| 回火对钒钛微合金化Mn-Cr系贝氏体型非调质钢组织和性能的影响 |
王占花, 惠卫军( ), 谢志奇, 张永健, 赵晓丽 |
| 北京交通大学机械与电子控制工程学院 北京 100044 |
|
| Effects of Tempering Temperature on Microstructure and Mechanical Properties of a Mn-Cr Type Bainitic Forging Steel |
WANG Zhanhua, HUI Weijun( ), XIE Zhiqi, ZHANG Yongjian, ZHAO Xiaoli |
| School of Mechanical, Electronic and Control Engineering, Beijing Jiaotong University, Beijing 100044, China |
引用本文:
王占花, 惠卫军, 谢志奇, 张永健, 赵晓丽. 回火对钒钛微合金化Mn-Cr系贝氏体型非调质钢组织和性能的影响[J]. 金属学报, 2020, 56(11): 1441-1451.
Zhanhua WANG,
Weijun HUI,
Zhiqi XIE,
Yongjian ZHANG,
Xiaoli ZHAO.
Effects of Tempering Temperature on Microstructure and Mechanical Properties of a Mn-Cr Type Bainitic Forging Steel[J]. Acta Metall Sin, 2020, 56(11): 1441-1451.
| [1] |
Chen S L, Hui W J, Wang L H, et al. Research and development of energy-saving high performance microalloyed forging steels [J]. Iron Steel, 2014, 49(6): 1
|
| [1] |
(陈思联, 惠卫军, 王连海等. 节能低成本高品质非调质钢的研发 [J]. 钢铁, 2014, 49(6): 1)
|
| [2] |
Buchmayr B. Critical assessment 22: Bainitic forging steels [J]. Mater. Sci. Technol., 2016, 32: 517
doi: 10.1080/02670836.2015.1114272
|
| [3] |
Sourmail T, Smanio V. Optimisation of the mechanical properties of air cooled bainitic steel components through tailoring of the transformation kinetics [J]. Mater. Sci. Eng., 2013, A582: 257
|
| [4] |
Keul C, Wirths V, Bleck W. New bainitic steels for forgings [J]. Arch. Civ. Mech. Eng., 2012, 12: 119
doi: 10.1016/j.acme.2012.04.012
|
| [5] |
Wu H, Liu C, Zhao Z B, et al. Design of air-cooled bainitic microalloyed steel for a heavy truck front axle beam [J]. Mater. Des., 2006, 27: 651
|
| [6] |
Wang X Y. Development of new type non-quenched-tempered steels [J]. Spec. Steel, 2001, 22(2): 1
|
| [6] |
(汪学瑶. 新型非调质钢的发展 [J]. 特殊钢, 2001, 22(2): 1)
|
| [7] |
An Z G, Huang Y X, Hou H Y, et al. Continuous cooling transformation of bainite non-quenched and tempered steel for automobile front axle [J]. Iron Steel, 2016, 51(12): 70
|
| [7] |
(安治国, 黄艳新, 侯环宇等. 汽车前轴用贝氏体型非调质钢连续冷却转变 [J]. 钢铁, 2016, 51(12): 70)
|
| [8] |
Feng J Q, Wang G L, Zou M H, et al. Research on non-quenched-tempered steel for heavy truck front axle [J]. Autom. Technol. Mater., 2014, (4): 1
|
| [8] |
(冯佳奇, 王敢利, 邹敏华等. 重型汽车前轴用非调质钢的研究 [J]. 汽车工艺与材料, 2014, (4): 1)
|
| [9] |
Jiang Z H, Wang P, Li D Z, et al. Effects of tempering temperature on the microstructure and mechanical properties of granular bainite in 2.25Cr-1Mo-0.25V steel [J]. Acta Metall. Sin., 2015, 51: 925
|
| [9] |
(蒋中华, 王 培, 李殿中等. 回火温度对2.25Cr-1Mo-0.25V钢粒状贝氏体显微组织和力学性能的影响 [J]. 金属学报, 2015, 51: 925)
|
| [10] |
Wang K K, Tan Z L, Gao G H, et al. Ultrahigh strength-toughness combination in bainitic rail steel: The determining role of austenite stability during tempering [J]. Mater. Sci. Eng., 2016, A662: 162
|
| [11] |
Zhou Y L, Jia T, Zhang X J, et al. Investigation on tempering of granular bainite in an offshore platform steel [J]. Mater. Sci. Eng., 2015, A626: 352
|
| [12] |
Peng J M, Luo Y, Wang H B, et al. Effect of tempering temperature and time on mechanical property of non-quenched and tempered bainitic steel [J]. Shanghai Met., 2009, 31(3): 16
|
| [12] |
(彭金明, 罗 毅, 汪宏斌等. 回火温度和时间对贝氏体型非调质钢力学性能的影响 [J]. 上海金属, 2009, 31(3): 16)
|
| [13] |
