: 吉林大学, 2016) | [29] | Dezellus O, Hodaj F, Eustathopoulos N.Chemical reaction-limited spreading: The triple line velocity versus contact angle relation[J]. Acta Mater., 2002, 50: 4741 | [30] | Cassie A B D. Contact angle[J]. Discuss. Faraday Soc., 1948, 3: 11 | [31] | León C, Drew R.The influence of nickel coating on the wettability of aluminum on ceramics[J]. Composites, 2002, 33A: 1429 | [32] | Zhou J, Dru?d?el A T, Duszczyk J.The effect of extrusion parameters on the fretting wear resistance of Al-based composites produced via powder metallurgy[J]. J. Mater. Sci., 1999, 34: 5089 | [33] | Shi Z, Ochiai S, Gu M, et al.The formation and thermostability of MgO and MgAl2O4 nanoparticles in oxidized SiC particle-reinforced Al-Mg composites[J]. Appl. Phys., 2002, 74A: 97 | [34] | Xu X Y, Wang H Y, Zha M, et al.Effects of Ti, Si, Mg and Cu additions on interfacial properties and electronic structure of Al(111)/4H-SiC(0001) interface: A first-principles study[J]. Appl. Surf. Sci., 2018, 437: 103 | [35] | Beer S Z.Liquid Metals: Chemistry and Physics[M]. New York: Marcel Dekker, 1972: 127 | [36] | Lee J C, Ahn J P, Shim J H, et al.Interfacial phenomena in the SiC/2024Al composite: II Tailoring the interface[J]. Korea Inst. Met. Mater., 2000, 38: 322 | [37] | Pai B C, Ramani G, Pillai R M, et al.Role of magnesium in cast aluminium alloy matrix composites[J]. J. Mater. Sci., 1995, 30: 1903 | [38] | Guo J.The effects and mutual action of alloy elements and SiC particulate surface condition on the interface of SiCp/Al composites [D]. Zhengzhou: Zhengzhou University, 2003(郭建. 合金元素及增强体表面状况对SiCp/Al复合材料界面的影响及其交互作用 [D]. 郑州: 郑州大学, 2003) | [39] | Guo J, Shen N F.Control of detrimental interface reaction in SiCp/Al composite materials[J]. Mater. Sci. Eng., 2002, 20: 605(郭建, 沈宁福. SiC颗粒增强Al基复合材料中有害界面反应的控制[J]. 材料科学与工程, 2002, 20: 605) | [40] | Pech-Canul M I, Katz R N, Makhlouf M M, et al. The role of silicon in wetting and pressureless infiltration of SiCp preforms by aluminum alloys[J]. J. Mater. Sci., 2000, 35: 2167 | [41] | Ramani G, Pillai R M, Pai B C, et al.Effect of mixing conditions and reactive elements on the porosity and dispersion of SiC particulate in cast Al-SiCp composites[J]. J. Mater. Sci., 1993, 12: 1117 | [42] | Ferro A C, Derby B.Wetting behaviour in the Al-Si/SiC System: Interface reactions and solubility effects[J]. Acta Metall. Mater., 1995, 43: 3061 | [43] | Lee J C, Byun J Y, Park S B, et al.Prediction of Si contents to suppress the formation of Al4C3 in the SiCp/Al composite[J]. Acta Mater., 1998, 46: 1771 | [44] | Fang X, Fan T X, Zhang D.Work of adhesion in Al/SiC composites with alloying element addition[J]. Metall. Mater. Trans., 2013, 44A: 5192 | [45] | Lee J C, Byun J Y, Oh C S, et al.Effect of various processing methods on the interfacial reactions in SiCp/2024 Al composites[J]. Acta Mater., 1997, 45: 5303 | [46] | Han D S, Jones H, Atkinson H V.The wettability of silicon carbide by liquid aluminium: The effect of free silicon in the carbide and of magnesium, silicon and copper alloy additions to the aluminium[J]. J. Mater. Sci., 1993, 28: 2654 | [47] | Candan E.Effect of alloying elements to aluminium on the wettability of Al/SiC system[J]. Turk. J. Eng. Environ. Sci., 2002, 26: 1 | [48] | Rodríguez-Reyes M, Pech-Canul M I, Rendón-Angeles J C, et al. Limiting the development of Al4C3 to prevent degradation of Al/SiCp composites processed by pressureless infiltration[J]. Compos. Sci. Technol., 2006, 66: 1056 | [49] | Fang X.Thoeretical prediction of interfacial reaction and work of adhesion in SiC/Al composites [D]. Shanghai: Shanghai Jiao Tong University, 2013(房鑫. SiC/Al复合材料界面反应与粘着功理论预测研究 [D]. 