| 钨含量对12%Cr耐热钢力学性能的影响 |
| 刘兴阳;藤田利夫 |
| 东北工学院;副教授;东京大学 |
|
| EFFECT OF W CONTENT ON MECHANICAL PROPERTIES OF 12%Cr-W-V-Nb HEAT RESISTANT STEEL |
| LIU Xingyang Northeast University of Technology; Shenyang; FUJITA Toshio University of Tokyo; Japan |
引用本文:
刘兴阳;藤田利夫. 钨含量对12%Cr耐热钢力学性能的影响[J]. 金属学报, 1991, 27(5): 27-32.
,
.
EFFECT OF W CONTENT ON MECHANICAL PROPERTIES OF 12%Cr-W-V-Nb HEAT RESISTANT STEEL[J]. Acta Metall Sin, 1991, 27(5): 27-32.
1 刘兴阳,藤田利夫,铁钢,1987;73:1034 2 刘兴阳,藤田利夫,铁钢,1988;74:513 3 田中秀毅,刘兴阳,柴田浩司,材料,1988;1:S531 4 Briggs J Z, Parker T D. The Super 12% Cr Steels Climax Molybdenun Comp. of Michigan, USA 1982 5 高桥纪雄·藤田利夫,铁钢,1974:60:1506 |
|