| 奥氏体化温度对中碳淬火-配分钢干滑动摩擦磨损性能的影响 |
杨继兰1, 蒋元凯1, 顾剑锋1, 郭正洪1( ), 陈海龑2 |
1 上海交通大学材料科学与工程学院 上海 200240 2 上海海事大学海洋科学与工程学院 上海 201306 |
|
| Effect of Austenitization Temperature on the Dry Sliding Wear Properties of a Medium Carbon Quenching and Partitioning Steel |
Jilan YANG1, Yuankai JIANG1, Jianfeng GU1, Zhenghong GUO1( ), Haiyan CHEN2 |
1 School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China 2 College of Ocean Science and Engineering, Shanghai Maritime University, Shanghai 201306, China |
引用本文:
杨继兰, 蒋元凯, 顾剑锋, 郭正洪, 陈海龑. 奥氏体化温度对中碳淬火-配分钢干滑动摩擦磨损性能的影响[J]. 金属学报, 2018, 54(1): 21-30.
Jilan YANG,
Yuankai JIANG,
Jianfeng GU,
Zhenghong GUO,
Haiyan CHEN.
Effect of Austenitization Temperature on the Dry Sliding Wear Properties of a Medium Carbon Quenching and Partitioning Steel[J]. Acta Metall Sin, 2018, 54(1): 21-30.
| [1] | Speer J G, Matlock D K, De Cooman B C, et al. Carbon partitioning into austenite after martensite transformation[J]. Acta Mater., 2003, 51: 2611 | | [2] | Santofimia M J, Nguyen-Minh T, Zhao L, et al.New low carbon Q&P steels containing film-like intercritical ferrite[J]. Mater. Sci. Eng., 2010, A527: 6429 | | [3] | Santofimia M J, Zhao L, Petrov R, et al.Microstructural development during the quenching and partitioning process in a newly designed low-carbon steel[J]. Acta Mater., 2011, 59: 6059 | | [4] | Wang L, Speer J G.Quenching and partitioning steel heat treatment[J]. Metall. Microstruct. Anal., 2013, 2: 268 | | [5] | Zhao C, Tang D, Jiang H T, et al.Process simulation and microstructure analysis of low carbon Si-Mn quenched and partitioned steel[J]. J. Iron Steel Res. Int., 2008, 15: 82 | | [6] | Speer J G,Rizzo Assun??o F C R,Matlock D K,et al. The "quenching and partitioning" process: Background and recent progress[J]. Mater. Res., 2005, 8: 417 | | [7] | Zhang K, Xu W Z, Guo Z H, et al.Effects of novel Q-P-T and traditional Q-T processes on the microstructure and mechanical properties of martensitic steels with different carbon content[J]. Acta Metall. Sin., 2011, 47: 489(张珂, 许为宗, 郭正洪等. 新型Q-P-T和传统Q-T工艺对不同C含量马氏体钢组织和力学性能的影响[J]. 金属学报, 2011, 47: 489) | | [8] | Weng Y Q, Dong H, Gan Y.Advanced Steels [M]. Beijing: Metallurgical Industry Press, 2011: 67 | | [9] | Wang C Y, Shi J, Liu S, et al.Study on three-body impact-abrasion of steel treated by quenching-partitioning-tempering process[J]. Chin. J. Mater. Res., 2009, 23: 305(王存宇, 时捷, 刘苏等. 淬火-配分-回火工艺处理钢的三体冲击磨损性能研究[J]. 材料研究学报, 2009, 23: 305) | | [10] | Liu S G, Dong S S, Yang F, et al.Application of quenching-partitioning-tempering process and modification to a newly designed ultrahigh carbon steel[J]. Mater. Des., 2014, 56: 37 | | [11] | Wang C Y, Li X D, Chang Y, et al. Comparison of three-body impact abrasive wear behaviors for quenching-partitioning-tempering and quenching-tempering 20Si2Ni3 steels[J]. Wear, 2016, 362-363: 121 | | [12] | Hu F, Wu K M, Hodgson P D.Effect of retained austenite on wear resistance of nanostructured dual phase steels[J]. Mater. Sci. Technol., 2016, 32: 40 | | [13] | Kim H J, Kweon Y G.The effects of retained austenite on dry sliding wear behavior of carburized steels[J]. Wear, 1996, 193: 8 | | [14] | Riviére J P, Brin C, Villain J P.Structure