上海: 上海交通大学, 2013) | [50] | Lee J C, Park S B, Seok H K, et al.Prediction of Si contents to suppress the interfacial reaction in the SiCp/2014 Al composite[J]. Acta Mater., 1998, 46: 2635 | [51] | Li J G, Coudurier L, Eustathopoulos N.Work of adhesion and contact-angle isotherm of binary alloys on ionocovalent oxides[J]. J. Mater. Sci., 1989, 24: 1109 | [52] | Zhong W M, L'Espérance G, Suéry M. Interfacial reactions in Al-Mg (5083)/Al2O3p composites during fabrication and remelting[J]. Metall. Mater. Trans., 1995, 26A: 2625 | [53] | Ghosh P K, Ray S.Influence of annealing on the mechanical properties of compocast Al(Mg)-Al2O3 particulate composite[J]. J. Mater. Sci., 1993, 28: 3783 | [54] | Sreekumar V M, Ravi K R, Pillai R M, et al.Thermodynamics and kinetics of the formation of Al2O3/MgAl2O4/MgO in Al-silica metal matrix composite[J]. Metall. Mater. Trans., 2008, 39A: 919 | [55] | Lee K B, Kim Y S, Kwon H.Fabrication of Al-3 Wt pct Mg matrix composites reinforced with Al2O3 and SiC particulates by the pressureless infiltration technique[J]. Metall. Mater. Trans., 1998, 29A: 3087 | [56] | Petitcorps Y L, Quenisset J M, Le Borgne G, et al.Segregation of magnesium in squeeze-cast aluminium matrix composites reinforced with alumina fibres[J]. Mater. Sci. Eng., 1991, A135: 37 | [57] | Hallstedt B, ?gren J, Liu Z K.Fibre-matrix interactions during fabrication of Al2O3 Mg metal matrix composites[J]. Mater. Sci. Eng., 1990, A129: 135 | [58] | Zuo R.The reaction and structure evolution at the interfaces of Al/Al alloy-SiC/SiCox [D]. Changchun: Jilin University, 2017(左蕊. Al/Al合金-SiC/SiCox界面反应与结构演变 [D]. 长春: 吉林大学, 2017) | [59] | Ribes H, Suéry M, L'esperance Q, et al. Microscopic examination of the interface region in 6061-Al/SiC composites reinforced with as-received and oxidized SiC particles[J]. Metall. Mater. Trans., 1990, 21A: 2489 | [60] | Fishkis M.Interfaces and fracture surfaces in Saffil/Al-Mg-Cu metal-matrix composites[J]. J. Mater. Sci., 1991, 26: 2651 | [61] | Lee J C, Lee H I, Ahn J P, et al.Modification of the interface in SiC/Al composites[J]. Metall. Mater. Trans., 2000, 31A: 2361 | [62] | Ma X C, Wu J B.An investigation on wettability and interfacial phenomena of Al-SiC system[J]. Mater. Sci. Eng., 1994, 12(1): 37(马晓春, 吴锦波. Al-SiC系润湿性与界面现象的研究[J]. 材料科学与工程, 1994, 12(1): 37) | [63] | Pan F S, Zhang J, Chen H, et al.Effect of rare earth additions on the wettability of An-Al-Zn-Mg-Cu/Al2O3 system[J]. Acta Mater. Compos. Sin., 1998, 15(1): 46(潘复生, 张静, 陈晖等. 稀土对Al-Zn-Mg-Cu/Al2O3陶瓷界面润湿性的影响[J]. 复合材料学报, 1998, 15(1): 46) | [64] | Carotenuto G, Gallo A, Nicolais L.Degradation of SiC particles in aluminium-based composites[J]. J. Mater. Sci., 1994, 29: 4967 | [65] | Eustathopoulos N, Coudurier L. Adsorption and wettability in metal/ceramic system [A]. Capillarity Today [C]. Berlin: Springer, 1991, vol.386: 15 | [66] | Saiz E, Tomsia A P.Atomic dynamics and Marangoni films during liquid-metal spreading[J]. Nat. Mater., 2004, 3: 903 | [67] | Tanaka S, Kohyama M.Ab initio calculations of 3C-SiC[111]/Ti polar interfaces [A]. 2000 International Semiconducting and Insulating Materials Conference[C]. Canberra, ACT, Australia, Australia: IEEE, 2000: 299 | [68] | Zhang L J, Yang D L, Qiu F, et al.Effects of reinforcement surface modification on the microstructures and tensile properties of SiCp/Al2014 composites[J]. Mater. Sci. Eng., 2015, A624: 102 | [69] | Shaga A.Fabrication of nacre-inspired Al alloy/SiC lamellar composites and their microstructures and properties [D]. Changchun: Jilin University, 2016(阿拉腾沙嘎. 仿珍珠贝Al合金/SiC层状复合材料的制备、组织与性能 [D]. 长春: 吉林大学, 2016) | [70] | Zhang H, Shen P, Shaga A, et al.Preparation of nacre-like composites by reactive infiltration of a magnesium alloy into porous silicon carbide derived from ice template[J]. Mater. Lett., 2016, 183: 299 | [71] | Shen P, Xi J W, Fu Y J, et al.Preparation of high-strength Al-Mg-Si/Al2O3 composites with lamellar structures using freeze casting and pressureless infiltration techniques[J]. Acta Metall. Sin.(Engl. Lett.), 2014, 27: 944 | [72] | Shaga A, Shen P, Sun C, et al.Lamellar-interpenetrated Al-Si-Mg/SiC composites fabricated by freeze casting and pressureless infiltration[J]. Mater. Sci. Eng., 2015, A630: 78 | [73] | Shaga A, Shen P, Guo R F, et al.Effects of oxide addition on the microstructure and mechanical properties of lamellar SiC scaffolds and Al-Si-Mg/SiC composites prepared by freeze casting and pressureless infiltration[J]. Ceram. Int., 2016, 42: 9653 |
|
|