| 时效析出相对铸造2507超级双相不锈钢力学及耐蚀性能的影响 |
| 向红亮,刘东,阮方如,何福善,黄利光 |
| 福州大学机械工程及自动化学院, 福州 350108 |
|
| EFFECTS OF PRECIPITATION FOR AGING ONMECHANICAL AND CORROSION RESISTANCE PROPERTIES OF CAST 2507 SUPER DUPLEX STAINLESS STEEL |
| XIANG Hongliang, LIU Dong, RUAN Fangru, HE Fushan, HUANG Liguang |
| School of Mechanical Engineering and Automation, Fuzhou University, Fuzhou 350108 |
引用本文:
向红亮 刘东 阮方如 何福善 黄利光. 时效析出相对铸造2507超级双相不锈钢力学及耐蚀性能的影响[J]. 金属学报, 2010, 46(8): 941-945.
,
,
,
,
.
EFFECTS OF PRECIPITATION FOR AGING ONMECHANICAL AND CORROSION RESISTANCE PROPERTIES OF CAST 2507 SUPER DUPLEX STAINLESS STEEL[J]. Acta Metall Sin, 2010, 46(8): 941-945.
| [1] Wu J. Corrosion & Protection in Petrochem Industry, 1996; 13: 6
(吴玖.石油化工腐蚀与防护. 1996; 13: 6)
[2] Graham G. 2th Int Conf on Duplex Stainless Steel. Beijing: Stainless steel council China Special steel Enterprises association, 2006:218
[3] Benson M, Snis M. 2th Int Conf on Duplex Stainless Steel. Beijing: Stainless steel council China Special steel Enterprises association, 2006:17
[4] Erich F, translated by Su Z X. Welding metallurgy of stainless steel, Beijing: Chemical Industry Press, 2004: 74
(Erich F著, 栗卓新译. 不锈钢焊接冶金. 北京: 化学工业出版社, 2004: 74)
[5] Henrik S, Rolf S. Mater Sci Eng, 2007, 444A: 271
[6] Elmer J W, Palmer T A. Mater Sci Eng, 2007, 459 A: 151
[7] Russell S W, Lundin C D. Final Report for the Development of Energy: the Development of Qualification Standards for Cast Duplex Stainless Steel the University of Tennessee Knoxville, 2005,2:8
[8] Ezuber H M,. El-Houd A,. El-Shawesh F. Desalination. 2007, 207: 268
[9]Huang C, Shih C. Mater Sci Eng, 2005,A402: 66
[10] Chen J Y, Yang Z Y, Yang W, Su J, Luo F H. J Iron Steel Res, 2006; 18:2
(陈嘉砚, 杨卓越, 杨武, 苏杰, 罗丰华. 钢铁研究学报. 2006, 18: 1)
[11] Long J M, Fan A M. Phys Test, 1997; 15(1):1
(龙晋明, 樊爱民. 物理测试. 1997; 15(1):1)
[12] Otarola T, Hollner S, Bonnefois B. Eng Fail Anal, 2005; 12: 930
[13] Marcelo M, Leonardo R F. Mater Char. 2007; doi:10.1016/j.matchar.2007.02.010.
[14] Pohl M, Storz O, Glogowski T. Mater Sci Eng, 2007, 58: 66.
[15].Redja A,. Proult A,. Donnadieu P,. Morniroli J. J Mater Sci, 2004; 39: 2386.
[16] Takuyo Y, Satoshi O, Hisashi K. J Nuclear Mater. 2006, 350: 47
[17] Xiang H L, He F S, Liu D. Acta Metall Sin, 2009; 45:1456
(向红亮, 何福善, 刘东. 金属学报, 2009; 45: 1456
[18] Jang Y, Kim S, Lee J. Metall Mater Trans, 2005; 36A: 1229
[19] Chiu P K, Wang S.H, Yang J R, Weng K L, Jason F. Mater Chem Phys, 2006; 98: 103
[20] Zhong Q P. Zhao Z H. Fractography. Beijing: High Education Press, 2006: 202
(钟群鹏, 赵子华. 断口学. 北京: 高等教育出版社, 2006:202)
[21] Tavares S S, Terra V. F, Neto P, Lima, D E. Matos. Microchimica Acta. 2005, 40: 4025
[22] Xiang H L, Huang W L, Liu D, He F S. Acta Metall Sin. 2010, 46:304
(向红亮, 黄伟林, 刘东, 何福善. 金属学报. 2010, 46: 304)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|