| Q-P-T处理贝氏体/马氏体复相高强钢疲劳断裂特性研究* |
桂晓露1,张宝祥2,高古辉1( ),赵平3,白秉哲1,3,翁宇庆1,3 |
1 北京交通大学机电学院材料中心, 北京 100044 2 北京有色金属研究总院有研亿金新材料有限公司, 北京 102200 3 清华大学材料学院先进材料教育部重点实验室, 北京 100084 |
|
| FATIGUE BEHAVIOR OF BAINITE/MARTENSITE MULTIPHASE HIGH STRENGTH STEEL TREATEDBY QUENCHING-PARTITIONING-TEMPERING PROCESS |
Xiaolu GUI1,Baoxiang ZHANG2,Guhui GAO1( ),Ping ZHAO3,Bingzhe BAI1,3,Yuqing WENG1,3 |
1 Materials Science and Engineering Research Center, School of Mechanical, Electronic and Control Engineering, Beijing Jiaotong University, Beijing 100044, China 2 GRIKIN Advanced Materials Co. Ltd., Beijing General Research Institute of Nonferrous Metals, Beijing 102200, China 3 Key Laboratory of Advanced Materials of Ministry of Education, School of Materials Science and Engineering, Tsinghua University, Beijing 100084, China |
引用本文:
桂晓露,张宝祥,高古辉,赵平,白秉哲,翁宇庆. Q-P-T处理贝氏体/马氏体复相高强钢疲劳断裂特性研究*[J]. 金属学报, 2016, 52(9): 1036-1044.
Xiaolu GUI,
Baoxiang ZHANG,
Guhui GAO,
Ping ZHAO,
Bingzhe BAI,
Yuqing WENG.
FATIGUE BEHAVIOR OF BAINITE/MARTENSITE MULTIPHASE HIGH STRENGTH STEEL TREATEDBY QUENCHING-PARTITIONING-TEMPERING PROCESS[J]. Acta Metall Sin, 2016, 52(9): 1036-1044.
| [1] | Rong Y H.Acta Metall Sin, 2011; 47: 1483 | | [1] | (戎咏华. 金属学报, 2011; 47: 1483) | | [2] | Matlock D K, Brautigam V E, Speer J G. Mater Sci Forum, 2003; 426-432: 1089 | | [3] | Zhao P, Gao G H,Misra R D K, Bai B Z. Mater Sci Eng, 2015; A630: 1 | | [4] | Zhang Y J, Hui W J, Xiang J Z, Dong H, Weng Y Q.Acta Metall Sin, 2009; 45: 880 | | [4] | (张永健, 惠卫军, 项金钟, 董瀚, 翁宇庆. 金属学报, 2009; 45: 880) | | [5] | Gao G H, Zhang H, Tan Z L, Liu W B, Bai B Z.Mater Sci Eng, 2013; A559: 165 | | [6] | Zhang C, Fang H S, Yang Z G, Bai B Z, Zhang W Z.Acta Metall Sin, 2001; 37: 561 | | [6] | (张弛, 方鸿生, 杨志刚, 白秉哲, 张文征. 金属学报, 2001; 37: 561) | | [7] | Parker E R.Metall Trans, 1977; 8A: 1025 | | [8] | Zhang K, Xu W Z, Guo Z H, Rong Y H, Wang M Q, Dong H.Acta Metall Sin, 2011; 47: 489 | | [8] | (张柯, 许为宗, 郭正洪, 戎咏华, 王毛球, 董瀚. 