| 奥氏体/铁素体层状条带结构高锰钢的微观组织及其性能 |
朱恺, 伍翠兰( ), 谢盼, 韩梅, 刘元瑞, 张香阁, 陈江华 |
| 湖南大学材料科学与工程学院 长沙 410082 |
|
| Microstructure and Mechanical Properties of an Austenite/Ferrite Laminate Structured High-Manganese Steel |
Kai ZHU, Cuilan WU( ), Pan XIE, Mei HAN, Yuanrui LIU, Xiangge ZHANG, Jianghua CHEN |
| College of Materials Science and Engineering, Hunan University, Changsha 410082, China |
引用本文:
朱恺, 伍翠兰, 谢盼, 韩梅, 刘元瑞, 张香阁, 陈江华. 奥氏体/铁素体层状条带结构高锰钢的微观组织及其性能[J]. 金属学报, 2018, 54(10): 1387-1398.
Kai ZHU,
Cuilan WU,
Pan XIE,
Mei HAN,
Yuanrui LIU,
Xiangge ZHANG,
Jianghua CHEN.
Microstructure and Mechanical Properties of an Austenite/Ferrite Laminate Structured High-Manganese Steel[J]. Acta Metall Sin, 2018, 54(10): 1387-1398.
| [1] | Latypov M I, Shin S, De Cooman B C, et al. Micromechanical finite element analysis of strain partitioning in multiphase medium manganese TWIP+TRIP steel[J]. Acta Mater., 2016, 108: 219 | | [2] | Frommeyer G, Brüx U, Neumann P, et al.Supra-ductile and high-strength manganese-TRIP/TWIP steels for high energy absorption purposes[J]. ISIJ Int., 2003, 43: 438 | | [3] | Li K, Injeti V S Y, Misra R D K, et al. On the strain rate sensitivity of aluminum-containing transformation-induced plasticity steels: Interplay between TRIP and TWIP effects[J]. Mater. Sci. Eng., 2017, A711: 515 | | [4] | Allain S, Chateau J P, Dahmoun D, et al. Modeling of mechanical twinning in a high manganese content austenitic steel [J]. Mater. Sci. Eng., 2004, A387-389: 272 | | [5] | Bouaziz O, Guelton N. Modelling of TWIP effect on work-hardening [J]. Mater. Sci. Eng., 2001, A319-321: 246 | | [6] | Wang Y M, Chen M W, Sheng H W, et al.Nanocrystalline grain structures developed in commercial purity Cu by low-temperature cold rolling[J]. J. Mater. Res., 2002, 17: 3004 | | [7] | Huang X X, Hansen N, Tsuji N.Hardening by annealing and softening by deformation in nanostructured metals[J]. Science, 2006, 312: 249 | | [8] | Valiev R.Nanostructuring of metals by severe plastic deformation for advanced properties[J]. Nat. Mater., 2004, 3: 511 | | [9] | Wu X L, Yang M X, Yuan F P, et al.Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility[J]. Proc. Natl. Acad. Sci. U. S. A., 2015, 112: 14501 | | [10] | Wang Y M, Ma E.Three strategies to achieve uniform tensile deformation in a nanostructured metal[J]. Acta Mater., 2004, 52: 1699 | | [11] | Song R, Ponge D, Raabe D, et al.Overview of processing, microstructure and mechanical properties of ultrafine grained bcc steels[J]. Mater. Sci. Eng., 2006, A441: 1 | | [12] | Rezaee A, Kermanpur A, Najafizadeh A, et al.Production of nano/ultrafine grained AISI 201L stainless steel through advanced thermo-mechanical treatment[J]. Mater. Sci. Eng., 2011, A528: 5025 | | [13] | Forouzan F, Najafizadeh A, Kermanpur A, et al.Production of nano/submicron grained AISI 304L stainless steel through the martensite reversion process[J]. Mater. Sci. Eng., 2010, A527: 7334 | | [14] | Dini G, Najafizadeh A, Monir-Vaghefi S M, et al. Grain size effect on the martensite formation in a high-manganese TWIP steel by the Rietveld method[J]. J. Mater. Sci. Technol., 2010, 26: 181 | | [15] | Yin Y Q, Wu C L, Xie P, et al.An ultrafine grained duplex Mn12Ni2MoTi(Al) steel fabricated by cold rolling and annealing[J]. Acta Metall. Sin., 2016, 52: 1527(尹炎祺, 伍翠兰, 谢盼等. 冷轧及退火制备的超细晶粒双相Mn12Ni2MoTi(Al)钢[J]. 