| 晶粒尺寸对冷轧退火纯Cu晶界特征分布的影响 |
| 蔡正旭1), 王卫国1), 方晓英1), 郭红2) |
1) 山东理工大学机械工程学院, 淄博 255049
2) 山东理工大学分析测试中心, 淄博 255049 |
|
| EFFECT OF GRAIN SIZE ON THE GRAIN BOUNDARY CHARACTER DISTRIBUTIONS OF COLD ROLLED AND ANNEALED PURE COPPER |
| CAI Zhengxu1), WANG Weiguo1), FANG Xiaoying1), GUO Hong2) |
1) School of Mechanical Engineering, Shandong University of Technology, Zibo 255049
2) Center of Testing and Analysis, Shandong University of Technology, Zibo 255049 |
引用本文:
蔡正旭 王卫国 方晓英 郭红. 晶粒尺寸对冷轧退火纯Cu晶界特征分布的影响[J]. 金属学报, 2010, 46(7): 769-774.
,
,
.
EFFECT OF GRAIN SIZE ON THE GRAIN BOUNDARY CHARACTER DISTRIBUTIONS OF COLD ROLLED AND ANNEALED PURE COPPER[J]. Acta Metall Sin, 2010, 46(7): 769-774.
| [1] |
Watanabe T. Res Mech, 1984; 11: 47 |
| [2] |
Palumbo G, Erb U. MRS Bull, 1999; 11: 27 |
| [3] |
Kumar B R, Das S K, Mahato B, Das A, Chowdhury S G. Mater Sci Eng, 2007; A454–455: 239 |
| [4] |
Wang W G. Mater Sci Forum, 2007; 539–543: 3389 |
| [5] |
Randle V. Acta Mater 1999, 47,4187 |
| [6] |
Shimada M, Kokawa H, Wang Z J, Sato, Y S, Karibe I. Acta Mater 2002, 50,2331 |
| [7] |
Michiuchi M, Kokawa H, Wang Z J, Sato Y S, Sakai K. Acta Mater 2006, 54,5179 |
| [8] |
Fang X Y, Zhang K, Guo H, Wang W G, Zhou B X. Mater Sci Eng, 2008; A487: 7 |
| [9] |
Xia S, Zhou B X, Chen W J, Wang W G. Scr Mater 2006, 54,2019 |
| [10] |
Wang W G, Zhou B X, Feng L. Acta Metall Sin, 2006; 42: 715 |
| |
王卫国, 周邦新, 冯 柳. 金属学报 2006, 42,715 浏览 |
| [11] |
Wang W G, Guo H. Mater Sci Eng, 2007; A445–446: 199 |
| [12] |
Humphreys F J, Hatherly M. Recrystallization and related annealing phenomenon. Oxford: Elsevier Ltd, 2004 |
| [13] |
Fang X Y, Wang W G, Cai Z X, Guo H, Zhou B X. Mater Sci Eng, 2010; A527: 1571 |
| [14] |
Wang W G, Yin F X, Guo H, Li H, Zhou B X. Mater Sci Eng, 2008; A491: 199 |
| [15] |
Zhang X, Wang W G, Guo H, Jiang Y. Acta Metall Sin, 2007; 43: 454 |
| |
张欣, 王卫国, 郭红, 姜英. 金属学报 2007, 43,454 浏览 |
| [16] |
Wang W G, Zhou B X, Guo H. Mater Sci Forum, 2010; 638–642: 2864 |
| [17] |
Cai Z X, Wang W G, Fang X Y, Guo H. Chin J Stereology Image Analysis (in press). |
| [18] |
(蔡正旭, 王卫国, 方晓英, 郭 红. 中国体视学与图像分析, 组版中) |
| [19] |
Brandon D G. Acta Metall, 1964; 14: 1479 |
| [20] |
Rohrer G S, Saylor D M, Dasher B E, Adams B L. Z Metall, 2004; 95: 197 |
| [21] |
Saylor D M, Dasher B E, Adams B L. Metall Mater Trans, 2004; 35A: 1981 |
| [22] |
Wright S I, Larsen R J.. J Microsc 2002, 205,245 |
| [23] |
Miura H, Sakai T, Jonas J J. Scr Mater, 2006; 55 167 |
| [24] |
Zhang Y B, Liu Q, Godfrey A, Liu W. Acta Metall Sin, 2009; 45: 1159 |
| |
张玉彬, 刘庆, Godfrey A, 刘伟. 金属学报 2009, 45,1159 浏览 |
| [25] |
Wang W G. Chin J Stereology Image Analysis, 2007; 12: 239 |
| |
(王卫国. 中国体视学与图像分析, 2007; 12: 239) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|