金属学报, 2011; 47: 489) | | [9] | Blonde R, Jimenez-Melero E, Zhao L, Wright J P, Bruck E, Zwaag van der S, Dijk van N H.Mater Sci Eng, 2014; A618: 280 | | [10] | Speer J G, Matlock D K, Cooman B C, Shroch J G.Acta Mater, 2003; 51: 2661 | | [11] | Edmonds D V, He K, Rizzo F C, Cooman De B C, Matlock D K, Speer J G. Mater Sci Eng, 2006; A438-440: 25 | | [12] | Wang X D, Guo Z H, Rong Y H.Mater Sci Eng, 2011; A529: 35 | | [13] | Zhou S, Zhang K, Wang Y, Gu J F, Rong Y H.Mater Sci Eng, 2011; A528: 8006 | | [14] | Gao G H, Zhang H, Gui X L, Tan Z L, Bai B Z, Weng Y Q.Acta Mater, 2015; 101: 31 | | [15] | Gao G H, Zhang H, Gui X L, Luo P, Tan Z L, Bai B Z.Acta Mater, 2014; 76: 425 | | [16] | Wei D Y, Gu J L, Fang H S, Bai B Z.Acta Metall Sin, 2003; 39: 734 | | [16] | (韦东远, 顾家琳, 方鸿生, 白秉哲. 金属学报, 2003; 39: 734) | | [17] | Yu Y, Gu J L, Bai B Z, Liu Y B, Li S X.Mater Sci Eng, 2009; A527: 212 | | [18] | de Diego-Calderon I, Rodriguez-Calvillo P, Lara A, Molina-Aldareguia J M, Petrov R H, De Knijf D, Sabirov I.Mater Sci Eng, 2015; A641: 215 | | [19] | Fan X.Metallic X-Ray Physics. Beijing: Mechanical Industry Press, 1989: 159 | | [19] | (范雄.金属X射线学. 北京: 机械工业出版社, 1989: 159) | | [20] | Wang S C, Wu Y W, Hua Y, Li Z C, Zhang H.J Mater Sci, 2010; 45: 5892 | | [21] | Gao G H, Zhang H, Gui X L, Tan Z L, Bai B Z.J Mater Sci Technol, 2015; 31: 199 | | [22] | Hsu T Y, Jin X J, Rong Y H.J Alloys Compd, 2013; 577S: 568 | | [23] | Sun J, Yu H, Wang S, Fan Y.Mater Sci Eng, 2014; A596: 89 | | [24] | Gao G H, Gui X L, An B F, Tan Z L, Bai B Z, Weng Y Q.Acta Metall Sin, 2015; 51: 21 | | [24] | (高古辉, 桂晓露, 安佰锋, 谭谆礼, 白秉哲, 翁宇庆. 金属学报, 2015; 51: 21) | | [25] | Bhadeshia H K D H, Edmonds D V.Met Sci, 1983; 17: 411 | | [26] | Bhadeshia H K D H, Edmonds D V.Met Sci, 1983; 17: 420 | | [27] | Nie W J, Shang C J, You Y, Zhang X B, Sundaresa S.Acta Metall Sin, 2012; 48: 797 | | [27] | (聂文金, 尚成嘉, 由洋, 张晓兵, Sundaresa S. 金属学报, 2012; 48: 797) | | [28] | Berns H, Wener L.Theor Appl Fract Mech, 1986; 6: 11 | | [29] | Zhu M L, Xuan F Z, Zhu K L, Wang G Z, Jia T Y.Acta Metall Sin, 2009; 45: 320 | | [29] | (朱明亮, 轩福贞, 朱奎龙, 王国珍, 贾天耀. 金属学报, 2009; 45: 320) | | [30] | Abareshi M, Emadoddin E.Mater Sci Eng, 2011; A32: 5099 | | [31] | Richman R H, Landgraf R W.Metall Trans, 1975; 6A: 955 | | [32] | Nakagawa H, Miyazaki T.J Mater Sci, 1999; 34: 3901 | | [33] | Parker E R.Metall Trans, 1977; 8A: 1025 | | [34] | Huang W G, Fang H S, Zheng Y K.Acta Metall Sin, 2001; 37: 927 | | [34] | (黄维刚, 方鸿生, 郑燕康. 金属学报, 2001; 37: 927) |
|
|