Please wait a minute...
金属学报  2010, Vol. 46 Issue (6): 761-768    DOI: 10.3724/SP.J.1037.2009.00685
  论文 本期目录 | 过刊浏览 |
选区激光熔化制备原位TiN-Ti5Si3复合材料的显微组织
顾冬冬1;2;3; 沈以赴1
1. 南京航空航天大学材料科学与技术学院; 南京 210016
2. Fraunhofer--Institut f\"{u}r Lasertechnik ILT; Aachen D--52074; Germany
3. Lehrstuhl fur Lasertechnik LLT; Rheinisch-Westfalische Technische Hochschule (RWTH) Aachen; Aachen D-52074; Germany
MICROSTRUCTURES OF IN SITU TiN–Ti5Si3 COMPOSITES PREPARED BY SELECTIVE LASER MELTING
GU Dongdong 1;2;3; SHEN Yifu1
1. College of Materials Science and Technology; Nanjing University of Aeronautics and Astronautics; Nanjing 210016
2. Fraunhofer–Institut f¨ur Lasertechnik ILT; Aachen D–52074; Germany
3. Lehrstuhl fur Lasertechnik LLT; Rheinisch–Westfalische Technische Hochschule (RWTH) Aachen; Aachen D–52074; Germany
引用本文:

顾冬冬 沈以赴. 选区激光熔化制备原位TiN-Ti5Si3复合材料的显微组织[J]. 金属学报, 2010, 46(6): 761-768.
, . MICROSTRUCTURES OF IN SITU TiN–Ti5Si3 COMPOSITES PREPARED BY SELECTIVE LASER MELTING[J]. Acta Metall Sin, 2010, 46(6): 761-768.

全文: PDF(3711 KB)  
摘要: 

利用高能球磨制备了Si3N4-Ti(摩尔比1∶9)纳米复合粉末, Si3N4和Ti平均晶粒尺寸均小于20 nm, 之后进行选区激光熔化成型,通过9Ti+Si3N4=4TiN+Ti5Si3反应生成TiN增强Ti5Si3基原位复合材料. 延长球磨时间, Si3N4-Ti复合粉末颗粒细化且比表面积增加,激光成型的TiN-Ti5Si3复合材料致密度可增至97.2%, 成型组织中TiN增强相形貌经历多棱角状→近圆形→枝晶状的转变.

关键词 : TiN-Ti5Si3复合材料,  选区激光熔化,  显微组织    
Abstract:

The selective laser melting (SLM) was used to process the high–energy ball milled Si3N4–Ti (mole ratio of 1∶9) nanocomposite powder in which the average grain sizes of Si3N4 and Ti were both less than 20 nm. The TiN reinfrced Ti5Si3 matrix in situ composites were prepard by means of the synthesis reaction 9Ti+Si3N4=4TiN+Ti5Si3 . s the milling time increased, thaverge particle size of te milled Si3N4–Ti composite powder decreased and the resultant specific surface area increased. The densification level of laser processed TiN–Ti5Si3  composites increased accordingly to 97.2%. The morphologies of TiN reinforcing phase in the corresponding SLM processed structures experienced a successive change from a poly–angular shape to a near–spherical shape and finally to a dendritic shape.

Key words: TiN–Ti5Si3 composites    selective laser melting    microstructure
收稿日期: 2009-10-19     
基金资助:

