| 等通道挤压制备医用超细晶Mg-3Sn-0.5Mn合金及其力学性能 |
潘瑜1,2, 张殿涛2, 谭雨宁2, 李珍1,2, 郑玉峰1,3, 李莉1,2( ) |
1 哈尔滨工程大学生物医学材料与工程研究中心 哈尔滨 150001 2 哈尔滨工程大学材料加工及智能制造研究所 哈尔滨 150001 3 北京大学前沿交叉学科研究院生物医用材料与组织工程中心 北京 100871 |
|
| Mechanical Properties of Biomedical Ultrafine Grained Mg-3Sn-0.5Mn Alloy Processed by Equal-Channel Angular Pressing |
Yu PAN1,2, Diantao ZHANG2, Yuning TAN2, Zhen LI1,2, Yufeng ZHENG1,3, Li LI1,2( ) |
1 Center for Biomedical Materials and Engineering, Harbin Engineering University, Harbin 150001, China 2 Institute of Material Processing and Intelligent Manufacturing, Harbin Engineering University, Harbin 150001, China 3 Center for Biomedical Materials and Tissue Engineering, Academy for Advanced Interdisciplinary, Peking University, Beijing 100871, China |
引用本文:
潘瑜, 张殿涛, 谭雨宁, 李珍, 郑玉峰, 李莉. 等通道挤压制备医用超细晶Mg-3Sn-0.5Mn合金及其力学性能[J]. 金属学报, 2017, 53(10): 1357-1363.
Yu PAN,
Diantao ZHANG,
Yuning TAN,
Zhen LI,
Yufeng ZHENG,
Li LI.
Mechanical Properties of Biomedical Ultrafine Grained Mg-3Sn-0.5Mn Alloy Processed by Equal-Channel Angular Pressing[J]. Acta Metall Sin, 2017, 53(10): 1357-1363.
| [2] | Agarwal S, Curtin J, Duffy B, et al.Biodegradable magnesium alloys for orthopaedic applications: A review on corrosion, biocompatibility and surface modifications[J]. Mater. Sci. Eng., 2016, C68: 948 | | [3] | Zheng Y F, Gu X N, Witte F.Biodegradable metals[J]. Mater. Sci. Eng., 2014, R77: 1 | | [4] | Cheng M Q, Wahafu T, Jiang G F, et al.A novel open-porous magnesium scaffold with controllable microstructures and properties for bone regeneration[J]. Sci. Rep., 2016, 6: 24134 | | [5] | Hou L D, Li Z, Pan Y, et al.In vitro and in vivo studies on biodegradable magnesium alloy[J]. Prog. Nat. Sci. Mater. Int., 2014, 24: 466 | | [6] | Hou L D, Li Z, Zhao H, et al.Microstructure, mechanical properties, corrosion behavior and biocompatibility of as-extruded biodegradable Mg-3Sn-1Zn-0.5Mn alloy[J]. J. Mater. Sci. Technol., 2016, 32: 874 | | [7] | Chen Y J, Xu Z G, Smith C, et al.Recent advances on the development of magnesium alloys for biodegradable implants[J]. Acta Biomater., 2014, 10: 4561 | | [8] | Amerstorfer F, Fischerauer S F, Fischer L, et al.Long-term in vivo degradation behavior and near-implant distribution of resorbed elements for magnesium alloys WZ21 and ZX50[J]. Acta Biomater., 2016, 42: 440 | | [9] | Cheng P F, Han P, Zhao C L, et al.Magnesium inference screw supports early graft incorporation with inhibition of graft degradation in anterior cruciate ligament reconstruction[J]. Sci. Rep., 2016, 6: 26434 | | [10] | Haude M, Ince H, Abizaid A, et al.Sustained safety and performance of the second-generation drug-eluting absorbable metal scaffold in patients with de novo coronary lesions: 12-month clinical results and angiographic findings of the BIOSOLVE-II first-in-man trial[J]. Eur. Heart J., 2016, 37: 2701 | | [11] | Haude M, Ince H, Abizaid A, et al.Safety and performance of the second-generation drug-eluting absorbable metal scaffold in patients with de-novo coronary artery lesions (BIOSOLVE-II): 6 month results