| 强磁场对Cu--80%Pb过偏晶合金中富Cu颗粒 迁移行为的影响 |
| 张林;王恩刚;左小伟;赫冀成 |
| 东北大学材料电磁过程研究教育部重点实验室; 沈阳 110004 |
|
| EFFECT OF HIGH MAGNETIC FIELD ON THE TRANSITION BEHAVIOR OF Cu–RICH PARTICLES IN Cu–80%Pb HYPERMONOTECTIC ALLOY |
| ZHANG Lin; WANG Engang; ZUO Xiaowei; HE Jicheng |
| Key Laboratory of Electromagnetic Processing of Materials; Ministry of Education; Northeastern University; Shenyang; 110004 |
引用本文:
张林 王恩刚 左小伟 赫冀成. 强磁场对Cu--80%Pb过偏晶合金中富Cu颗粒 迁移行为的影响[J]. 金属学报, 2010, 46(4): 423-428.
,
,
,
.
EFFECT OF HIGH MAGNETIC FIELD ON THE TRANSITION BEHAVIOR OF Cu–RICH PARTICLES IN Cu–80%Pb HYPERMONOTECTIC ALLOY[J]. Acta Metall Sin, 2010, 46(4): 423-428.
| [1] Dhindaw B K. Stefanescu D M, Singh A K, Curreri P A. Metall Trans, 1988; 19A: 2839
[2] Liu Y, Guo J J, Jia J, Su Y Q, Ding H S. Acta Metall Sin, 2000; 36: 1233
(刘 源, 郭景杰, 贾均, 苏彦庆, 丁宏升. 金属学报, 2000; 36: 1233)
[3] Yang S, Liu W J, Jia J. Mater Sci Technol, 2002; 10: 19
(杨森, 刘文今, 贾均. 材料科学与工艺, 2002; 10: 19)
[4] Zu D Y, Yang X H, Han X M,Wei B B. Chin J Nonferrous Met, 2003; 13: 328
(朱定一, 杨晓华, 韩秀君, 魏炳波. 中国有色金属学报, 2003; 13: 328)
[5] Yasuda H, Ohnaka I, Kawakami O, Ueno K, Kishio K. ISIJ Int, 2003; 43: 942
[6] Zhao J Z, Li H L, Wang Q L, Zhao L, He J. Acta Metall Sin, 2009; 45: 1344
(赵九洲, 李海丽, 王青亮, 赵雷, 何杰. 金属学报, 2009; 45: 1344)
[7] Ratke L, Diefenbach S. Mate Sci Eng, 1995; R15: 263
[8] Zhao J Z, Li H L, Zhao L. Acta Metall Sin, 2009; 45: 1435
(赵九洲, 李海丽, 赵雷. 金属学报, 2009; 45: 1435)
[9] Zhang L, Wang E G, Zuo X W, He J C. Acta Metall Sin, 2008; 44: 165
(张林, 王恩刚, 左小伟, 赫冀成. 金属学报, 2008; 44: 165)
[10] Xu Z M, Li T X, Zhang X P, Zhou R H. J Shanghai Jiaotong Univ, 2001; 35: 668
(许振明, 李天晓, 张雪萍, 周尧和. 上海交通大学学报, 2001; 35: 668)
[11] Zhong Y B, Ren Z M, Sun Q X, Jiang Z W, Deng K, Xu K D. Acta Metall Sin, 2003; 39: 1269
(钟云波, 任忠鸣, 孙秋霞, 江志文, 邓康, 徐匡迪. 金属学报, 2003; 39: 1269)
[12] Shu D, Sun B, Li K, hou Y. Scr Mater, 2003; 48: 1385
[13] Colli F, Fabbri M, Negrini F, Asai S, Sassa K. Int J Comput Math Electr Electron Eng, 2003; 22: 58
[14] Zhang L, Yao G C, Jiao W L. J Northeastern Univ (Nat Sci), 2004; 25: 682
(张 磊, 姚广春, 焦万丽. 东北大学学报(自然科学版), 2004; 25: 682)
[15] Zhang L. PhD Dissertation, Northeastern University, Shenyang, 2008
(张 林. 东北大学博士学位论文, 沈阳, 2008)
[16] Ratke L, Voorhees P W. Growth and Coarsening. Berlin: Springer–Verlag, 2002: 1
[17] Walter H U, Vreeburg J P B. Fluid Sciences and Materials Science in Space. Berlin: Springer–Verlag, 1987: 1
[18] Brandes E A, Brook G B. Smithells Metals Reference Book. 7th Ed., Oxford: Butterworth–Heinemann, 1998: 1
[19] Happel J. AIChE J, 1959; 5: 174
[20] Chester W. J Fluid Mech, 1957; 3: 304 |
|