德国洪堡基金项目和江苏省自然科学基金项目BK2009374 资助

作者简介: 顾冬冬, 男, 1980年生, 副教授, 博士

[1] Wang L J, Jiang W, Bai S Q, Wang G, Chen L D. J Inorg Mater, 2004; 19: 1436
(王连军, 江莞, 柏胜强, 王刚, 陈立东. 无机材料学报, 2004; 19: 1436)
[2] Pierson H O. Handbook of Refractory Carbides and Nitrides: Properties, Characteristics, Processing and Applications. Park Ridge, NJ: Noyes Publications, 1996: 181
[3] Greil P. Adv Mater, 2002; 14: 709
[4] Tjong S C, Ma Z Y. Mater Sci Eng, 2000; R29: 49
[5] Kruth J P, Levy G, Klocke F, Childs T H C. CIRP Ann Manuf Technol, 2007; 56: 730
[6] Lin X, Yang H O, Chen J, Huang W D. Acta Metall Sin, 2006; 42: 361
 (林 鑫, 杨海欧, 陈 静, 黄卫东. 金属学报, 2006; 42: 361)
[7] Dong C, Zhang S Q, Li A, Wang H M. Acta Metall Sin, 2008; 44: 598
(董翠, 张述泉, 李安, 王华明. 金属学报, 2008; 44: 598)
[8] Xi M Z, Zhang Y Z, Tu Y, Shi L K, Jin J T. Acta Metall Sin, 2008; 44: 826
(席明哲, 张永忠, 涂义, 石力开, 金具涛. 金属学报, 2008; 44: 826)
[9] Gu D D, Wang Z Y, Shen Y F, Li Q, Li Y F. Appl Surf Sci, 2009; 255: 9230
[10] Gu D D, Shen Y F, Meng G B. Mater Lett, 2009; 63: 2536
[11] Gu D D, Shen Y F. Acta Metall Sin, 2007; 43: 968
(顾冬冬, 沈以赴. 金属学报, 2007; 43: 968)
[12] Huang Q L, Cai J, Pan W, Chen J, Lian J. Mater Lett, 1997; 31: 221
[13] Fischer P, Romano V, Weber H P, Karapatis N P, Boillat E, Glardon R. Acta Mater, 2003; 51: 1651
[14] Simchi A, Pohl H. Mater Sci Eng, 2003; A359: 119
[15] Guan Q L, Wang H Y, Li S L, Liu C, Jiang Q C. J Mater Sci, 2009; 44: 1902

[1] 张雷雷, 陈晶阳, 汤鑫, 肖程波, 张明军, 杨卿. K439B铸造高温合金800℃长期时效组织与性能演变[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] 卢楠楠, 郭以沫, 杨树林, 梁静静, 周亦胄, 孙晓峰, 李金国. 激光增材修复单晶高温合金的热裂纹形成机制[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] 孙蓉蓉, 姚美意, 王皓瑜, 张文怀, 胡丽娟, 仇云龙, 林晓冬, 谢耀平, 杨健, 董建新, 成国光. Fe22Cr5Al3Mo-xY合金在模拟LOCA下的高温蒸汽氧化行为[J]. 金属学报, 2023, 59(7): 915-925.
[4] 吴东江, 刘德华, 张子傲, 张逸伦, 牛方勇, 马广义. 电弧增材制造2024铝合金的微观组织与力学性能[J]. 金属学报, 2023, 59(6): 767-776.
[5] 张东阳, 张钧, 李述军, 任德春, 马英杰, 杨锐. 热处理对选区激光熔化Ti55531合金多孔材料力学性能的影响[J]. 金属学报, 2023, 59(5): 647-656.
[6] 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆. 尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响[J]. 金属学报, 2023, 59(5): 623-635.
[7] 李殿中, 王培. 金属材料的组织定制[J]. 金属学报, 2023, 59(4): 447-456.
[8] 唐伟能, 莫宁, 侯娟. 增材制造镁合金技术现状与研究进展[J]. 金属学报, 2023, 59(2): 205-225.
[9] 芮祥, 李艳芬, 张家榕, 王旗涛, 严伟, 单以银. 新型纳米复合强化9Cr-ODS钢的设计、组织与力学性能[J]. 金属学报, 2023, 59(12): 1590-1602.
[10] 朱智浩, 陈志鹏, 刘田雨, 张爽, 董闯, 王清. 基于不同 α / β 团簇式比例的Ti-Al-V合金的铸态组织和力学性能[J]. 金属学报, 2023, 59(12): 1581-1589.
[11] 戚钊, 王斌, 张鹏, 刘睿, 张振军, 张哲峰. 应力比对含缺陷选区激光熔化TC4合金稳态疲劳裂纹扩展速率的影响[J]. 金属学报, 2023, 59(10): 1411-1418.
[12] 卢海飞, 吕继铭, 罗开玉, 鲁金忠. 激光热力交互增材制造Ti6Al4V合金的组织及力学性能[J]. 金属学报, 2023, 59(1): 125-135.
[13] 王孟, 杨永强, Trofimov Vyacheslav, 宋长辉, 周瀚翔, 王迪. 粉末粒径对AlSi10Mg合金选区激光熔化成形的影响[J]. 金属学报, 2023, 59(1): 147-156.
[14] 杨超, 卢海洲, 马宏伟, 蔡潍锶. 选区激光熔化NiTi形状记忆合金研究进展[J]. 金属学报, 2023, 59(1): 55-74.
[15] 祝国梁, 孔德成, 周文哲, 贺戬, 董安平, 疏达, 孙宝德. 选区激光熔化 γ' 相强化镍基高温合金裂纹形成机理与抗裂纹设计研究进展[J]. 金属学报, 2023, 59(1): 16-30.