| 低密度Ti2AlNb基合金热轧板微观组织的热稳定性 |
冯艾寒1, 陈强2, 王剑3, 王皞4, 曲寿江1( ), 陈道伦5( ) |
1同济大学 材料科学与工程学院 上海 200092 2西南技术工程研究所 重庆 400039 3宝钛集团有限公司 宝鸡 721014 4上海理工大学 材料与化学学院 增材制造研究院 上海 200093 5Department of Mechanical and Industrial Engineering, Toronto Metropolitan University, Toronto, Ontario M5B 2K3, Canada |
|
| Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate |
FENG Aihan1, CHEN Qiang2, WANG Jian3, WANG Hao4, QU Shoujiang1( ), CHEN Daolun5( ) |
1School of Materials Science and Engineering, Tongji University, Shanghai 200092, China 2Southwest Technology and Engineering Research Institute, Chongqing 400039, China 3BaoTi Group Co., Ltd., Baoji 721014, China 4Interdisciplinary Center for Additive Manufacturing, School of Materials and Chemistry, University of Shanghai for Science and Technology, Shanghai 200093, China 5Department of Mechanical and Industrial Engineering, Toronto Metropolitan University, Toronto, Ontario M5B 2K3, Canada |
引用本文:
冯艾寒, 陈强, 王剑, 王皞, 曲寿江, 陈道伦. 低密度Ti2AlNb基合金热轧板微观组织的热稳定性[J]. 金属学报, 2023, 59(6): 777-786.
Aihan FENG,
Qiang CHEN,
Jian WANG,
Hao WANG,
Shoujiang QU,
Daolun CHEN.
Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. Acta Metall Sin, 2023, 59(6): 777-786.
| 1 |
Banerjee D, Gogia A K, Nandi T K, et al. A new ordered orthorhombic phase in a Ti3Al-Nb alloy [J]. Acta Metall., 1988, 36: 871
doi: 10.1016/0001-6160(88)90141-1
|
| 2 |
Banerjee D. The intermetallic Ti2AlNb [J]. Prog. Mater. Sci., 1997, 42: 135
doi: 10.1016/S0079-6425(97)00012-1
|
| 3 |
Qu S J, Feng A H, Shagiev M R, et al. Superplastic behavior of the fine-grained Ti-21Al-18Nb-1Mo-2V-0.3Si intermetallic alloy [J]. Lett. Mater., 2018, 8: 567
doi: 10.22226/2410-3535
|
| 4 |
Zhu H P, Qu S J, Qi G Y, et al. High temperature oxidation behavior of as-rolled Ti2AlNb-based alloy [J]. Chin. J. Rare Met., 2016, 40: 104
|
| 4 |
朱慧萍, 曲寿江, 祁广源 等. Ti2AlNb基合金轧板高温抗氧化性能研究 [J]. 稀有金属, 2016, 40: 104
|
| 5 |
Xiang J M, Mi G B, Qu S J, et al. Thermodynamic and microstructural study of Ti2AlNb oxides at 800oC [J]. Sci. Rep., 2018, 8: 12761
doi: 10.1038/s41598-018-31196-w
pmid: 30143715
|
| 6 |
Zhang Y L, Feng A H, Qu S J, et al. Microstructure and low cycle fatigue of a Ti2AlNb-based lightweight alloy [J]. J. Mater. Sci. Technol., 2020, 44: 140
doi: 10.1016/j.jmst.2020.01.032
|
| 7 |
Feng A H, Li B B, Shen J. Recent advances on Ti2AlNb-based alloys [J]. J. Mater. Metall., 2011, 10: 30
|
| 7 |
冯艾寒, 李渤渤, 沈 军. Ti2AlNb基合金的研究进展 [J]. 材料与冶金学报, 2011, 10: 30
|
| 8 |
Shen J, Feng A H. Recent advances on microstructural controlling and hot forming of Ti2AlNb-based alloys [J]. Acta Metall. Sin., 2013, 49: 1286
doi: 10.3724/SP.J.1037.2013.00607
|
| 8 |
沈 军, 冯艾寒. Ti2AlNb基合金微观组织调制及热成形研究进展 [J]. 金属学报, 2013, 49: 1286
