Please wait a minute...
金属学报  2010, Vol. 46 Issue (9): 1098-1102    DOI: 10.3724/SP.J.1037.2009.00859
  论文 本期目录 | 过刊浏览 |
纳米压痕法测量Cu膜的硬度和弹性模量
黎业生1), 汪伟2)
1) 江西理工大学材料与化学工程学院, 赣州 341000
2) 中国科学院金属研究所材料科学国家(联合)实验室, 沈阳 110016
MEASUREMENTS OF HARDNESS AND ELASTIC MODULUS OF Cu THIN FILM BY MEANS OF NANOINDENTATION
LI Yesheng1), WANG Wei2)
1) School of Materials Science and Chemical Engineering, Jiangxi University of Science and Technology, Ganzhou 341000
2) Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
引用本文:

黎业生 汪伟. 纳米压痕法测量Cu膜的硬度和弹性模量[J]. 金属学报, 2010, 46(9): 1098-1102.
, . MEASUREMENTS OF HARDNESS AND ELASTIC MODULUS OF Cu THIN FILM BY MEANS OF NANOINDENTATION[J]. Acta Metall Sin, 2010, 46(9): 1098-1102.

全文: PDF(608 KB)  
摘要: 

利用纳米压痕技术对沉积在Si衬底上1 μm厚Cu膜的硬度H和弹性模量$E$进行了测量. 结果表明, 由单一刚度测量(SSM) 和连续刚度测量(CSM) 2种方法测得的$E$值基本一致. 然而由于Cu膜的室温蠕变行为显著, 用SSM 方法测得薄膜的H值显著小于用CSM方法测得的$H$值. 对加载曲线进行分析表明, 在压入深度为528-587 nm时薄膜硬度显示基体效应, 压入深度与薄膜厚度的比值与有限元计算结果吻合较好.

关键词 : 纳米压痕,  Cu膜,  硬度,  弹性模量    
Abstract:

Hardness (H) and elastic modulus (E) of 1 $\mu$m thick Cu film deposited on Si substrate were measured by means of nanoindentation technique. The E value of Cu film obtained by using single stiffness measurement (SSM) is consistent with that obtained from continuous stiffness measurement (CSM). However, the H value obtained from SSM is much smaller than that from CSM because of occurrence of significant creep during the holding period at ambient temperature. The analysis of loading curves shows that the substrate effect on hardness measurement appears as the indentation depth is about 528-587 nm, indicating the ratio of penetration depth to film thickness (about 0.5) is consistent with the finite element calculation.

Key words: nanoindentation    Cu film    hardness    elastic modulus
收稿日期: 2009-12-24     
基金资助:

国家自然科学基金项目50571097和江西省自然科学基金项目2007GZC0712资助

作者简介: 黎业生, 男, 1966年生, 教授

[1] Tsui T Y, Vlassak J, Nix W D. J Mater Res, 1999; 14: 2204
[2] Page T F, Pharr G M, Hay J C, Oliver W C, Lucas B N, Herbert E, Riester L. In: Moody N R, Gerberich W W, Burnham N eds., Fundamentals of Nanoindentation and Nanotrobology. Warrendale, PA: Materials Research Society, 1998: 53
[3] Zhang G P, Liu Y, Wang W, Tan J. Appl Phy Lett, 2006; 88: 2
[4] Fang T H, Chang W J. Microelectron Eng, 2003; 65: 231
[5] Hong S H, Kim K S, Kim Y M, Hahn J H, Lee C S, Park J H. Compos Sci Technol, 2005; 65: 1401
[6] Beegan D, Chowdhury S, Laugier M T. Surf Coat Technol, 2007; 201: 5804
[7] Chang S Y, Lee Y S, Chang T K. Mater Sci Eng, 2006; A423: 52
[8] Han S M, Saha R, Nix W D. Acta Mater, 2006; 54: 1571
[9] Nix W D, Gao H. J Mech Phys Solids, 1998; 46: 411
[10] MeyersMA, MishraA, BensonD J. Prog Mater Sci, 2006; 51: 427
[11] Wu F F, Zhang Z F, Mao S X. Acta Mater, 2009; 57: 257
[12] Zhang G P, Wang W, Zhang B, Tan J, Liu C S. Scr Mater, 2005; 52: 1147
[13] Li Y S, Li H, Ma Y H, Xie J, Wang J J. Rare Met Mater Eng, 2009; 38: 147
(黎业生, 李洪, 马永红, 谢 骏, 王家佳. 稀有金属材料与工程, 2009; 38: 147)
[14] Chen X, Vlassak J J. J Mater Res, 2001; 16: 2974
[15] Saha R, Nix W D. Acta Mater, 2002; 50: 23
[16] Wang W, Lu K. Philos Mag, 2006; 86: 5309
[17] Chen J, Wang W, Lu L, Lu K. Acta Metall Sin, 2001; 37: 1179
(陈吉, 汪 伟, 卢 磊, 卢 柯. 金属学报, 2001; 37: 1179)
[18] Chen J, Lu L, Lu K. Scr Mater, 2006; 54: 1913
[19] Zhang T H, to be published
(张泰华, 待发表)

