| 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理 |
李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成( ), 任玉平, 秦高梧 |
| 东北大学 材料科学与工程学院 材料各向异性与织构教育部重点实验室 沈阳 110819 |
|
| Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion |
LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng( ), REN Yuping, QIN Gaowu |
| Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education), School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China |
引用本文:
李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
Jingren LI,
Dongsheng XIE,
Dongdong ZHANG,
Hongbo XIE,
Hucheng PAN,
Yuping REN,
Gaowu QIN.
Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. Acta Metall Sin, 2023, 59(8): 1087-1096.
| 1 |
Song J F, Chen J, Xiong X M, et al. Research advances of magnesium and magnesium alloys worldwide in 2021 [J]. J. Magnes. Alloy., 2022, 10: 863
doi: 10.1016/j.jma.2022.04.001
|
| 2 |
Yang Q S, Jiang B, Song B, et al. The effects of orientation control via tension-compression on microstructural evolution and mechanical behavior of AZ31 Mg alloy sheet [J]. J. Magnes. Alloy., 2022, 10: 411
doi: 10.1016/j.jma.2020.08.005
|
| 3 |
Luo Q, Guo Y L, Liu B, et al. Thermodynamics and kinetics of phase transformation in rare earth-magnesium alloys: A critical review [J]. J. Mater. Sci. Technol., 2020, 44: 171
doi: 10.1016/j.jmst.2020.01.022
|
| 4 |
Luo Q, Zhai C, Gu Q F, et al. Experimental study and thermodynamic evaluation of Mg-La-Zn system [J]. J. Alloys Compd., 2020, 814: 152297
doi: 10.1016/j.jallcom.2019.152297
|
| 5 |
Pan F S, Jiang B. Development and application of plastic processing technologies of magnesium alloys [J]. Acta Metall. Sin., 2021, 57: 1362
doi: 10.11900/0412.1961.2021.00349
|
| 5 |
潘复生, 蒋 斌. 镁合金塑性加工技术发展及应用 [J]. 金属学报, 2021, 57: 1362
doi: 10.11900/0412.1961.2021.00349
|
| 6 |
Zha M, Wang S Q, Fang Y, et al. Advancement in research of rolled magnesium alloys with high performance [J]. J. Net. Form. Eng., 2020, 12(5): 20
|
| 6 |
查 敏, 王思清, 方 圆 等. 高性能轧制镁合金研究进展 [J]. 精密成形工程, 2020, 12(5): 20
|
| 7 |
Jiang M G, Xu C, Yan H, et al. Quasi-in-situ observing the rare earth texture evolution in an extruded Mg-Zn-Gd alloy with bimodal microstructure [J]. J. Magnes. Alloy., 2021, 9: 1797
doi: 10.1016/j.jma.2020.09.001
|
| 8 |
Wu G H, Tong X, Jiang R, et al. Grain refinement of as-cast Mg-RE alloys: Research progress and future prospect [J]. Acta Metall. Sin., 2022, 58: 385
doi: 10.11900/0412.1961.2021.00519
|
| 8 |
吴国华, 童 鑫, 蒋 锐 等. 铸造Mg-RE合金晶粒细化行为研究现状与展望 [J]. 金属学报, 2022, 58: 385
doi: 10.11900/0412.1961.2021.00519
|
| 9 |
Zhang O, Hu H J, Hu G, et al. Research progress on composite refinement strengthening of magnesium alloy [J]. J. Net. Form. Eng., 2021, 13(6): 98
|
| 9 |
章 欧, 胡红军, 胡 刚 等. 镁合金复合细晶强化研究进展 [J]. 精密成形工程, 2021, 13(6): 98
|
| 10 |
Li J R, Xie D S, Zeng Z R, et al. Mechanistic investigation on Ce addition in tuning recrystallization behavior and mechanical property of Mg alloy [J]. J. Mater. Sci. Technol., 2023, 132: 1
doi: 10.1016/j.jmst.2022.05.042
|
| 11 |
Li J R, Zhang A Y, Pan H C, et al. Effect of extrusion speed on microstructure and mechanical properties of the Mg-Ca binary alloy [J]. J. Magnes. Alloy., 2021, 9: 1297
doi: 10.1016/j.jma.2020.05.011
|
| 12 |
Xie D S, Pan H C, Li M, et al. Role of Al addition in modifying microstructure and mechanical properties of Mg-1.0wt%Ca based alloys [J]. Mater. Charact., 2020, 169: 110608
doi: 10.1016/j.matchar.2020.110608
|
| 13 |
Li Z H, Sasaki T T, Uedono A, et al. Role of Zn on the rapid age-hardening in Mg-Ca-Zn alloys [J]. Scr. Mater., 2022, 216: 114735
doi: 10.1016/j.scriptamat.2022.114735
|
| 14 |
Zhang A Y, Kang R, Wu L, et al. A new rare-earth-free Mg-Sn-Ca-Mn wrought alloy with ultra-high strength and good ductility [J]. Mater. Sci. Eng., 2019, A754: 269
