    					| 加工硬化和退火软化效应对316不锈钢厚壁管-管对接接头残余应力计算精度的影响 |  
						| 李索, 陈维奇, 胡龙, 邓德安(  ) |  
					| 重庆大学 材料科学与工程学院 重庆 400045 |  
						|  |  
    					| Influence of Strain Hardening and Annealing Effect on the Prediction of Welding Residual Stresses in a Thick-Wall 316 Stainless Steel Butt-Welded Pipe Joint |  
						| LI Suo, CHEN Weiqi, HU Long, DENG Dean(  ) |  
						| College of Materials Science and Engineering, Chongqing University, Chongqing 400045, China |  
								李索, 陈维奇, 胡龙, 邓德安. 加工硬化和退火软化效应对316不锈钢厚壁管-管对接接头残余应力计算精度的影响[J]. 金属学报, 2021, 57(12): 1653-1666.	
																												Suo LI,
																								Weiqi CHEN,
																								Long HU,
																												Dean DENG. 
				Influence of Strain Hardening and Annealing Effect on the Prediction of Welding Residual Stresses in a Thick-Wall 316 Stainless Steel Butt-Welded Pipe Joint[J]. Acta Metall Sin, 2021, 57(12): 1653-1666.
 
					
						| 
								
									|  
          
          
            
             
			              
            
									            
									                
																																															
