| 定向凝固NiAl-Cr(Mo)-Hf(Ho)共晶合金的组织与性能 |
| 肖旋1;谢亿2;郭建亭3 |
1. 沈阳理工大学材料科学与工程学院; 沈阳 110168
2. 湖南省电力公司试验研究院; 长沙 410007
3. 中国科学院金属研究所; 沈阳 110016 |
|
| MICROSTRUCTURES AND MECHANICAL PROPERTIES OF DIRECTIONALLY SOLIDIFIED NiAl–Cr(Mo)–Hf(Ho) EUTECTIC ALLOY |
| XIAO Xuan 1; XIE Yi 2; GUO Jianting 3 |
1. School of Materials Science and Engineering; Shenyang Ligong University; Shenyang 110168
2. Hunan Electric Power Test and Research Institute; Changsha 410007
3. Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
肖璇 谢亿 郭建亭. 定向凝固NiAl-Cr(Mo)-Hf(Ho)共晶合金的组织与性能[J]. 金属学报, 2010, 46(6): 701-707.
,
,
.
MICROSTRUCTURES AND MECHANICAL PROPERTIES OF DIRECTIONALLY SOLIDIFIED NiAl–Cr(Mo)–Hf(Ho) EUTECTIC ALLOY[J]. Acta Metall Sin, 2010, 46(6): 701-707.
| [1] Noebe R D, Bowman R R, Nathal N V. Int Mater Rev, 1993; 38: 193
[2] Miracle D B. Acta Metall Mater, 1993; 41: 649
[3] Johnson D R, Oliver B F, Noebe R D, Whittenberger J D. Intermetallics, 1995; 3: 493
[4] Yang J M, Jeng S M, Bain K, Amato R A. Acta Metall Mater, 1997; 45: 295
[5] Johnson D R, Chen X F, Oliver B F, Noebe R D, Whittenberger J D. Intermetallics, 1995; 3: 99
[6] Walter J L, Cline H E. Metall Trans, 1970; 1: 1221
[7] Cline H E, Walter J L. Metall Trans, 1970; 1: 2907
[8] Cline H E, Walter J L, Lifshine E, Russell R R. Metall Trans, 1971; 2: 189
[9] Chen X F, Johnson D R, Noebe R D, Oliver B F. J Mater Res, 1995; 10: 1159
[10] Raj S V, Locci I E. Intermetallics, 2001; 9: 217
[11] Whittenberger J D, Raj S V, Locci I E, Salem J A. Intermetallics, 1999; 7: 1159
[12] Raj S V, Locci I E, Salem J A, Pawlik R J. Metall Mater Trans, 2002; 33A: 597
[13] Jachson K H, Hunt J D. Trans Metall Soc AIME, 1966; 236: 1129
[14] Whittenberger J D, Locci I E, Darolia R, Bowman R R. Mater Sci Eng, 1999; A268: 165
[15] Takeyama M, Liu C T. J Mater Res, 1990; 5: 1189
[16] Guo J T, Cui C Y, Qi Y H, Ye H Q. J Alloys Compd, 2002; 343: 142
[17] Guo J T, Huai K W, Gao Q, Ren W L, Li G S. Intermetallics , 2007; 15: 727
[18] Ren W L, Guo J T, Li G S, Zhou J. Mater Lett, 2003; 57: 1374 |
|