and topography modifications of austenitic steel surfaces after friction in sliding contact[J]. Appl. Phys., 2003, 76A: 277 | | [15] | Zandrahimi M, Bateni M R, Poladi A, et al.The formation of martensite during wear of AISI 304 stainless steel[J]. Wear, 2007, 263: 674 | | [16] | Molinari A, Pellizzari M, Gialanella S, et al.Effect of deep cryogenic treatment on the mechanical properties of tool steels[J]. J. Mater. Proc. Technol., 2001, 118: 350 | | [17] | Wei X C, Li J, Meng H.Tribological characteristics of HSLA TRIP steel containing meta-stable retained austenite[J]. Tribology, 2006, 26: 49(韦习成, 李健, Meng H.含亚稳残余奥氏体HSLA TRIP钢的摩擦磨损性能研究[J]. 摩擦学学报, 2006, 26: 49) | | [18] | Liu Y, Yu W P, Zhang J D, et al.Effect of deep cryogenic treatment on microstructure and mechanical properties of T8A steel[J]. Trans. Mater. Heat Treat., 2010, 31(10): 48(刘勇, 于文平, 张金东等. 深冷处理对T8A钢组织和力学性能的影响[J]. 材料热处理学报, 2010, 31(10): 48) | | [19] | Wu H Y.Study on friction-induced martensite transformation of retained austenite and its wear resistance[J]. Hot Work. Technol., 2007, 36(16): 32(吴海燕. 残余奥氏体的摩擦诱发马氏体相变行为及其耐磨特性的研究[J]. 热加工工艺, 2007, 36(16): 32) | | [20] | Arques J L, Prado J M.The dry wear resistance of a carbonitrided steel[J]. Wear, 1985, 103: 321 | | [21] | Siepak J.The influence of contact stress on the wear of a carburized steel case with a high content of retained austenite[J]. Wear, 1982, 80: 301 | | [22] | Jatczak C F.Retained Austenite and its Measurement by X-ray Diffraction [R]. SAE Technical Paper 800426. Detroit: Society of Automotive Engineers, Inc., 1980: 6 | | [23] | Xiong Z L, Cai Q W, Jiang H T, et al.Research on mechanical stability of austenite in TRIP steels[J]. J. Mater. Eng., 2011, (3): 11(熊自柳, 蔡庆伍, 江海涛等. TRIP钢中奥氏体的力学稳定性研究[J]. 材料工程, 2011, (3): 11) | | [24] | Huang F, Yang J L, Guo Z H, et al.Effect of partitioning treatment on the mechanical property of Fe-0.19C-1.47Mn-1.50Si steel with refined martensitic microstructure[J]. Metall. Mater. Trans., 2016, 47A: 1072 | | [25] | Yao Y Q.The research on friction and wear properties of low-carbon low-alloy steels [D].Nanjing: Nanjing University of Science and Technology, 2013)(姚寅群.低碳低合金钢摩擦磨损性能研究 [D]. 南京: 南京理工大学, 2013) | | [26] | Wang Y, Lei T Q, Liu J J.Tribo-metallographic behavior of high carbon steels in dry sliding: II. Microstructure and wear[J]. Wear, 1999, 231: 12 | | [27] | Sun J S.Wear of Metals [M]. Beijing: Metallurgical Industry Press, 1992: 182(孙家枢. 金属的磨损 [M]. 北京: 冶金工业出版社, 1992: 182) | | [28] | Xu Y L, Qin H Q, Pang Z G, et al.Wear resistance at high temperature of H13 steel after RE-N-C-S-V-Nb multi-element penetrating[J]. Surf. Technol., 2015, 44(4): 60(徐永礼, 覃海泉, 庞祖高等. RE-N-C-S-V-Nb多元共渗H13钢的高温耐磨性[J]. 表面技术, 2015, 44(4): 60) | | [29] | Wang M S, Zhu Y F.The plastic induced martensite transformation of a medium manganese austenite steel[J].Phys. Tests. Chem. Anal. (Phys.Test.), 1991, A(1): 23(王明胜, 朱延福.奥氏体中锰钢的形变诱发马氏体[J]. 理化检验(物理分册), 1991, A(1): 23) | | [30] | Society of Heat Treatment,Chinese Society of Mechanical Engineers. The Friction Wear and Heat Treatment of Metals [M]. Beijing: Mechanical Industry Press, 1988: 93(中国机械工程学会热处理学会. 金属的摩擦磨损与热处理 [M]. 北京: 机械工业出版社, 1988: 93) |
|
|