Please wait a minute...
金属学报  2014, Vol. 50 Issue (11): 1367-1376    DOI: 10.11900/0412.1961.2014.00207
  本期目录 | 过刊浏览 |
柱状晶组织HAl77-2铝黄铜的力学性能与加工硬化行为
莫永达1, 姜雁斌1,2, 刘新华1,2, 谢建新1,2()
1 北京科技大学材料先进制备技术教育部重点实验室, 北京 100083
2 北京科技大学现代交通金属材料与加工技术北京实验室, 北京 100083
MECHANICAL PROPERTIES AND WORK HARDENING BEHAVIOR OF COLUMNAR-GRAINED HAl77-2 BRASS
MO Yongda1, JIANG Yanbin1,2, LIU Xinhua1,2, XIE Jianxin1,2()
1 Key Laboratory for Advanced Materials Processing of Ministry of Education, University of Science and Technology Beijing, Beijing 100083
2 Beijing Laboratory of Metallic Materials and Processing for Modern Transportation, University of Science
and Technology Beijing, Beijing 100083
引用本文:

莫永达, 姜雁斌, 刘新华, 谢建新. 柱状晶组织HAl77-2铝黄铜的力学性能与加工硬化行为[J]. 金属学报, 2014, 50(11): 1367-1376.
Yongda MO, Yanbin JIANG, Xinhua LIU, Jianxin XIE. MECHANICAL PROPERTIES AND WORK HARDENING BEHAVIOR OF COLUMNAR-GRAINED HAl77-2 BRASS[J]. Acta Metall Sin, 2014, 50(11): 1367-1376.

全文: PDF(10012 KB)   HTML
摘要: 

利用室温单向拉伸实验、EBSD和TEM等手段, 研究了柱状晶组织HAl77-2铝黄铜的力学性能与加工硬化行为, 探讨了晶粒尺寸对拉伸变形加工硬化速率和塑性变形能力的影响及其机制. 结果表明, 柱状晶组织HAl77-2铝黄铜加工硬化速率-真应变关系曲线第2阶段具有显著上升趋势, 晶内形成平行分布的小角度亚晶界使位错滑移长度减小并阻碍位错运动是加工硬化速率上升的主要原因, 不同于文献报道的等轴晶组织黄铜加工硬化第2阶段形成形变孪晶使滑移长度减小的机制. 随着晶粒尺寸的增大, 柱状晶组织HAl77-2铝黄铜的屈服强度和抗拉强度降低, 而断后伸长率显著增大, 由晶粒尺寸为2.0 mm的70.4%增大到晶粒尺寸为6.0 mm的84.4%. 较高的抗塑性失稳能力和较好的晶内变形均匀性是大晶粒柱状晶试样具有更优塑性变形能力的主要原因.

关键词 : HAl77-2铝黄铜,  柱状晶组织,  力学性能,  加工硬化速率,  晶粒尺寸    
Abstract:

The mechanical properties and work hardening behavior of columnar-grained HAl77-2 brass were investigated by means of room temperature tensile test, EBSD and TEM. The effects of grain size on the work hardening rate and tensile ductility of the alloy were discussed. Some references reported that deformation twinning developed in the equiaxed-grained brass led to a reduction in slip length of dislocation and an increase in the work hardening rate at the second stage in the curve of work-hardening vs strain. In this work, however, the results showed that the low-angle subgrain boundaries distributed parallelly were formed in the columnar grain and reduced the slip length of dislocation at the second stage, which was responsible for the rise of the work hardening rate. With increasing grain size, both the yield strength and ultimate tensile strength of the columnar-grained HAl77-2 brass decreased, but its elongation to failure increased significantly from 70.4% for the grain size of 2.0 mm to 84.4% for the grain size of 6.0 mm. Higher performance to resist the plastic instability and better deformation uniformity mainly contributed to the ductility improvement of the larger-grain-sized columnar-grained HAl77-2 brass.

Key words: HAl77-2 brass    columnar grain    mechanical property    work hardening rate    grain size
收稿日期: 2014-08-02     
ZTFLH:  TG146.1  
基金资助:*国家科技支撑计划项目2011BAE23B00和国家自然科学基金项目51104016 资助
作者简介: null

莫永达, 男, 1987年生, 博士生

图1  定向凝固装置示意图
图2  不同铸型保温温度条件下制备的柱状晶组织铸锭的横、纵截面宏观组织形貌
图3  柱状晶组织HAl77-2铝黄铜室温拉伸工程应力-应变曲线
Grain size / mm ss / MPa sb / MPa d / %
2.0 55 218 70.4
3.2 48 199 75.1
6.0 45 182 84.4
表1  柱状晶组织HAl77-2铝黄铜室温拉伸力学性能
图4  柱状晶组织HAl77-2铝黄铜试样的加工硬化速率变化曲线
图5  晶粒尺寸2.0 mm的柱状晶组织HAl77-2铝黄铜形变显微组织
图6  拉伸变形后柱状晶组织HAl77-2铝黄铜的TEM像
图7  晶粒尺寸6.0 mm的柱状晶组织HAl77-2铝黄铜形变显微组织
图8  不同晶粒尺寸柱状晶组织HAl77-2铝黄铜晶内取向差变化
图9  不同晶粒尺寸试样拉伸断口附近形变显微组织
图10  晶粒尺寸2.0 mm试样拉伸断口附近典型变形组织
图11  晶粒尺寸6.0 mm试样拉伸断口附近典型变形组织
[1] Kazdal Zeytin H. Mater Charact, 2008; 59: 167
[2] Pola A, Gelfi M, Eleonora Depero L, Roberti R. Eng Fail Anal, 2008; 15: 54
[3] Trostmann A, Morin O. Desalin Water Treat, 2010; 22: 299
[4] Mei J, Liu X H, Jiang Y B, Chen S, Xie J X. Int J Min Met Mater, 2013; 20: 748
[5] Huang H Y, Wang Y, Xie J X. Mater Sci Eng, 2014; A596: 103
[6] Wang Y, Huang H Y, Xie J X. Mater Sci Eng, 2011; A530: 418
[7] Xie J X, Wang Y, Huang H Y. Chin J Nonferrous Met, 2011; 21: 2324
[7] (谢建新, 王 宇, 黄海友.中国有色金属学报, 2011; 21: 2324)
[8] Gan C L, Liu X F, Huang H Y, Xie J X. Mater Sci Eng, 2013; A579: 202
[9] Xie J X, Liu X H, Liu X F, Mei J. Chin Pat, 201110210692.9, 2011
[9] (谢建新, 刘新华, 刘雪峰, 梅 俊. 中国专利, 201110210692.9, 2011)
[10] Xiao G H, Tao N R, Lu K. Scr Mater, 2011; 65: 119
[11] Zhang P, An X H, Zhang Z J, Wu S D, Li S X, Zhang Z F, Figueiredo R B, Gao N, Langdonet T G. Scr Mater, 2012; 67: 871
[12] Thompson A W, Baskes M I, Flanagan W F. Acta Mater, 1973; 21: 1017
[13] Hong S I, Laird C. Acta Metall Mater, 1990; 38: 1581
[14] Christian J W, Mahajan S. Prog Mater Sci, 1995; 39: 1
[15] El-Danaf E, Kalidindi S R, Doherty R D. Metall Mater Trans, 1999; 30A: 1223
[16] Dong H, Thompson A W. Metall Trans, 1985; 16A: 1025
[17] Kocks U F, Mecking H. Prog Mater Sci, 2003; 48: 171
[18] Asgari S, El-Danaf E, Kalidindi S R, Doherty R D. Metall Mater Trans, 1997; 28A: 1781
[19] Sakharova N A, Fernandes J V, Vieira M F. Mater Sci Eng, 2009; A507: 13
[20] Engler O,Randle V. Introduction to Texture Analysis: Macrotexture, Microtexture, and Orientation Mapping. 2nd Ed, New York: CRC press, 2009: 392
[21] Dieter G E, Bacon D. Mechanical Metallurgy. 3rd Ed, New York: McGraw-Hill, 1986: 289
[22] Duggan B J, Hatherly M, Hutchinson W B, Wakefield P T. Metall Sci, 1978; 12: 343
[1] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] 张健, 王莉, 谢光, 王栋, 申健, 卢玉章, 黄亚奇, 李亚微. 镍基单晶高温合金的研发进展[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] 郑亮, 张强, 李周, 张国庆. 增/降氧过程对高温合金粉末表面特性和合金性能的影响:粉末存储到脱气处理[J]. 金属学报, 2023, 59(9): 1265-1278.
[4] 张雷雷, 陈晶阳, 汤鑫, 肖程波, 张明军, 杨卿. K439B铸造高温合金800℃长期时效组织与性能演变[J]. 金属学报, 2023, 59(9): 1253-1264.
[5] 陈礼清, 李兴, 赵阳, 王帅, 冯阳. 结构功能一体化高锰减振钢研究发展概况[J]. 金属学报, 2023, 59(8): 1015-1026.
[6] 丁桦, 张宇, 蔡明晖, 唐正友. 奥氏体基Fe-Mn-Al-C轻质钢的研究进展[J]. 金属学报, 2023, 59(8): 1027-1041.
[7] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[8] 李福林, 付锐, 白云瑞, 孟令超, 谭海兵, 钟燕, 田伟, 杜金辉, 田志凌. 初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响[J]. 金属学报, 2023, 59(7): 855-870.
[9] 袁江淮, 王振玉, 马冠水, 周广学, 程晓英, 汪爱英. Cr2AlC涂层相结构演变对力学性能的影响[J]. 金属学报, 2023, 59(7): 961-968.
[10] 吴东江, 刘德华, 张子傲, 张逸伦, 牛方勇, 马广义. 电弧增材制造2024铝合金的微观组织与力学性能[J]. 金属学报, 2023, 59(6): 767-776.
[11] 刘满平, 薛周磊, 彭振, 陈昱林, 丁立鹏, 贾志宏. 后时效对超细晶6061铝合金微观结构与力学性能的影响[J]. 金属学报, 2023, 59(5): 657-667.
[12] 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆. 尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响[J]. 金属学报, 2023, 59(5): 623-635.
[13] 张东阳, 张钧, 李述军, 任德春, 马英杰, 杨锐. 热处理对选区激光熔化Ti55531合金多孔材料力学性能的影响[J]. 金属学报, 2023, 59(5): 647-656.
[14] 李述军, 侯文韬, 郝玉琳, 杨锐. 3D打印医用钛合金多孔材料力学性能研究进展[J]. 金属学报, 2023, 59(4): 478-488.
[15] 吴欣强, 戎利建, 谭季波, 陈胜虎, 胡小锋, 张洋鹏, 张兹瑜. 耐Pb-Bi腐蚀Si增强型铁素体/马氏体钢和奥氏体不锈钢的研究进展[J]. 金属学报, 2023, 59(4): 502-512.