| 8090Al-Li合金的微观结构与力学性能 |
| 刘玉林;张匀;赵洪恩;胡壮麒;师昌绪 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;研究员;中国科学院金属研究所 |
|
| MICROSTRUCTURE AND MECHANICAL PROPERTIES OF 8090 AI-Li ALLOY |
| LIU Yulin;ZHANG Yun;ZHAO Hong'en;HU Zhuangqi;SHI Changxu Institute of Metal Research; Academia Sinica; Shenyang Correspondent: HU Zhuangqi; professor; Institute of Metal Research; Academia Sinica |
引用本文:
刘玉林;张匀;赵洪恩;胡壮麒;师昌绪. 8090Al-Li合金的微观结构与力学性能[J]. 金属学报, 1991, 27(5): 21-26.
,
,
,
,
.
MICROSTRUCTURE AND MECHANICAL PROPERTIES OF 8090 AI-Li ALLOY[J]. Acta Metall Sin, 1991, 27(5): 21-26.
1 张匀,赵洪恩,姚大平,高国忠,陈继志,胡壮麒.金属学报,1989;25:A161 2 Lin F S, Chakrabortty S B, Starke E A Jr. Metall Trans, 1982; 13A: 401 3 Crooks R E, Starke E A Jr. Metall Trans, 1984; 15A: 1367 4 Webster D, Kirkbride R. Metall Trans, 1986; 17A: 2007 5 Venkateswara Rao K T, Ritchie R O. Mater Sci Technol, 1989; 5: 882 6 Srivatsan T S, Plan Place T. J Mater Sci, 1989; 24: 1543 7 Shakesheff A J, McDarmaid D S, Gregson P J. In: Sanders T H Jr., Starke E A Jr. eds., Aluminum-Lithium Alloys, Proc 5th Int Aluminum-Lithium Conf, Williamsburg, Virginia, March 27--31, 1989, Birmingham, UK: Materials and Component Engineering Publications Ltd., 1989: 201 8 Verdu C, Gentzbittel J M, Fourgeres R. In: Sanders T H Jr., Starke E A Jr. eds., Aluminum-Lithium Alloys, Proc 5th Int Aluminum-Lithium Conf, Williamsburg, Virginia, March 27--31, 1989, Birmingham, UK: Materials and Component Engineering Publications Ltd., 1989: 899 9 Gatenby K M, Reynolds M A, White J. In: Sanders T H Jr., Starke E A Jr. eds., Aluminum-Lithium Alloys, Proc 5th Int Aluminum-Lithium Conf, Williamsburg, Virginia, March 27--31, 1989, Birmingham, UK: Materials and Component Engineering Publications Ltd., 1989: 909 10 Gregson P J, Flower H M. Acta Metall, 1985; 33: 527 11 Harris S J, Noble B, Dinsdale K, et al. In: Baker C, Gregson P J, Harris S J, Peel C J eds., Aluminium-Lithium Alloys III, Proc 3th Int Aluminium-Lithium Conf, University of Oxford, 8--11 July, 1985, London: The Institute of Metals, 1986: 610 12 姚大平,胡壮麒,李依依,张匀,师昌绪,金属学报,1990;26:A97 13 Starke E A Jr., Sanders T H Jr., Palmer I G. J Met, 1981; 33(8) : 24 14 Balmuth E S. Ser Metall, 1984; 18: 301 15 Sanders T H Jr., Starke E A Jr. In: Sanders T H Jr.. Starke E A Jr. eds., Aluminum-Lithium Alloys, Proc 5th Int Aluminum-Lithium Conf. Wiliamsburg, Virginia, March 27--31, 1989, Birmingham, UK: Materials and Component Engineering Publications Ltd.. 1989: 1 16 Furukawa M, Miura Y, Nemoto M. Trans Jpn Inst Met, 1985; 26: 230 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|