Luo Y, Peng J M, Wang H B,et al. Effect of tempering on microstructure and mechanical properties of a non-quenched bainitic steel [J]. Mater. Sci. Eng., 2010, A527: 3433
|
| [14] |
Xu Z B, Hui W J, Wang Z H, et al. Mechanical properties of a microalloyed bainitic steel after hot forging and tempering [J]. J. Iron Steel Res. Int., 2017, 24: 1085
|
| [15] |
Wang Z H, Hui W J, Chen Z, et al. Effect of vanadium on microstructure and mechanical properties of bainitic forging steel [J]. Mater. Sci. Eng., 2020, A771: 138653
|
| [16] |
Shao C W, Hui W J, Zhang Y J, et al. Microstructure and mechanical properties of a novel cold rolled medium-Mn steel with superior strength and ductility [J]. Acta Metall. Sin., 2019, 55: 191
|
| [16] |
(邵成伟, 惠卫军, 张永健等. 一种新型高强度高塑性冷轧中锰钢的组织和力学性能 [J]. 金属学报, 2019, 55: 191)
|
| [17] |
Gao G H, Zhang H, Bai B Z. Effect of tempering temperature on low temperature impact toughness of a low carbon Mn-series bainitic steel [J]. Acta Metall. Sin., 2011, 47: 513
|
| [17] |
(高古辉, 张 寒, 白秉哲. 回火温度对Mn系低碳贝氏体钢的低温韧性的影响 [J]. 金属学报, 2011, 47: 513)
|
| [18] |
Wang H C, Zhou C, Xu F,et al. Optimization experimental research on 42CrMo steel used in the fastener for rail transportation [J]. Metall. Eng., 2015, 2(4): 198
|
| [18] |
(王海川, 周 超, 徐 飞等. 轨道交通紧固件用钢42CrMo的优化试验研究 [J]. 冶金工程, 2015, 2(4): 198)
|
| [19] |
Li X Y. Jiuquan steel production of 40Cr steel heat treatment process test research [J]. Gansu Metall., 2015, 37(1): 64
|
| [19] |
(李晓燕. 对酒钢生产的40Cr钢热处理工艺试验研究 [J]. 甘肃冶金, 2015, 37(1): 64)
|
| [20] |
Wan D C, Cai Q W, Yu W, et al. Tempering microstructure and mechanical properties of an ultra high strength bainitic steel [J]. Trans. Mater. Heat Treat., 2013, 34(5): 143
|
| [20] |
(万德成, 蔡庆伍, 余 伟等. 超高强贝氏体钢的回火组织与力学性能 [J]. 材料热处理学报, 2013, 34(5): 143)
|
| [21] |
Srivatsa K, Srinivas P, Balachandran G, et al. Room temperature microstructure and property evaluation of a heat treated fully bainitic 20CrMoVTiB410 Steel [J]. JOM, 2016, 68: 2704
|
| [22] |
Jiao D T, Cai Q W, Wu H B. Effects of cooling process after rolling on microstructure and yield ratio of high-strain pipeline steel X80 [J]. Acta Metall. Sin., 2009, 45: 1111
|
| [22] |
(焦多田, 蔡庆伍, 武会宾. 轧后冷却制度对X80级抗大变形管线钢组织和屈强比的影响 [J]. 金属学报, 2009, 45: 1111)
|
| [23] |
DeArdo A J. Multi-phase microstructures and their properties in high strength low carbon steels [J]. ISIJ Int., 1995, 35: 946
|
| [24] |
Zhao H, Wang X M, Zhang X F, et al. Effect of tempering on microstructure and mechanical properties of low carbon bainitic steel [A]. Proceedings of the 8th (2011) China Iron and Steel Annual Conference [C]. Beijing: China Metal Society, 2011: 6
|
| [24] |
(赵 慧, 王学敏, 张小帆等. 回火对低碳贝氏体钢组织与性能的影响 [A]. 第八届(2011)中国钢铁年会论文集 [C]. 北京: 中国金属学会, 2011: 6)
|
| [25] |
Li Z J, Xiao N M, Li D Z, et al. Influence of microstructure on impact toughness of G18CrMo2-6 steel during tempering [J]. Acta Metall. Sin., 2014, 50: 777
|
| [25] |
(李振江, 肖纳敏, 李殿中等. G18CrMo2-6钢回火组织及冲击韧性研究 [J]. 金属学报, 2014, 50: 777)
|
| [26] |
Li B Z, Li C S, Jin X, et al. Effect of M-A constituents formed in thermo-mechanical controlled process on toughness of 20CrNi2MoV steel [J]. J. Iron Steel Res. Int., 2019, 26: 1340
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |