| AH32耐蚀钢显微组织对其腐蚀行为的影响 |
| 郝雪卉1,董俊华1,魏洁1,柯伟1,王长罡1,徐小连2,叶其斌2
|
1. 中国科学院金属研究所, 沈阳 110016
2. 鞍钢股份有限公司 技术中心, 鞍山 114009 |
|
| INFLUENCE OF MICROSTRUCTURE OF AH32 CORROSION RESISTANT STEEL ON CORROSION BEHAVIOR |
| HAO Xuehui1, DONG Junhua1, WEI Jie1, KE Wei1, WANG Changgang1,XU Xiaolian2, YE Qibin2 |
1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2. Technology Center of Angang Steel Co., Ltd., Anshan 114009 |
引用本文:
郝雪卉,董俊华,魏洁,柯伟,王长罡,徐小连,叶其斌. AH32耐蚀钢显微组织对其腐蚀行为的影响[J]. 金属学报, 2012, 48(5): 534-540.
,
,
,
,
,
.
INFLUENCE OF MICROSTRUCTURE OF AH32 CORROSION RESISTANT STEEL ON CORROSION BEHAVIOR[J]. Acta Metall Sin, 2012, 48(5): 534-540.
| [1] Yang M. Encyclopedia Environ Health, 2011; 49: 33[2] King J. Mar Policy, 2005; 29: 235[3] Li P, Li J D, Zhao S L, Kong L Z, Zhai Y C. Fire Saf J, 2005; 40: 331[4] Chen L. Mar Equip/Mater Market, 2009; (1): 31 (陈力. 船舶物资与市场, 2009; (1): 31)[5] Zhang Z G. World Iron Steel, 2008; (6): 60 (张作贵. 世界钢铁, 2008; (6): 60)[6] Performance Standard for Corrosion Resistant for Cargo Oil Tanks of Oil Tankers. IMO, 2010; 53(7): 42[7] Wen Y. Mar Equip/Mater Market, 2008; (4): 29 (文言. 船舶物资与市场, 2008; (4): 29)[8] Soares C G, Garbatov Y, Zayed A, Wang G. Corros Sci, 2008; 50: 3095[9] Shiomi H, Kaneko M, Kashima K, Imamura H. TSCF2007 Shipbuilder Meet. Busan, 2007: 1[10] Sakashita S, Tatsumi A, Imamura H, Ikeda H. Shipbuilding Technol ISSF 2007. Osaka, 2007: 1[11] Kashima K, Tanino Y, Kubo S, Inami A, Miyuki. Shipbuilding Technol ISSF 2007. Osaka, 2007: 5[12] Han D, Jiang Y M, Shi C, Zhao L, Li J. Corros Sci, 2011; 53: 3796[13] Hou B R, Li Y T, Li Y X, Zhang J L. Mater Sci, 2000; 23: 189[14] Guo J, Yang S W, Shang C J, Wang Y, He X L. Corros Sci, 2008; 51: 242[15] Wang X T, Duan J Z, Zhang J, Hou B R. Mater Letts, 2008; 62: 1291[16] Melchers R E. Corros Sci, 2004; 46: 1669[17] Lopez D A, Perez T, Simision S N. Mater Des, 2003; 24: 561[18] Otero E, Pardo A, Utrilla, Saenz E, Perez F J. Mater Charact, 1995; 35: 145[19] Suchanek J, Kuklik V, Zdravecka E. Wear, 2009; 267 :2092[20] Feng G H, Yang G, Yang D J, Bai G Y, Ren Q H, Li Y. Iron Steel, 2000; 35(3): 22 (冯光宏, 杨钢, 杨德江, 向德渊, 任庆海, 李岩. 钢铁, 2000; 35(3): 22)[21] Zhou G F, He X L. Dev Appl Mater, 1999; 14(3): 1 (周桂峰, 贺信莱. 材料开发与应用, 1999; 14(3): 1)[22] Cao C N. Principles of Electrochemistry of Corrosion. Beijing: Chemical Industry Press, 2008: 149 (曹楚南. 腐蚀电化学原理. 北京: 化学工业出版社, 2008: 149)[23] Zhang G X, Si C Y, Yu D W. Phys Test Chem Anal part: Phys Test, 2001; 37(6): 264 (张国星, 斯初阳, 虞敌卫. 理化检验--物理分册, 2001; 37(6): 264)[24] Cleary H J, Greene N D. Corros Sci, 1969; 9(1): 3[25] Lotz U, Sydberger T. Corrosion, 1988; 44: 800 |
|