| 马氏体不锈钢上梯度纳米结构表层的形成及其对电化学腐蚀行为的影响* |
黄海威1,王镇波1( ),刘莉2,雍兴平3,卢柯1,4 |
1 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016
2 中国科学院金属研究所, 沈阳 110016
3 沈阳鼓风机集团股份有限公司, 沈阳 110869
4 南京理工大学格莱特纳米科技研究所, 南京 210094 |
|
| FORMATION OF A GRADIENT NANOSTRUCTURED SURFACE LAYER ON A MARTENSITIC STAINLESS STEEL AND ITS EFFECTS ON THE ELECTRO- CHEMICAL CORROSION BEHAVIOR |
Haiwei HUANG1,Zhenbo WANG1( ),Li LIU2,Xingping YONG3,Ke LU1,4 |
1 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
3 Shenyang Blower Works Group Co. Ltd., Shenyang 110869
4 Herbert Gleiter Institute of Nanoscience, Nanjing University of Science and Technology, Nanjing 210094 |
引用本文:
黄海威, 王镇波, 刘莉, 雍兴平, 卢柯. 马氏体不锈钢上梯度纳米结构表层的形成及其对电化学腐蚀行为的影响*[J]. 金属学报, 2015, 51(5): 513-518.
Haiwei HUANG,
Zhenbo WANG,
Li LIU,
Xingping YONG,
Ke LU.
FORMATION OF A GRADIENT NANOSTRUCTURED SURFACE LAYER ON A MARTENSITIC STAINLESS STEEL AND ITS EFFECTS ON THE ELECTRO- CHEMICAL CORROSION BEHAVIOR[J]. Acta Metall Sin, 2015, 51(5): 513-518.
| [1] | Lu K, Lu J. J Mater Sci Technol, 1999; 15: 193 | | [2] | Lu K, Lu J. Mater Sci Eng, 2004; A375: 38 | | [3] | Fang T H, Li W L, Tao N R, Lu K. Science, 2011; 331: 1587 | | [4] | Wang Z B, Tao N R, Li S, Wang W, Liu G, Lu J, Lu K. Mater Sci Eng, 2003; A352: 144 | | [5] | Villegas J C, Shaw L L. Acta Mater, 2009; 57: 5782 | | [6] | Huang H W, Wang Z B, Yong X P, Lu K. Mater Sci Technol, 2013; 29: 1200 | | [7] | Pacquentin W, Caron N, Oltra R. Appl Surf Sci, 2014; 288: 34 | | [8] | Li Y, Wang F, Liu G. Corrosion, 2004; 60: 891 | | [9] | Hao Y W, Deng B, Zhong C, Jiang Y M, Li J. J Iron Steel Res Int, 2009; 16: 68 | | [10] | Balusamy T, Sankara Narayanan T S N, Ravichandran K, Park I S, Lee M H. Corros Sci, 2013; 74: 332 | | [11] | Chen T, John H, Xu J, Lu Q, Hawk J, Liu X. Corros Sci, 2013; 77: 230 | | [12] | Wang T, Yu J, Dong B. Surf Coat Technol, 2006; 200: 4777 | | [13] | Huang R, Han Y. Mater Sci Eng, 2013; C33: 2353 | | [14] | Jelliti S, Richard C, Retraint D, Roland T, Chemkhi M, Demangel C. Surf Coat Technol, 2013; 224: 82 | | [15] | Raja K S, Namjoshi S A, Misra M. Mater Lett, 2005; 59: 570 | | [16] | Wang X Y, Li D Y. Electrochim Acta, 2002; 47: 3939 | | [17] | Huang H W, Wang Z B, Lu J, Lu K. Acta Mater, 2015; 87: 150 | | [18] | Zhou L, Liu G, Ma X L, Lu K. Acta Mater, 2008; 56: 78 | | [19] | Wang L M, Wang Z B, Lu K. Acta Mater, 2011; 59: 3710 | | [20] | Arifvianto B, Suyitno, Mahardika M. Appl Surf Sci, 2012; 258: 4538 | | [21] | Bagherifard S, Guagliano M. Eng Fract Mech, 2012; 81: 56 | | [22] | Meng G Z, Li Y, Wang F H. Electrochim Acta, 2006; 51: 4277 | | [23] | Liu L, Li Y, Wang F H. Acta Metall Sin, 2014; 50: 212 (刘 莉, 李 瑛, 王福会. 金属学报, 2014; 50: 212) | | [24] | Moon J, Ha H Y, Lee T H, Lee C. Mater Chem Phys, 2013; 142: 556 | | [25] | Hara T, Asahi H. ISIJ Int, 2000; 40: 1134 | | [26] | Peyre P, Scherpereel X, Berthe L, Carboni C, Fabbro R, Béranger G, Lemaitre C. Mater Sci Eng, 2000; A280: 294 | | [27] | Sun Y, Bailey R. Surf Coat Technol, 2014; 253: 284 | | [28] | Li W, Li D Y. Acta Mater, 2006; 54: 445 |
|
|