| 退火温度对含Nb高锰钢力学和阻尼性能的影响 |
王玉, 胡斌, 刘星毅, 张浩, 张灏云, 官志强, 罗海文( ) |
| 北京科技大学 冶金与生态工程学院 北京 100083 |
|
| Influence of Annealing Temperature on Both Mechanical and Damping Properties of Nb-Alloyed High Mn Steel |
WANG Yu, HU Bin, LIU Xingyi, ZHANG Hao, ZHANG Haoyun, GUAN Zhiqiang, LUO Haiwen( ) |
| School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
王玉, 胡斌, 刘星毅, 张浩, 张灏云, 官志强, 罗海文. 退火温度对含Nb高锰钢力学和阻尼性能的影响[J]. 金属学报, 2021, 57(12): 1588-1594.
Yu WANG,
Bin HU,
Xingyi LIU,
Hao ZHANG,
Haoyun ZHANG,
Zhiqiang GUAN,
Haiwen LUO.
Influence of Annealing Temperature on Both Mechanical and Damping Properties of Nb-Alloyed High Mn Steel[J]. Acta Metall Sin, 2021, 57(12): 1588-1594.
| 1 |
Jee K K, Jang W Y, Baik S H, et al. Damping mechanism and application of Fe-Mn based alloys [J]. Mater. Sci. Eng., 1999, A273-275: 538
|
| 2 |
Huang S K, Wen Y H, Li N, et al. Application of damping mechanism model and stacking fault probability in Fe-Mn alloy [J]. Mater. Charact., 2008, 59: 681
|
| 3 |
Sawaguchi T, Bujoreanu L G, Kikuchi T, et al. Effects of Nb and C in solution and in NbC form on the transformation-related internal friction of Fe-17Mn (mass%) alloys [J]. ISIJ Int., 2008, 48: 99
|
| 4 |
Choi W S, De Cooman B C. Effect of carbon on the damping capacity and mechanical properties of thermally trained Fe-Mn based high damping alloys [J]. Mater. Sci. Eng., 2017, A700: 641
|
| 5 |
Jun J H, Choi C S. The influence of Mn content on microstructure and damping capacity in Fe-(17∼23)%Mn alloys [J]. Mater. Sci. Eng., 1998, A252: 133
|
| 6 |
Kim J C, Han D W, Baik S H, et al. Effects of alloying elements on martensitic transformation behavior and damping capacity in Fe-17Mn alloy [J]. Mater. Sci. Eng., 2004, A378: 323
|
| 7 |
Huang S K, Li N, Wen Y H, et al. Temperature dependence of the damping capacity in Fe-19.35Mn alloy [J]. J. Alloys Compd., 2008, 455: 225
|
| 8 |
Wang S H, Li J, Chai F, et al. Influence of solution temperature on γ→ε transformation and damping capacity of Fe-19Mn Alloy [J]. Acta Metall. Sin., 2020, 56: 1217
|
| 8 |
王世宏, 李 健, 柴 锋等. 固溶温度对Fe-19Mn合金的γ→ε相变和阻尼性能的影响 [J]. 金属学报, 2020, 56: 1217
|
| 9 |
Wang H J, Wang H, Zhang R Q, et al. Effect of high strain amplitude and pre-deformation on damping property of Fe-Mn alloy [J]. J. Alloys Compd., 2019, 770: 252
|
| 10 |
Huang S K, Li N, Wen Y H, et al. Effects of deep-cooling and temperature on damping capacity of Fe-Mn alloy [J]. Acta Metall. Sin., 2007, 43: 807
|
| 10 |
黄姝珂, 李 宁, 文玉华等. 深冷处理和温度对Fe-Mn合金阻尼性能的影响 [J]. 金属学报, 2007, 43: 807
|
| 11 |
Huang S K, Li N, Wen Y H, et al. Effect of Si and Cr on stacking fault probability and damping capacity of Fe-Mn alloy [J]. Mater. Sci. Eng., 2008, A479: 223
|
| 12 |
Shin S, Kwon M, Cho W, et al. The effect of grain size on the damping capacity of Fe-17 wt%Mn [J]. Mater. Sci. Eng., 2017, A683: 187
|
| 13 |
Wang H, Wang F, Liu H T, et al. Influence of alloy elements (Mo, Nb, Ti) on the strength and damping capacity of Fe-Cr based alloy [J]. Mater. Sci. Eng., 2016, A667: 326
|
| 14 |
Hughes D A, Hansen N, Bammann D J. Geometrically necessary boundaries, incidental dislocation boundaries and geometrically necessary dislocations [J]. Scr. Mater., 2003, 48: 147
|
| 15 |
Pierce D T, Jiménez J A, Bentley J, et al. The influence of manganese content on the stacking fault and austenite/ε-martensite interfacial energies in Fe-Mn-(Al-Si) steels investigated by experiment and theory [J]. Acta Mater., 2014, 68: 238
|
| 16 |
Cho S H, Kang K B, Jonas J J. Effect of manganese on recrystallisation kinetics of niobium microalloyed steel [J]. Mater. Sci. Technol., 2002, 18: 389
|
| 17 |
Takaki S, Nakatsu H, Tokunaga Y. Effects of austenite grain size on ε martensitic transformation in Fe-15mass%Mn Alloy [J]. Mater. Trans. JIM, 1993, 34: 489
|
| 18 |
Bracke L, Verbeken K, Kestens L, et al. Microstructure and texture evolution during cold rolling and annealing of a high Mn TWIP steel [J]. Acta Mater., 2009, 57: 1512
|
| 19 |
Zhao P C, Chen B, Zheng Z G, et al. Microstructure and texture evolution in a post-dynamic recrystallized titanium during annealing, monotonic and cyclic loading [J]. Metall. Mater. Trans., 2020, 52A: 394
|
| 20 |
Sevsek S, Brasche F, Molodov D A, et al. On the influence of grain size on the TWIP/TRIP-effect and texture development in high-manganese steels [J]. Mater. Sci. Eng., 2019, A754: 152
|
| 21 |
Ma Y L, Ge T S. Dislocation damping peaks appearing within the temperature range for the direct and inverse martensitic transformations of an iron-manganese alloy [J]. Acta Phys. Sin., 1964, 20: 909
|
| 21 |
马应良, 葛庭燧. 铁锰合金在正、反马氏体型相变温度范围内出现的位错内耗峰 [J]. 物理学报, 1964, 20: 909
|
| 22 |
Yang X S, Sun S, Ruan H H, et al. Shear and shuffling accomplishing polymorphic fcc γ→hcp ε→bct α martensitic phase transformation [J]. Acta Mater., 2017, 136: 347
|
| 23 |
Yang D P, Wu D, Yi H L. Reverse transformation from martensite into austenite in a medium-Mn steel [J]. Scr. Mater., 2019, 161: 1
|
| 24 |
Filho I R S, da Silva A K, Sandim M J R, et al. Martensite to austenite reversion in a high-Mn steel: Partitioning-dependent two-stage kinetics revealed by atom probe tomography, in-situ magnetic measurements and simulation [J]. Acta Mater., 2019, 166: 178
|
| 25 |
Li X, Wei L L, Chen L Q, et al. Work hardening behavior and tensile properties of a high-Mn damping steel at elevated temperatures [J]. Mater. Charact., 2018, 144: 575
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|