| 超轻α固溶体基Mg-6Li-3Zn合金的位错蠕变 |
| 曹富荣1; 管仁国1; 丁桦1; 李英龙1; 周舸1; 崔建忠2 |
1.东北大学材料与冶金学院; 沈阳 110819
2.东北大学材料电磁过程教育部重点实验室; 沈阳 110819 |
|
| DISLOCATION CREEP IN SUPER–LIGHT α SOLID SOLUTION BASE Mg–6Li–3Zn ALLOY |
| CAO Furong1; GUAN Renguo1; DING Hua1; LI Yinglong1; ZHOU Ge1;CUI Jianzhong2 |
1.College of Materials and Metallurgy; Northeastern University; Shenyang 110819
2.Key Lab of Materials Electromagnetic Process; Ministry of Education; Northeastern University; Shenyang 110819 |
引用本文:
曹富荣 管仁国 丁桦 李英龙 周舸 崔建忠. 超轻α固溶体基Mg-6Li-3Zn合金的位错蠕变[J]. 金属学报, 2010, 46(6): 715-722.
,
,
,
,
.
DISLOCATION CREEP IN SUPER–LIGHT α SOLID SOLUTION BASE Mg–6Li–3Zn ALLOY[J]. Acta Metall Sin, 2010, 46(6): 715-722.
| [1] Counts W A, Friak M, Raabe D, Neugebauer J. Acta Mater, 2009; 57: 69
[2] Kim W J, Kim M J, Wang J Y. Mater Sci Eng, 2009; A516: 17
[3] Cao F R, Lei F, Cui J Z, Wen J L. Acta Metall Sin, 1999; 35: 770
(曹富荣, 雷方, 崔建忠, 温景林. 金属学报, 1999; 35: 770)
[4] Nayeb–Hashemi A A, Clark J B, Pelton A D. Bull Alloy Phase Diagram, 1984; 5: 365
[5] Raynor G V. The Physical Metallurgy of Magnesium and Its Alloys. London: Pergamon Press, 1959: 25
[6] Kassner M E, Perez–Prado M T. Prog Mater Sci, 2000; 45: 1
[7] Yavari P, Langdon T G. Acta Metall, 1982; 30: 2181
[8] Somekawa H, Hirai K, Watanabe H, Takigawa Y, Higashi K. Mater Sci Eng, 2005; A407: 53
[9] Li Y, Langdon T G. Acta Mater, 1998; 46: 1143
[10] Weinberg A F, Levinson D W, Rostoker W. Trans ASM, 1956; 48: 855
[11] Cao F R, Ding H, Li Y L, Zhou G, Cui J Z. Mater Sci Eng, 2010, A527: 2335
[12] Sherby O D, Wadsworth J. In: Krauss G ed., Deformation, Processing and Structure. Metals Park, Ohio: ASM, 1982: 355
[13] Hirai K, Somekawa H, Takigawa Y, Higashi K. Scr Mater, 2007; 56: 237
[14] King H W. J Mater Sci, 1966; 1: 79
[15] Murr L E. Interfacial Phenomena in Metals and Alloys. Mass: Addison Wesley, 1975: 55
[16] Koster W. Z Metallk, 1948; 39: 1
[17] Friedel J. Dislocations. Oxford: Pergamon Press, 1964: 202
[18] Wang J S, Nix W D. Acta Metall, 1986; 34: 545
[19] Fuentes–Samaniego R, Nix W D. Scr Metall, 1981; 15: 15
[20] Brown A W, Ashby M F. Acta Metall, 1980; 28: 1085
[21] Wolfenstine J, Gonzalez–Docel G, Sherby O D. J Mater Res, 1990; 5: 1359
[22] Ruano O A, Wadsworth J, Sherby O D. J Mater Sci, 1985; 20: 3735
[23] Pilling J, Ridley N. Superplasticity in Crystalline Solids. London: The Institute of Metals, 1989: 118
[24] Cao F R. PhD Thesis, Northeastern University, Shenyang, 1999
(曹富荣. 东北大学博士学位论文, 沈阳, 1999)
[25] Stowell M J, Livesey D W, Ridley N. Acta Metall, 1984; 32: 35
[26] Mukherjee A K. Mater Sci Eng, 1971; 8: 83
[27] Taleff E M, Ruano O A, Wolfenstine J, Sherby O D. J Mater Res, 1992; 7: 2131 |
|