|
| 9 |
Li Z J, Tian W, Li J W, et al. Application of Ti2AlNb alloy electron beam welding on aero-engine casing [J]. Gas Turbine Exp. Res., 2020, 33(3): 52
|
| 9 |
李祚军, 田 伟, 李晋炜 等. Ti2AlNb合金电子束焊接在航空发动机机匣中的应用 [J]. 燃气涡轮试验与研究, 2020, 33(3): 52
|
| 10 |
Zhang H Y, Yan N, Liang H Y, et al. Phase transformation and microstructure control of Ti2AlNb-based alloys: A review [J]. J. Mater. Sci. Technol., 2021, 80: 203
doi: 10.1016/j.jmst.2020.11.022
|
| 11 |
Ravi C, Vajeeston P, Mathijaya S, et al. Electronic structure, phase stability, and cohesive properties of Ti2 XAl (X = Nb, V, Zr) [J]. Phys. Rev., 1999, 60B: 15683
|
| 12 |
Pathak A, Singh A K. A first principles study of Ti2AlNb intermetallic [J]. Solid State Commun., 2015, 204: 9
doi: 10.1016/j.ssc.2014.12.002
|
| 13 |
Morris M A, Morris D G. Strain localization, slip-band formation and twinning associated with deformation of a Ti-24at.%Al-11at.%Nb alloy [J]. Philos. Mag., 1991, 63A: 1175
|
| 14 |
Kazantseva N V, Demakov S L, Popov A A. Microstructure and plastic deformation of orthorhombic titanium aluminides Ti2AlNb. III. Formation of transformation twins upon the B2→Ophase transformation [J]. Phys. Met. Metallogr., 2007, 103: 378
doi: 10.1134/S0031918X07040102
|
| 15 |
Kazantseva N V, Demakov S L, Popov A A. Microstructure and plastic deformation of orthorhombic titanium aluminides Ti2AlNb. IV. Formation of the transformation twins upon the α2→O phase transformation [J]. Phys. Met. Metallogr., 2007, 103: 388
doi: 10.1134/S0031918X07040114
|
| 16 |
Liang X B, Zhou J J, Zhang J W, et al. High cycle fatigue at high temperatures of the lamellar microstructure of Ti-22Al-25Nb alloy [J]. Titanium Ind. Prog., 2019, 36(2): 20
|
| 16 |
梁晓波, 周俊吉, 张建伟 等. 板条组织Ti-22Al-25Nb合金高温高周疲劳行为 [J]. 钛工业进展, 2019, 36(2): 20
|
| 17 |
Luo C, Zhang Y, Wang X Y, et al. Effect of heat treatment on microstructure and properties of cast Ti-22Al-25Nb alloy [J]. Aerosp. Manuf. Technol., 2020, (2): 18
|
| 17 |
骆 晨, 张 寅, 王新英 等. 热处理对铸造Ti2AlNb合金组织和力学性能的影响 [J]. 航天制造技术, 2020, (2): 18
|
| 18 |
Li B B. Plate preparation, microstructure and mechanical properties of low-density Ti2AlNb-based alloys [D]. Harbin: Harbin Institute of Technology, 2011
|
| 18 |
李渤渤. 低密度Ti2AlNb基合金板材制备及组织与力学性能研究 [D] 哈尔滨: 哈尔滨工业大学, 2011
|
| 19 |
Chen Z. Research on microstructure and mechanical properties of Ti2AlNb-based alloy fabricated by multiple isothermal forging [D]. Harbin: Harbin Institute of Technology, 2013
|
| 19 |
陈 卓. Ti2AlNb基合金多向等温锻造组织与力学性能研究 [D]. 哈尔滨: 哈尔滨工业大学, 2013
|
| 20 |
Li S Y. Phase transformation and superplasticity deformation mechanism in Ti2AlNb-based alloys [D]. Harbin: Harbin Institute of Technology, 2013