																| 1 | Ming H L, Zhang Z M, Wang J Q, et al. Microstructure and local properties of a domestic safe-end dissimilar metal weld joint by using hot-wire GTAW [J]. Acta Metall. Sin., 2017, 53: 57 |  
																| 1 | 明洪亮, 张志明, 王俭秋等. 国产核电安全端异种金属焊接件的微观结构及局部性能研究 [J]. 金属学报, 2017, 53: 57 |  
																| 2 | Kansai Electric Power Company. Results of the investigation on the welded joint in the pressurizer spray line piping of the unit 3 of the Oi nuclear power plant (Data set) [R]. Tokyo: Nuclear Regulation Authority, 2020 |  
																| 2 | 関西電力株式会社. 大飯発電所3号機加圧器スプレイライン配管溶接部の調査結果 (データ集) [R]. 東京: 原子力規制委員会, 2020 |  
																| 3 | Mankins W L. Recovery, recrystallization, and grain-growth structures [A]. ASM Handbook, Vol.9: Metallography and Microstructures [M]. Ohio: ASM International, 2004: 207 |  
																| 4 | Qiao D X. Strain hardening recovery and its influence on welding residual stresses in reactor safe-end in power plants [D]. Beijing: Tsinghua University, 2013 |  
																| 4 | 乔东虓. 核电安全端焊接中应变硬化回复及其对残余应力的影响 [D]. 北京: 清华大学, 2013 |  
																| 5 | Deng D A, Kiyoshima S. Influence of annealing temperature on calculation accuracy of welding residual stress in a SUS304 stainless steel joint [J]. Acta Metall. Sin., 2014, 50: 626 |  
																| 5 | 邓德安, Kiyoshima S. 退火温度对SUS304不锈钢焊接残余应力计算精度的影响 [J]. 金属学报, 2014, 50: 626 |  
																| 6 | Zang W L, Gunnars J, Dong P S, et al. Improvement and validation of weld residual stress modelling procedure [R]. Stockholm: Swedish Radiation Safety Authority, 2009 |  
																| 7 | Xu J J, Gilles P, Duan Y G, et al. Temperature and residual stress simulations of the NeT single-bead-on-plate specimen using SYSWELD [J]. Int. J. Press. Vessels Pip., 2012, 99-100: 51 |  
																| 8 | Xu J J. Effect of material hardening model on welding residual stresses of 316L stainless steel [J]. Trans. China Weld. Inst., 2014, 35(3): 97 |  
																| 8 | 徐济进. 材料硬化模型对316L不锈钢焊接残余应力的影响 [J]. 焊接学报, 2014, 35(3): 97 |  
																| 9 | Muránsky O, Hamelin C J, Smith M C, et al. The effect of plasticity theory on predicted residual stress fields in numerical weld analyses [J]. Comput. Mater. Sci., 2012, 54: 125 |  
																| 10 | Muránsky O, Hamelin C J, Patel V I, et al. The influence of constitutive material models on accumulated plastic strain in finite element weld analyses [J]. Int. J. Solids Struct., 2015, 69-70: 518 |  
																| 11 | Deng D A, Zhang C H, Pu X W, et al. Influence of material model on prediction accuracy of welding residual stress in an austenitic stainless steel multi-pass butt-welded joint [J]. J. Mater. Eng. Perform., 2017, 26: 1494 |  
																| 12 | Wang Q, Liu X S, Wang P, et al. Numerical simulation of residual stress in 10Ni5CrMoV steel weldments [J]. J. Mater. Process. Technol., 2017, 240: 77 |  
																| 13 | Geng L Y, Tu S D, Gong J M, et al. Simulation of residual stress in butt girth welding of ultra-thick 13MnNiMoR steel cylinder by different material hardening models [J]. Mater. Mech. Eng., 2019, 43(3): 60 |  
																| 13 | 耿鲁阳, 涂善东, 巩建鸣等. 不同材料硬化模型模拟13MnNiMoR钢超厚圆筒对接环焊接残余应力 [J]. 机械工程材料, 2019, 43(3): 60 |  
																| 14 | Yu X H, Qiao D X, Feng Z L, et al. High temperature dynamics strain hardening behavior in stainless steels and nickel alloys [A]. Proceedings of the ASME 2014 Pressure Vessels and Piping Conference [C]. Anaheim, CA, USA: ASME, 2014: V06BT06A072 |  
																| 15 | Yu X H, Crooker P, Wang Y L, et al. High-temperature deformation constitutive law for dissimilar weld residual stress modeling: Effect of thermal load on strain hardening [A]. Proceedings of the ASME 2015 Pressure Vessels and Piping Conference [C]. Boston, MA, USA: ASME, 2015: V06BT06A073 |  
																| 16 | Japan Nuclear Energy Safety Organization. Annual report on the integrity assessment of flawed components with structural discontinuity [R]. Tokyo: Japan Nuclear Energy Safety Organization, 2005 |  
																| 16 | 原子力安全基盤機構. 複雑形状部機器配管健全性実証事業に関する報告書 [R]. 東京: 原子力安全基盤機構, 2005 |  
																| 17 | Hojo K, Ogawa K, Ogawa N, et al. Sensitivity analysis of residual stress simulation of dissimilar metal joint of safe end nozzle and key issues for standard procedure to maintenance rules [A]. Proceedings of the ASME 2010 Pressure Vessels and Piping Division/K-PVP Conference [C]. Bellevue, WA, USA: ASME, 2010: 929 |  
																| 18 | Ruud C O. Residual stress measurements [A]. ASM Handbook, Vol.8: Mechanical Testing and Evaluation [M]. Ohio: ASM International, 2000: 886 |  
																| 19 | Ma N S, Nakacho K, Ohta T, et al. Inherent strain method for residual stress measurement and welding distortion prediction [A]. Proceedings of the ASME 2016 35th International Conference on Ocean, Offshore and Arctic Engineering [C]. Busan, South Korea: ASME, 2016: V009T13A001 |  
																| 20 | Ogawa K, Chidwick L O, Kingston E J, et al. Measurement of residual stresses in the dissimilar metal weld joint of a safe-end nozzle component [A]. Proceedings of the ASME 2009 Pressure Vessels and Piping Conference [C]. Prague, Czech Republic: ASME, 2009: 529 |  
																| 21 | Dai P Y, Hu X, Lu S J, et al. Influence of size factor on calculation accuracy of welding residual stress of stainless steel pipe by 2D axisymmetric model [J]. Acta Metall. Sin., 2019, 55: 1058 |  
																| 21 | 戴培元, 胡 兴, 逯世杰等. 尺寸因素对2D轴对称模型计算不锈钢管焊接残余应力精度的影响 [J]. 金属学报, 2019, 55: 1058 |  
																| 22 | Lu S J, Wang H, Dai P Y, et al. Effect of creep on prediction accuracy and calculating efficiency of residual stress in post weld heat treatment [J]. Acta Metall. Sin., 2019, 55: 1581 |  
																| 22 | 逯世杰, 王 虎, 戴培元等. 蠕变对焊后热处理残余应力预测精度和计算效率的影响 [J]. 金属学报, 2019, 55: 1581 |  
																| 23 | Depradeux L, Coquard R. Influence of viscoplasticity, hardening, and annealing effects during the welding of a three-pass slot weld (NET-TG4 round robin) [J]. Int. J. Press. Vessels Pip., 2018, 164: 39 |  
																| 24 | Ludwik P. Elements der Technologischen Mechanik [M]. Berlin, Heidelberg: Springer-Verlag, 1909: 32 |  
																| 25 | Chaboche J L. A review of some plasticity and viscoplasticity constitutive theories [J]. Int. J. Plast., 2008, 24: 1642 |  
																| 26 | Leblond J B, Mottet G, Devaux J, et al. Mathematical models of anisothermal phase transformations in steels, and predicted plastic behaviour [J]. Mater. Sci. Technol., 1985, 1: 815 |  
																| 27 | Satoh K. Transient thermal stresses of weld heat-affected zone by both-ends-fixed bar analogy [J]. Trans. Jpn. Weld. Soc., 1972, 3: 125 |  
																| 28 | Depradeux L. Simulation numérique du soudage-acier 316L-validation sur cas tests de complexité croissante [D]. Lyon, France: INSA de Lyon, 2004 |  
																| 29 | Deng D A, Zhang Y B, Li S, et al. Influence of solid-state phase transformation on residual stress in P92 steel welded joint [J]. Acta Metall. Sin., 2016, 52: 394 |  
																| 29 | 邓德安, 张彦斌, 李 索等. 固态相变对P92钢焊接接头残余应力的影响 [J]. 金属学报, 2016, 52: 394 |  
																| 30 | Deng D A, Ren S D, Li S, et al. Influence of multi-thermal cycle and constraint condition on residual stress in P92 steel weldment [J]. Acta Metall. Sin., 2017, 53: 1532 |  
																| 30 | 邓德安, 任森栋, 李 索等. 多重热循环和约束条件对P92钢焊接残余应力的影响 [J]. 金属学报, 2017, 53: 1532 |  
																| 31 | Dong P S. On the mechanics of residual stresses in girth welds [J]. J. Press. Vessel Technol., 2007, 129: 345 |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |