|
|
|
| 偏析对DZ483镍基高温合金糊状区内液相密度的影响 |
| 封少波,张楠楠,罗兴宏 |
| 中国科学院金属研究所, 沈阳 110016 |
|
| INFLUENCE OF SEGREGATION ON LIQUID DENSITY IN THE MUSHY ZONE OF DZ483 Ni-BASED SUPERALLOY |
| FENG Shaobo, ZHANG Nannan, LUO Xinghong |
| Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
封少波,张楠楠,罗兴宏. 偏析对DZ483镍基高温合金糊状区内液相密度的影响[J]. 金属学报, 2012, 48(5): 541-546.
,
,
.
INFLUENCE OF SEGREGATION ON LIQUID DENSITY IN THE MUSHY ZONE OF DZ483 Ni-BASED SUPERALLOY[J]. Acta Metall Sin, 2012, 48(5): 541-546.
| [1] Pan Q Y, Huang W D, Li Y M, Lin X, Zhou Y H. J Mater Sci Lett,1996; 15: 2112[2] Zhang T, Ren W L, Dong J W, Li X, Ren Z M, Cao G H, Zhong Y B,Deng K, Lei Z S, Guo J T. J Alloys Compd, 2009; 487: 612[3] Liu G, Liu L, Zhao X B, Zhang W G, Jin T, Zhang J, Fu H Z. Acta Metall Sin, 2010; 46: 77 (刘刚, 刘林, 赵新宝, 张卫国, 金涛, 张军, 傅恒志.金属学报, 2010; 46: 77)[4] Shi C X, Zhong Z Y. Acta Metall Sin, 2010; 46: 1281 (师昌绪, 仲增墉. 金属学报, 2010; 46: 1281)[5] Zhang S, Tian S G, Yu H C, Su Y, Yu X F, Yu L L. Acta Metall Sin,2011; 47: 61 (张姝, 田素贵, 于慧臣, 苏勇, 于兴福, 于莉丽. 金属学报, 2011; 47: 61)[6] Gu J P, Beckermann C, Giamei A F. Metall Mater Trans,1997; 28A: 1533[7] Schneider M C, Gu J P, Beckermann C, Boettinger W J, Kattner U R. Metall Mater Trans, 1997; 28A: 1517[8] Auburtin P, Wang T, Cockcroft S L, Mitchell A. Metall Mater Trans,2000; 31B: 801[9] Beckermann C, Gu J P, Boettinger W J. Metall Mater Trans,2000; 31A: 2545[10] Valdes J, King P, Liu X B. Metall Mater Trans,2010; 41A: 2408[11] Amouyal Y, Seidman D N. Acta Mater, 2011; 59: 6729[12] Madison J, Spowart J E, Rowenhorst D J, Aagesen L K,Thornton K, Pollock T M. Metall Mater Trans, 2012; 43A: 369[13] Lu J W, Chen F L. J Cryst Growth, 1996; 165: 137[14] Pollock T M, Murphy W H. Metall Mater Trans, 1996; 27A: 1081[15] Neilson D G, Incropera F P. Warme Stoffubertrag, 1991; 27: 1[16] Du W, Li J G, Fu H Z. Trans Nonferrous Met Soc, 1998; 8: 83[17] Hobbs R A, Tin S, Rae C M F. Metall Mater Trans,2005; 36A: 2761[18] Huang T W, Liu L, Zhang W G, Zhang J, Fu H Z. Acta Metall Sin, 2009; 45: 1225 (黄太文, 刘林, 张卫国, 张军, 傅恒志. 金属学报, 2009; 45: 1225)[19] Long F, Yoo Y S, Seo S M, Jin T, Hu Z Q, Jo C Y. J Mater Sci Technol, 2011; 27: 101[20] Cutler E R, Wasson A J, Fuchs G E. J Cryst Growth,2009; 311: 3753[21] D'Souza N, Lekstrom M, Dong H B. Mater Sci Eng,2008; A490: 258[22] Tin S, Pollock T M. J Mater Sci, 2004; 39: 7199[23] Tin S, Pollock T M. Metall Mater Trans, 2003; 34A: 1953[24] Wang L, Li C Q, Dong J X, Zhang M C. Chem Eng Commun,2009; 196: 754[25] Wang L, Yao Y J, Dong J X, Zhang M C. Chem Eng Commun,2010; 197: 1571[26] Guan X R, Zheng Z, Tong J, Liu E Z, Yu Y S, Zhu Y X,Zhai Y C. Chin J Nonferrous Met, 2009; 19: 272 (管秀荣, 郑志, 佟健, 刘恩泽, 于永泗, 朱耀宵, 翟玉春.中国有色金属学报, 2009; 19: 272)[27] Mukai K, Li Z S, Mills K C. Metall Mater Trans,2005; 36B: 255[28] De Laeter J R, Bohlke J K, De Bievre P, Hidaka H, Peiser H S,Rosman K J R, Taylor P D P. Pure Appl Chem, 2003; 75: 683[29] Li Z S, Mills K C, McLean M, Mukai K. Metall Mater Trans,2005; 36B: 247 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|