|
| 20 |
李少雨. Ti2AlNb基合金相变及超塑性变形机理研究 [D]. 哈尔滨: 哈尔滨工业大学, 2013
|
| 21 |
Zhou Y, Cao J X, Huang X, et al. Microstructure evolution and comprehensive mechanical properties of β/B2 processed Ti-22Al-23Nb-2(Mo, Zr) alloy [J]. J. Aeronaut. Mater., 2020, 40(4): 25
|
| 21 |
周 毅, 曹京霞, 黄 旭 等. β/B2锻造Ti-22Al-23Nb-2(Mo, Zr)合金的组织演化与综合力学性能 [J]. 航空材料学报, 2020, 40(4): 25
|
| 22 |
Li J J, Zeng W D, Xue C. Effects of hot deformation parameters on lamellar microstructure evolution of Ti2AlNb based alloy [J]. Chin. J. Nonferrous Met., 2014, 24: 1998
|
| 22 |
李君珺, 曾卫东, 薛 晨. 热变形参数对Ti2AlNb基合金片层组织演变的影响 [J]. 中国有色金属学报, 2014, 24: 1998
|
| 23 |
Wang S L, Zeng W D, Ma X, et al. Effect of solution temperature on microstructure of Ti-22Al-25Nb alloy [J]. Mater. Heat Treat., 2009, 38(8): 106
|
| 23 |
王邵丽, 曾卫东, 马 雄 等. 固溶温度对Ti-22Al-25Nb合金微观组织的影响 [J]. 材料热处理技术, 2009, 38(8): 106
|
| 24 |
Boehlert C J, Majumdar B S, Seetharaman V, et al. Part I. The microstructural evolution in Ti-Al-Nb O + bcc orthorhombic alloys [J]. Metall. Mater. Trans., 1999, 30A: 2305
|
| 25 |
Boehlert C J. The phase evolution and microstructural stability of an orthorhombic Ti-23Al-27Nb alloy [J]. J. Phase Equilib., 1999, 20: 101
doi: 10.1007/s11669-999-0007-z
|
| 26 |
Boehlert C J, Miracle D B. Part II. The creep behavior of Ti-Al-Nb O + bcc orthorhombic alloys [J]. Metall. Mater. Trans., 1999, 30A: 2349
|
| 27 |
Boehlert C J. Microstructure, creep, and tensile behavior of a Ti-12Al-38Nb (at.%) beta+orthorhombic alloy [J]. Mater. Sci. Eng., 1999, A267: 82
|
| 28 |
Boehlert C J. Part III. The tensile behavior of Ti-Al-Nb O + bcc orthorhombic alloys [J]. Metall. Mater. Trans., 2001, 32A: 1977
|
| 29 |
Lin P, He Z B, Yuan S J, et al. Instability of the O-phase in Ti-22Al-25Nb alloy during elevated-temperature deformation [J]. J. Alloys Compd., 2013, 578: 96
doi: 10.1016/j.jallcom.2013.05.018
|
| 30 |
Bendersky L A, Boettinger W J, Roytburd A. Coherent precipitates in the b.c.c./orthorhombic two-phase field of the Ti-Al-Nb system [J]. Acta Metall. Mater., 1991, 39: 1959
doi: 10.1016/0956-7151(91)90165-W
|
| 31 |
Muraleedharan K, Gogia A K, Nandy T K, et al. Transformations in a Ti-24Al-15Nb alloy: Part I. Phase equilibria and microstructure [J]. Metall. Trans., 1992, 23A: 401
|
| 32 |
Popov A A, Illarionov A G, Grib S V, et al. Phase and structural transformations in the alloy on the basis of the orthorhombic titanium aluminide [J]. Phys. Met. Metallogr., 2008, 106: 399
doi: 10.1134/S0031918X08100104
|
| 33 |
Kazantseva N V, Lepikhin S V. Study of the Ti-Al-Nb phase diagram [J]. Phys. Met. Metall., 2006, 102: 169
doi: 10.1134/S0031918X06080084
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|