| DZ468合金高周疲劳性能研究 |
| 刘恩泽; 郑志; 佟 健; 宁礼奎; 管秀荣 |
| 中国科学院金属研究所; 沈阳 110016 |
|
| STUDY ON HIGH CYCLE FATIGUE PROPERTIES OF DZ468 SUPERALLOY |
| LIU Enze; ZHENG Zhi; TONG Jian; NING Likui; GUAN Xiurong |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
刘恩泽 郑志 佟健 宁礼奎 管秀荣. DZ468合金高周疲劳性能研究[J]. 金属学报, 2010, 46(6): 708-714.
.
STUDY ON HIGH CYCLE FATIGUE PROPERTIES OF DZ468 SUPERALLOY[J]. Acta Metall Sin, 2010, 46(6): 708-714.
| [1] Yu Z F, Zheng Z, Liu E Z, Yu Y S, Zhu Y X. J Chin Soc Corros Prot, 2008; 28: 277
(于忠峰, 郑志, 刘恩泽, 于永泗, 朱耀宵. 中国腐蚀与防护学报, 2008; 28: 277)
[2] Ning L K, Zheng Z, Tan Y, Liu E Z, Tong J, Yu Y S, Wang H. Acta Metall Sin, 2009; 45: 161
(宁礼奎, 郑 志, 谭 毅, 刘恩泽, 佟健, 于永泗, 王华. 金属学报, 2009; 45: 161)
[3] Liu E Z, Sun S C, Tu G F, Zheng Z, Ning L K, Zhang L F. Acta Metall Sin, 2009; 45: 1217
(刘恩泽, 孙树臣, 涂赣峰, 郑 志, 宁礼奎, 张凌峰. 金属学报, 2009; 45: 1217)
[4] Hoffelner W. Metall Trans, 1982; 13A: 1245
[5] Sajjadi S A, Nategh S. Mater Sci Eng, 2001; A307: 158
[6] Liu Y, Yu J J, Xu Y. Mater Sci Eng, 2007; A454: 357
[7] Hoffelner W, Gudmundson P. Eng Fract Mech, 1982; 16: 365
[8] Jones B F. Int J Fatigue, 1984; 6: 75
[9] Pope D P, Ezz S S. Int Met Rev, 1984; 29: 136
[10] Sieborger D, Knake H, Glatzel U. Mater Sci Eng, 2001; A298: 26
[11] Shi C X, Yan M G, Zhu Z Q. China Aeronautical Materials Handbooks. Beijing: China Standard Press, 2001: 550
(师昌绪, 颜鸣皋, 朱之琴. 中国航空材料手册, 北京: 中国标准出版社, 2001: 550)
[12] Zheng Y R, Cai Y L, Ruan Z C, Ma S. J Aeronaut Mater, 2006; 26: 25
(郑运荣, 蔡玉林, 阮中慈, 马书. 航空材料学报, 2006; 26: 25)
[13] Zheng Y R, Wang Yu P, Xie J H, Caron P, Khan T. In: Reichman S, Duhl D N, Maurer G, Antolovich S eds., Superalloys 1988, PA: TMS, 1988: 335
[14] Zheng Y R, Cai Y L, Ruan Z C. Acta Metall Sin, 1987; 23: A430
(郑运荣, 蔡玉林, 阮中慈. 金属学报, 1987; 23: A430)
[15] Zheng Y R, Cai Y L, Wang L B. Acta Metall Sin, 1983; 19: A190
(郑运荣, 蔡玉林, 王罗宝. 金属学报, 1983; 19: A190)
[16] Zheng Y R. Chin J Aeronaut, 198; 7: 482
(郑运荣. 航空学报, 1986; 7: 482)
[17] Gell M, Leverant G R. Acta Metall, 1968; 16: 553
[18] Bowen A W, Forsyh P J EMater Sci Eng, 1981; 49: 141
[19] Forsyth P J E. Acta Metall, 1963; 11: 703
[20] Laird C. Fatigue Crack Propagation, STP415. Philadelphia: ASTM, 1967: 131
[21] Liu Y. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2008
(刘 源. 中国科学院金属研究所博士学位论文, 沈阳, 2008)
[22] Chu Z K. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2008
(储昭贶. 中国科学院金属研究所博士学位论文, 沈阳, 2008) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|