林艳丽 何祝斌 苑世剑. 管材自由胀形时胀形区轮廓形状的影响因素[J]. 金属学报, 2010, 46(6): 729-735.
,
,
.
THE FACTORS AFFECTING THE PROFILE OF MIDDLE BULGE REGION DURING TUBE BULGE TEST[J]. Acta Metall Sin, 2010, 46(6): 729-735.
| [1] Dohamnn F, Bohm A, Dudziak K U. In: Wang Z R ed., Advanced Technology of Plasticity 1993–Proc 4th Int Conf on Technology of Plasticity, Beijing: International Academic Publishers, 1993: 447
[2] Yuan S J, Liu G, He Z B, Wang X S, Han C, Teng B G, Xu Y C. Digital Manuf Sci, 2008; 6(4): 2
(苑世剑, 刘钢, 何祝斌, 王小松, 韩 聪, 滕步刚, 徐永超. 数字制造科学, 2008; 6(4): 2)
[3] Sokolowski T, Gerke K, Ahmetoglu M, Altan T. J Mater Process Technol, 2000; 98: 34
[4] Price E G. Can Metall Q, 1972; 11: 129
[5] Arsene S, Bai J B. J Test Eval, 1996; 24: 386
[6] Wang H, Bouchard R, Eagleson R. J Test Eval, 2002; 30: 382
[7] He Z B, Yuan S J, Cha W W, Liang Y C. Acta Metall Sin, 2008; 44: 423
(何祝斌, 苑世剑, 查微微, 梁迎春. 金属学报, 2008; 44: 423)
[8] Woo D M. J Eng Mater Technol, 1973; 95: 219
[9] Woo D M, Hawkes P J. J Inst Met, 1966; 96: 357
[10] Fuchizawa S. In: Lange K ed., Advanced Technology of Plasticity 1987–Proc 2th Int Conf on Technology of Plasticity, Berlin: Springer Verlag, 1987: 727
[11] Fuchizawa S, Narazaki M, Yuki H. In: Wang Z R ed., Advanced Technology of Plasticity 1993–Proc 4th Int Conf on Technology of Plasticity, Beijing: International Academic Publishers, 1993: 488
[12] Koc M, Aue–u–lan Y, Altan T. Int J Mach Tool Manuf, 2001; 41: 761
[13] Hwang Y M, Lin Y K. J Mater Process Technol, 2002; 126: 821
[14] Hwang Y M, Lin Y K, Altan T. Int J Mach Tool Manuf, 2007; 47: 343
[15] Hwang Y M, Lin Y K. J Eng Mater Technol, 2007; 129, 414
[16] Strano M, Altan T. J Mater Process Technol, 2004; 146: 92
[17] Bortot P, Ceretti E, Giardini C. J Mater Process Technol, 2008; 203: 381 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|