| 新型无Ni高N奥氏体不锈钢的低温变形行为 |
| 徐明舟,王建军,刘春明 |
| 东北大学材料各向异性与织构教育部重点实验室, 沈阳 110819 |
|
| LOW TEMPERATURE DEFORMATION BEHAVIOR OF HIGH–NITROGEN NICKEL–FREE AUSTENITIC STAINLESS STEELS |
| XU Mingzhou, WANG Jianjun, LIU Chunming |
| Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819 |
引用本文:
徐明舟 王建军 刘春明. 新型无Ni高N奥氏体不锈钢的低温变形行为[J]. 金属学报, 2011, 47(10): 1335-1341.
,
,
.
LOW TEMPERATURE DEFORMATION BEHAVIOR OF HIGH–NITROGEN NICKEL–FREE AUSTENITIC STAINLESS STEELS[J]. Acta Metall Sin, 2011, 47(10): 1335-1341.
| [1] Cheng X N, Dai Q X. The Design and Control of Austenitic Stainless Steel. Beijing: National Defense IndustryPress, 2005: 3(程晓农, 戴起勋. 奥氏体钢设计与控制. 北京: 国防工业出版社, 2005: 3)[2] Mudali U K, Raj B, translated by Li J, Huang Y H. High Nitrogen Steels and Stainless Steels, Manufacturing, Properties and Applications. Beijing: Chemical Industry Press, 2006: 5(Mudali U K, Raj B著, 李晶, 黄运华 译. 高氮钢和不锈钢--生产、性能与应用. 北京: 化学工业出版社, 2006: 5)[3] Ilola R J, Hänninen H E, Ullakko K M. ISIJ Int, 1996; 36: 873[4] Tomota Y, Endo S. ISIJ Int, 1990; 30: 656[5] Gavriljuk V G, Sozinova A L, Foct J, Petrov J N, Polushkin Y A. Acta Mater, 1998; 46: 1157[6] Milititsky M, Matlock D K, Regully A, Dewispelaere N, Penning J, Hanninen H. Mater Sci Eng, 2008; A496: 189[7] Tomoto Y, Xia Y, Inoue K. Acta Mater, 1998; 46: 1577[8] Ishizaka J, Orita K, Terao K. Tetsu Hagan´e, 1992; 78: 1846[9] Tobler R L, Leyn D. Metall Mater Trans, 1988; 19A: 1626[10] Ojima M, Adachi Y, Tomota Y, Ikeda K, Katada Y. J Jpn Inst Met, 2009; 73: 283[11] Milititsky M, Matlock D K, Regully A. Mater Sci Eng, 2008; A496: 189[12] Saller G, Hahn K S, Scheu C, Clemens H. Mater Sci Eng, 2006; A427: 246[13] Liu S X, Liu X M, Liu R, Wang C X, Xing F. J Iron Steel Res, 2005; 17: 40(刘树勋, 刘宪民, 刘蕤, 王春旭, 邢峰. 钢铁研究学报, 2005; 17: 40)[14] Simmons J W. Acta Mater, 1997; 45: 2467[15] Breedis J, Robertson W. Acta Metall, 1962; 10: 1077[16] Lee T H, Oh C S, Kim S J. Scr Mater, 2008; 58: 110[17] Liu S Y, Liu D Y, Liu S C. J Mater Sci, 2007; 42: 7514[18] Cheng X N, Dai Q X. The Design and Control of Austenitic Stainless Steel. Beijing: National Defense Industry Press, 2005: 28(程晓农, 戴起勋. 奥氏体钢设计与控制. 北京: 国防工业出版社, 2005: 28)[19] Gavriljuk V G, Berns H. High Nitrogen Steels. Berlin: Springer, 1999: 192[20] Kibey S, Liu J B, Curtis M J, Johnson D D, Sehitoglu H. Acta Mater, 2006; 54: 2991[21] Hu B F, Jia C C. Acta Metall Sin, 2001; 37: 703(胡本芙, 贾成厂. 金属学报, 2001; 37: 703)[22] Hübner W, Pyzalla A, Assmus K, Wild E, Wroblewski T. Wear, 2003; 255: 476[23] Gulyaev A P, Lebedev D V, Gadzhibalaev G A. Met Sci Heat Treat, 1973; 15: 1051[24] Wang S T. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2008(王松涛. 中国科学院金属研究所博士学位论文, 沈阳, 2008)[25] Byun T S, Hashimoto N, Farrell K. Acta Mater, 2004; 52:3889[26] Wang W, Yan W, Yang K, Shan Y Y. J Mater Eng Perform,2010; 19: 1214 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|