| 人工模拟海洋大气环境下Sn-0.7Cu无铅焊料的点蚀行为及微量Ga的影响 |
| 颜忠,冼爱平 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 |
|
| PITTING CORROSION BEHAVIOR OF Sn–0.7Cu LEAD–FREE ALLOY IN SIMULATED MARINE ATMOSPHERIC ENVIROMENT AND THE EFFECT OF TRACE Ga |
| YAN Zhong, XIAN Aiping |
| Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
颜忠 冼爱平. 人工模拟海洋大气环境下Sn-0.7Cu无铅焊料的点蚀行为及微量Ga的影响[J]. 金属学报, 2011, 47(10): 1327-1334.
,
.
PITTING CORROSION BEHAVIOR OF Sn–0.7Cu LEAD–FREE ALLOY IN SIMULATED MARINE ATMOSPHERIC ENVIROMENT AND THE EFFECT OF TRACE Ga[J]. Acta Metall Sin, 2011, 47(10): 1327-1334.
| [1] Abtew M, Selvaduray G. Mater Sci Eng, 2000; 27R: 95[2] Rizvil M J, Bailey C, Chan Y C, Lu H. J Alloys Compd,2007; 438: 116[3] Lin C H, Chen S W, Wang C H. J Electron Mater, 2002;31: 907[4] Ning B, Chen X, Zhou F. J Electron Mater, 2008; 37: 1012[5] Andersson C, Sun P, Liu J. J Alloys Compd, 2008; 457:97[6] Ho C E, Yang S C, Kao C R. J Mater Sci: Mater Electron,2007; 18: 155[7] Nishikawa H, Piao J Y, Takemoto T. J Electron Mater,2006; 35: 1127[8] Jang J W, Ramanathan L N. J Appl Phys, 2008; 103:123506[9] Hasiao Y H, Tseng H W, Liu C Y. J Electron Mater, 2009;38: 2573[10] Liu M, Xian A P. J Electron Mater, 2009, 38: 2353[11] Liang S W, Chen C, Han J K, Xu L H, Tu K N, Lai Y S.J Appl Phys, 2010; 107: 093715[12] Xian A P, Gong G L. J Electron Mater, 2007; 36: 1669[13] Gong G L, Xian A P. Acta Metall Sin, 2007; 43: 759(贡国良, 冼爱平. 金属学报, 2007; 43: 759)[14] Wanees S A, Mohamed A E, Azeem M A, Fatah A N. Int J Electrochem Sci, 2008; 3: 1005[15] Wu B Y, Chan Y C, Alam M O. J Mater Res, 2006; 21: 62[16] Hassan H H, Fahmy K. Int J Electrochem Sci, 2008; 3: 29[17] Li D Z, Conway P P, Liu C Q. Corros Sci, 2008; 50: 995[18] Mohanty U S, Lin K L. Corros Sci, 2006; 48: 662[19] Fazioa E, Neria F, Ruggeria R, Sabatinob G, Trussoc S, Manninod G. Appl Surf Sci, 2011; 257: 2520[20] Morimoto H, Tatsumisago M, Minami T. Electrochem Solid–State Lett, 2001; 4A: 16[21] Dolbec R, ElKhakani M A, Serventi A M, Trudeau M, Saint–Jacques R G. Thin Solid Films, 2002; 49: 230[22] Fan H Y, Wang G N, Hu L L. Solid–State Sci, 2009; 11: 2065[23] Chang H, Chen H T, Li M Y, Wang N, Fu Y G. J Electron Mater, 2009; 38: 2170[24] Wagner C. J Chem Phys, 1950; 18: 62 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|