[1] 王海峰, 张志明, 牛云松, 杨延格, 董志宏, 朱圣龙, 于良民, 王福会. 前置渗氧对TC4钛合金低温等离子复合渗层微观结构和耐磨损性能的影响[J]. 金属学报, 2023, 59(10): 1355-1364.
[2] 梁琛, 王小娟, 王海鹏. 快速凝固Ti-Al-Nb合金B2相形成机制与显微力学性能[J]. 金属学报, 2022, 58(9): 1169-1178.
[3] 王韬, 龙弟均, 余黎明, 刘永长, 李会军, 王祖敏. 超高压烧结制备14Cr-ODS钢及微观组织与力学性能[J]. 金属学报, 2022, 58(2): 184-192.
[4] 朱彬, 杨兰, 刘勇, 张宜生. 基于纳米压痕逆算法的热冲压马氏体/贝氏体双相组织的微观力学性能[J]. 金属学报, 2022, 58(2): 155-164.
[5] 项兆龙, 张林, XIN Yan, 安佰灵, NIU Rongmei, LU Jun, MARDANI Masoud, HAN Ke, 王恩刚. Cr含量对FeCrCoSi永磁合金调幅分解组织及其性能的影响[J]. 金属学报, 2022, 58(1): 103-113.
[6] 胡龙, 王义峰, 李索, 张超华, 邓德安. 基于SH-CCT图的Q345钢焊接接头组织与硬度预测方法研究[J]. 金属学报, 2021, 57(8): 1073-1086.
[7] 兰亮云, 孔祥伟, 邱春林, 杜林秀. 基于多尺度力学实验的氢脆现象的最新研究进展[J]. 金属学报, 2021, 57(7): 845-859.
[8] 孙小钧, 何杰, 陈斌, 赵九洲, 江鸿翔, 张丽丽, 郝红日. Fe含量对Zr60Cu40-xFex相分离非晶合金组织结构、电阻性能和纳米压痕行为的影响[J]. 金属学报, 2021, 57(5): 675-683.
[9] 曹庆平, 吕林波, 王晓东, 蒋建中. 物理气相沉积制备金属玻璃薄膜及其力学性能的样品尺寸效应[J]. 金属学报, 2021, 57(4): 473-490.
[10] 王明康, 苑峻豪, 刘宇峰, 王清, 董闯, 张中伟. Ti对Zr-Nb二元合金β结构稳定性和力学性能的影响[J]. 金属学报, 2021, 57(1): 95-102.
[11] 童文辉, 张新元, 李为轩, 刘玉坤, 李岩, 国旭明. 激光工艺参数对TiC增强钴基合金激光熔覆层组织及性能的影响[J]. 金属学报, 2020, 56(9): 1265-1274.
[12] 张林, 郭晓, 高建文, 邓安元, 王恩刚. 电磁搅拌对TiB2颗粒增强钢组织和力学性能的影响[J]. 金属学报, 2020, 56(9): 1239-1246.
[13] 刘震鹏, 闫志巧, 陈峰, 王顺成, 龙莹, 吴益雄. 金刚石工具用Cu-10Sn-xNi合金的制备和性能表征[J]. 金属学报, 2020, 56(5): 760-768.
[14] 刘继召, 黄鹤飞, 朱振博, 刘阿文, 李燕. 氙离子辐照后Hastelloy N合金的纳米硬度及其数值模拟[J]. 金属学报, 2020, 56(5): 753-759.
[15] 邓聪坤,江鸿翔,赵九洲,何杰,赵雷. Ag-Ni偏晶合金凝固过程研究[J]. 金属学报, 2020, 56(2): 212-220.