金属学报, 2016, 52: 1527) | | [16] | Tsuji N, Ueji R, Minamino Y, et al.A new and simple process to obtain nano-structured bulk low-carbon steel with superior mechanical property[J]. Scr. Mater., 2002, 46: 305 | | [17] | Eizadjou M, Talachi A K, Manesh H D, et al.Investigation of structure and mechanical properties of multi-layered Al/Cu composite produced by accumulative roll bonding (ARB) process[J]. Compos. Sci. Technol., 2008, 68: 2003 | | [18] | Fang T H, Li W L, Tao N R, et al.Revealing extraordinary intrinsic tensile plasticity in gradient nano-grained copper[J]. Science, 2011, 331: 1587 | | [19] | Tan H F, Zhang B, Luo X M, et al.Strain rate dependent tensile plasticity of ultrafine-grained Cu/Ni laminated composites[J]. Mater. Sci. Eng., 2014, A609: 318 | | [20] | Lee H, Min C J, Sohn S S, et al.Novel medium-Mn (austenite+martensite) duplex hot-rolled steel achieving 1.6GPa strength with 20% ductility by Mn-segregation-induced TRIP mechanism[J]. Acta Mater., 2018, 147: 247 | | [21] | Ueji R, Tsuji N, Minamino Y, et al.Effect of rolling reduction on ultrafine grained structure and mechanical properties of low-carbon steel thermomechanically processed from martensite starting structure[J]. Sci. Technol. Adv. Mater., 2004, 5: 153 | | [22] | Wu X L, Yang M X, Yuan F P, et al.Combining gradient structure and TRIP effect to produce austenite stainless steel with high strength and ductility[J]. Acta Mater., 2016, 112: 337 | | [23] | Ma X L, Huang C X, Moering J, et al.Mechanical properties of copper/bronze laminates: Role of interfaces[J]. Acta Mater., 2016, 116: 43 | | [24] | Zhang L, Chen Z, Wang Y H, et al.Fabricating interstitial-free steel with simultaneous high strength and good ductility with homogeneous layer and almella structure[J]. Scr. Mater., 2017, 141: 111 | | [25] | Chen H, Zhang C Y, Zhu J N, et al.Austenite/ferrite interface migration and alloying elements partitioning: An overview[J]. Acta Metall. Sin., 2018, 54: 217(陈浩, 张璁雨, 朱加宁等. 奥氏体/铁素体界面迁移与元素配分的研究进展[J]. 金属学报, 2018, 54: 217) | | [26] | Xie P, Han M, Wu C L, et al.A high-performance TRIP steel enhanced by ultrafine grains and hardening precipitates[J]. Mater. Des., 2017, 127: 1 | | [27] | De Amar K, Murdock D C, Mataya M C, et al.Quantitative measurement of deformation-induced martensite in 304 stainless steel by X-ray diffraction[J]. Scr. Mater., 2004, 50: 1445 | | [28] | Chen Y, Wu C L, Xie P, et al.A phase-transformation-strengthened surface layer on Fe-20Mn-3Al-3Si steel fabricated by mechanical grinding[J]. Acta Metall. Sin., 2014, 50: 423(陈燕, 伍翠兰, 谢盼等. 机械磨擦制备的Fe-20Mn-3Al-3Si钢表面相变强化层[J]. 金属学报, 2014, 50: 423) | | [29] | Xu H J, Xu Y B, Jiao H T, et al.Influence of grain size and texture prior to warm rolling on microstructure, texture and magnetic properties of Fe-6.5%wt%Si steel[J]. J. Magn. Magn. Mater., 2018, 453: 236 | | [30] | De Moor E, Matlock D K, Speer J G, et al.Austenite stabilization through manganese enrichment[J]. Scr. Mater., 2011, 64: 185 | | [31] | Lee S, Kim J, Lee S J, et al.Effect of nitrogen on the critical strain for dynamic strain aging in high-manganese twinning-induced plasticity steel[J]. Scr. Mater., 2011, 65: 528 | | [32] | Oh K H, Jeong J S, Koo Y M, et al.The evolution of the rolling and recrystallization textures in cold-rolled Al containing high Mn austenitic steels[J]. Mater. Chem. Phys., 2015, 161: 9 | | [33] | Lee D A.Elastic properties of thin films of cubic system[J]. Thin Solid Films, 2003, 434: 183 | | [34] | Lee D A.A stability criterion for deformation and deposition textures of metals during annealing[J]. J. Mater. Process. Technol., 2001, 117: 307 |
|
|