| 纳米压痕法测量Cu膜的硬度和弹性模量 |
| 黎业生1), 汪伟2) |
1) 江西理工大学材料与化学工程学院, 赣州 341000
2) 中国科学院金属研究所材料科学国家(联合)实验室, 沈阳 110016 |
|
| MEASUREMENTS OF HARDNESS AND ELASTIC MODULUS OF Cu THIN FILM BY MEANS OF NANOINDENTATION |
| LI Yesheng1), WANG Wei2) |
1) School of Materials Science and Chemical Engineering, Jiangxi University of Science and Technology, Ganzhou 341000
2) Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
黎业生 汪伟. 纳米压痕法测量Cu膜的硬度和弹性模量[J]. 金属学报, 2010, 46(9): 1098-1102.
,
.
MEASUREMENTS OF HARDNESS AND ELASTIC MODULUS OF Cu THIN FILM BY MEANS OF NANOINDENTATION[J]. Acta Metall Sin, 2010, 46(9): 1098-1102.
| [1] Tsui T Y, Vlassak J, Nix W D. J Mater Res, 1999; 14: 2204
[2] Page T F, Pharr G M, Hay J C, Oliver W C, Lucas B N, Herbert E, Riester L. In: Moody N R, Gerberich W W, Burnham N eds., Fundamentals of Nanoindentation and Nanotrobology. Warrendale, PA: Materials Research Society, 1998: 53
[3] Zhang G P, Liu Y, Wang W, Tan J. Appl Phy Lett, 2006; 88: 2
[4] Fang T H, Chang W J. Microelectron Eng, 2003; 65: 231
[5] Hong S H, Kim K S, Kim Y M, Hahn J H, Lee C S, Park J H. Compos Sci Technol, 2005; 65: 1401
[6] Beegan D, Chowdhury S, Laugier M T. Surf Coat Technol, 2007; 201: 5804
[7] Chang S Y, Lee Y S, Chang T K. Mater Sci Eng, 2006; A423: 52
[8] Han S M, Saha R, Nix W D. Acta Mater, 2006; 54: 1571
[9] Nix W D, Gao H. J Mech Phys Solids, 1998; 46: 411
[10] MeyersMA, MishraA, BensonD J. Prog Mater Sci, 2006; 51: 427
[11] Wu F F, Zhang Z F, Mao S X. Acta Mater, 2009; 57: 257
[12] Zhang G P, Wang W, Zhang B, Tan J, Liu C S. Scr Mater, 2005; 52: 1147
[13] Li Y S, Li H, Ma Y H, Xie J, Wang J J. Rare Met Mater Eng, 2009; 38: 147
(黎业生, 李洪, 马永红, 谢 骏, 王家佳. 稀有金属材料与工程, 2009; 38: 147)
[14] Chen X, Vlassak J J. J Mater Res, 2001; 16: 2974
[15] Saha R, Nix W D. Acta Mater, 2002; 50: 23
[16] Wang W, Lu K. Philos Mag, 2006; 86: 5309
[17] Chen J, Wang W, Lu L, Lu K. Acta Metall Sin, 2001; 37: 1179
(陈吉, 汪 伟, 卢 磊, 卢 柯. 金属学报, 2001; 37: 1179)
[18] Chen J, Lu L, Lu K. Scr Mater, 2006; 54: 1913
[19] Zhang T H, to be published
(张泰华, 待发表) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|