| 双水口注流连铸复合钢坯结晶器流场和合金元素浓度场研究 |
| 李宝宽; 代凤羽; 齐凤升; 杨冉 |
| 东北大学材料与冶金学院; 沈阳 110819 |
|
| FLOW FIELD AND CONCENTRATION FIELD OF ALLOYING ADDITION IN CLAD STEEL CONTINUOUS CASTING MOLD USING LONG AND SHORT NOZZLES |
| LI Baokuan; DAI Fengyu; QI Fengsheng; YANG Ran |
| School of Materials and Metallurgy; Northeastern University; Shenyang 110819 |
引用本文:
李宝宽 代凤羽 齐凤升 杨冉. 双水口注流连铸复合钢坯结晶器流场和合金元素浓度场研究[J]. 金属学报, 2010, 46(6): 736-742.
,
,
,
.
FLOW FIELD AND CONCENTRATION FIELD OF ALLOYING ADDITION IN CLAD STEEL CONTINUOUS CASTING MOLD USING LONG AND SHORT NOZZLES[J]. Acta Metall Sin, 2010, 46(6): 736-742.
| [1] Wang Y D, Wang L X, Li G P. China Metall, 2001; 2: 5
(王一德, 王立新, 李国平. 中国冶金, 2001; 2: 5)
[2] Erkkila P. Ironmaking Steelmaking, 2004; 31: 277
[3] Manokhin A L, Doroshev Y F, Rovenskaya T V, Bykov A A, Nechaeve L S. Steel USSR, 1978; 12: 673
[4] Xie J X. Mater Eng, 2000; 4: 38
(谢建新. 材料工程, 2000; 4: 38)
[5] Takeuchi E, Zeze M, Tanaka H, Harada H, Mizoguchi S. Ironmaking Steelmaking, 1997; 24: 257
[6] Yasuda H, Ohnaka I. CAMP ISIJ, 1999; 12: 27
[7] Li B K, Okane T, Umeda T. Metall Mater Trans, 2001; 32B: 1053
[8] Li B K, Tsukihashi F. ISIJ Int, 2001; 41: 844
[9] Li B K, Okane T, Umeda T. Metall Mater Trans, 2000; 31B: 1491
[10] Harada H, Takeuchi E, Zeze M, Tanaka H. Appl Math Model, 1998; 22: 873
[11] Zeze M, Harada H, Takeuchi E. ISIJ Int, 1999; 39: 563
[12] Kozuka T. CAMP ISIJ, 1999; 12: 18
[13] Zheng H X, Li B K, Chang Z Z. Acta Metall Sin, 2001; 37: 877
(郑红霞, 李宝宽, 昌泽舟. 金属学报, 2001; 37: 877)
[14] Qian Z D, Li BW, Li D H,Wang E G, He J C. Acta Metall Sin, 2001; 37: 1223
(钱忠东, 李本文, 李东辉, 王恩刚, 赫冀成. 金属学报, 2001; 37: 1223)
[15] Hwang Y S, Cha P R, Nam H S. ISIJ Int, 1997; 37: 1112 |
|