| 25钢在海水中的微生物单因素腐蚀 |
| 吴进怡1; 3; 柴柯1; 肖伟龙1;杨雨辉2; 韩恩厚3 |
1. 海南大学材料与化工学院海南优势资源化工材料应用技术教育部重点实验室; 海口 570228
2. 海南大学农学院; 海口 570228
3. 中国科学院金属研究所金属腐蚀与防护国家重点实验室; 沈阳 110016 |
|
| THE SINGLE EFFECT OF MICROBE ON THE CORROSION BEHAVIORS OF 25 STEEL IN SEAWATER |
| WU Jinyi 1; 3; CHAI Ke 1; XIAO Weilong 1; YANG Yuhui 2; Han Enhou 3 |
1. Key Laboratory of Ministry of Education for Application Technology of Chemical Materials in Hainan Superior Resources; Material and Chemical Engineering College; Hainan University; Haikou 570228
2. Agricultural College; Hainan University; Haikou 570228
3. State Key Laboratory for Corrosion and Protection of Metals; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
吴进怡 柴柯 肖伟龙 杨雨辉 韩恩厚. 25钢在海水中的微生物单因素腐蚀[J]. 金属学报, 2010, 46(6): 755-760.
,
,
,
,
.
THE SINGLE EFFECT OF MICROBE ON THE CORROSION BEHAVIORS OF 25 STEEL IN SEAWATER[J]. Acta Metall Sin, 2010, 46(6): 755-760.
| [1] Little B, Wagner P. Mater Performance, 1997; 36(6): 40
[2] Little B, Wagner P. J Adhes, 1986; 20: 187
[3] Li X B, Wang W, Wang J, Liu W Y. Corros Sci Prot Technol, 2002; 14: 218
(李相波, 王伟, 王佳, 刘五一. 腐蚀科学与防护技术, 2002; 14: 218)
[4] Jung H G, Yoo J Y, Woo J S. ISIJ Int, 2003; 43: 1603
[5] Mathiyarasu J, Palaniswamy N, Muralidharan V S. Corros Rev, 2000; 18: 65
[6] Walsh D, Pope D, Danford M, Huff T. JOM, 1993; 45(9): 22
[7] Liu D Y, Wei K J, Li W J, Cao F Y. J Chin Soc Corros Prot, 2003; 23: 211
(刘大扬, 魏开金, 李文军, 曹付炎. 中国腐蚀与防护学报, 2003; 23: 211)
[8] Busalmen J P, V´azquez M, de S´anchez S R. Electrochim Acta, 2002; 47: 1857
[9] de Damborenea J J, Crist´obal A B, Arenas M A, L´opez V, Conde A. Mater Lett, 2007; 61: 821
[10] Crist´obal A B, Arenas M A, Conde A, de Damborenea J. Electrochim Acta, 2006; 52: 546
[11] Sand W. Int Biodeterior Biodegrad, 1997; 40: 183
[12] Mansfeld F, Little B. Corros Sci, 1991; 32: 247
[13] Buchanan R E, Gibbons N E, Bergey’s. Manual of Determinative Bacteriology. 8th Ed., Baltimore, Maryland: The Williams and Wilkins Company, 1974: 7
[14] Sreekumari K R, Nandakumar K, Takao K, Kikuchi Y. ISIJ Int, 2003; 43: 1799
[15] Little B, Wagner P, Mansfeld F. Electrochim Acta, 1992; 37: 2185
[16] Ponmariappan S, Maruthamuthu S, Palaniswamy N, Palaniappan R. Corros Rev, 2004; 22: 307 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|