|
| 15 |
Li M, Xie D S, Li J R, et al. Realizing ultra-fine grains and ultra-high strength in conventionally extruded Mg-Ca-Al-Zn-Mn alloys: The multiple roles of Nano-precipitations [J]. Mater. Charact., 2021, 175: 111049
doi: 10.1016/j.matchar.2021.111049
|
| 16 |
Pan H C, Kang R, Li J R, et al. Mechanistic investigation of a low-alloy Mg-Ca-based extrusion alloy with high strength-ductility synergy [J]. Acta Mater., 2020, 186: 278
doi: 10.1016/j.actamat.2020.01.017
|
| 17 |
Song J F, Pan F S, Jiang B, et al. A review on hot tearing of magnesium alloys [J]. J. Magnes. Alloy., 2016, 4: 151
doi: 10.1016/j.jma.2016.08.003
|
| 18 |
Aljarrah M, Medraj M. Thermodynamic modelling of the Mg-Ca, Mg-Sr, Ca-Sr and Mg-Ca-Sr systems using the modified quasichemical model [J]. Calphad, 2008, 32: 240
doi: 10.1016/j.calphad.2007.09.001
|
| 19 |
Wang T, Jiang L, Mishra R K, et al. Effect of Ca addition on the intensity of the rare earth texture component in extruded magnesium alloys [J]. Metall. Mater. Trans., 2014, 45A: 4698
|
| 20 |
Zeng Z R, Stanford N, Davies C H J, et al. Magnesium extrusion alloys: A review of developments and prospects [J]. Int. Mater. Rev., 2019, 64: 27
doi: 10.1080/09506608.2017.1421439
|
| 21 |
Cihova M, Schäublin R, Hauser L B, et al. Rational design of a lean magnesium-based alloy with high age-hardening response [J]. Acta Mater., 2018, 158: 214
doi: 10.1016/j.actamat.2018.07.054
|
| 22 |
Wang F L, Barrett C D, McCabe R J, et al. Dislocation induced twin growth and formation of basal stacking faults in {10 1 ¯ 2} twins in pure Mg [J]. Acta Mater., 2019, 165: 471
doi: 10.1016/j.actamat.2018.12.003
|
| 23 |
Wang F L, Agnew S R. Dislocation transmutation by tension twinning in magnesium alloy AZ31 [J]. Int. J. Plast., 2016, 81: 63
doi: 10.1016/j.ijplas.2016.01.012
|
| 24 |
He C, Zhang Y, Liu C Q, et al. Unexpected partial dislocations within stacking faults in a cold deformed Mg-Bi alloy [J]. Acta Mater., 2020, 188: 328
doi: 10.1016/j.actamat.2020.02.010
|
| 25 |
Jiang M G, Xu C, Yan H, et al. Correlation between dynamic recrystallization and formation of rare earth texture in a Mg-Zn-Gd magnesium alloy during extrusion [J]. Sci. Rep., 2018, 8: 16800
doi: 10.1038/s41598-018-35170-4
pmid: 30429510
|
| 26 |
Ye J, Mishra R K, Sachdev A K, et al. In situ TEM compression testing of Mg and Mg-0.2wt.%Ce single crystals [J]. Scr. Mater., 2011, 64: 292
doi: 10.1016/j.scriptamat.2010.09.047
|
| 27 |
Wang J Y, Chen Y W, Chen Z, et al. Deformation mechanisms of Mg-Ca-Zn alloys studied by means of micropillar compression tests [J]. Acta Mater., 2021, 217: 117151
doi: 10.1016/j.actamat.2021.117151
|
| 28 |
Ashby M F. The deformation of plastically non-homogeneous materials [J]. Philos. Mag., 1970, 21: 399
|
| 29 |
Kubin L P, Mortensen A. Geometrically necessary dislocations and strain-gradient plasticity: A few critical issues [J]. Scr. Mater., 2003, 48: 119
doi: 10.1016/S1359-6462(02)00335-4
|
| 30 |
Zhang D D, Pan H C, Li J R, et al. Fabrication of exceptionally high-strength Mg-4Sm-0.6Zn-0.4Zr alloy via low-temperature extrusion [J]. Mater. Sci. Eng., 2022, A833: 142565
|
| 31 |
Wen Y, Guan B, Xin Y C, et al. Solute atom mediated Hall-Petch relations for magnesium binary alloys [J]. Scr. Mater., 2022, 210: 114451
doi: 10.1016/j.scriptamat.2021.114451
|
| 32 |
Wang F L, Bhattacharyya J J, Agnew S R. Effect of precipitate shape and orientation on Orowan strengthening of non-basal slip modes in hexagonal crystals, application to magnesium alloys [J]. Mater. Sci. Eng., 2016, A666: 114
|
| 33 |
Yang Y, Liu Y, Yan S, et al. On the micromechanism of superior strength and ductility synergy in a heterostructured Mg-2.77Y alloy [J]. J. Magnes. Alloy., 2022,
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|