of a prospective, multicentre, non-randomised, first-in-man trial[J]. Lancet, 2016, 387: 31 | | [12] | Zhao D W, Witte F, Lu F Q, et al.Current status on clinical applications of magnesium-based orthopaedic implants: A review from clinical translational perspective[J]. Biomaterials, 2017, 112: 287 | | [13] | Ge Q, Dellasega D, Demir A G, et al.The processing of ultrafine-grained Mg tubes for biodegradable stents[J]. Acta Biomater., 2013, 9: 8604 | | [14] | Mostaed E, Vedani M, Hashempour M, et al.Influence of ECAP process on mechanical and corrosion properties of pure Mg and ZK60 magnesium alloy for biodegradable stent applications[J]. Biomatter, 2014, 4: e28283 | | [15] | Mostaed E, Hashempour M, Fabrizi A, et al.Microstructure, texture evolution, mechanical properties and corrosion behavior of ECAP processed ZK60 magnesium alloy for biodegradable applications[J]. J. Mech. Behav. Biomed. Mater., 2014, 37: 307 | | [16] | Orlov D, Ralston K D, Birbilis N, et al.Enhanced corrosion resistance of Mg alloy ZK60 after processing by integrated extrusion and equal channel angular pressing[J]. Acta Mater., 2011, 59: 6176 | | [17] | Sunil B R, Kumar T S S, Chakkingal U, et al. In vitro and in vivo studies of biodegradable fine grained AZ31 magnesium alloy produced by equal channel angular pressing[J]. Mater. Sci. Eng., 2016, C59: 356 | | [18] | Su C W, Lu L, Lai M O.A model for the grain refinement mechanism in equal channel angular pressing of Mg alloy from microstructural studies[J]. Mater. Sci. Eng., 2006, A434: 227 | | [19] | Balogh L, Figueiredo R B, Ungár T, et al.The contributions of grain size, dislocation density and twinning to the strength of a magnesium alloy processed by ECAP[J]. Mater. Sci. Eng., 2010, A528: 533 | | [20] | Del Valle J A, Carre?o F, Ruano O A. Influence of texture and grain size on work hardening and ductility in magnesium-based alloys processed by ECAP and rolling[J]. Acta Mater., 2006, 54: 4247 | | [21] | Yuan W, Panigrahi S K, Su J Q, et al.Influence of grain size and texture on Hall-Petch relationship for a magnesium alloy[J]. Scr. Mater., 2011, 65: 994 | | [22] | Petch N J.The cleavage strength of polycrystals[J]. J. Iron Steel Inst., 1953, 174: 25 | | [23] | Chokshi A H, Rosen A, Karch J, et al.On the validity of the hall-petch relationship in nanocrystalline materials[J]. Scr. Metall., 1989, 23: 1679 | | [24] | Srinivasarao B, Dudamell N V, Pérez-Prado M T. Texture analysis of the effect of non-basal slip systems on the dynamic recrystallization of the Mg alloy AZ31[J]. Mater. Charact., 2013, 75: 101 | | [25] | Wang L F, Mostaed E, Cao X Q, et al.Effects of texture and grain size on mechanical properties of AZ80 magnesium alloys at lower temperatures[J]. Mater. Des., 2016, 89: 1 | | [26] | Xu W Q, Birbilis N, Sha G, et al.A high-specific-strength and corrosion-resistant magnesium alloy[J]. Nat. Mater., 2015, 14: 1229 | | [27] | Zhao M C, Liu M, Song G L, et al.Influence of the β-phase morphology on the corrosion of the Mg alloy AZ91[J]. Corro. Sci., 2008, 50: 1939 |
|
|