| TiC含量对铁基复合材料力学性能及耐磨性能的影响 |
董虎林,包海萍,彭建洪( ) |
| 青海民族大学物理与电子信息工程学院 西宁 810007 |
|
| Effect of TiC Contents on Mechanical Properties and Wear Resistance of Iron-Based Composites |
Hulin DONG,Haiping BAO,Jianhong PENG( ) |
| Department of Physics and Electron Information Engineering, Qinghai University for Nationality, Xining 810007, China |
引用本文:
董虎林,包海萍,彭建洪. TiC含量对铁基复合材料力学性能及耐磨性能的影响[J]. 金属学报, 2019, 55(8): 1049-1057.
Hulin DONG,
Haiping BAO,
Jianhong PENG.
Effect of TiC Contents on Mechanical Properties and Wear Resistance of Iron-Based Composites[J]. Acta Metall Sin, 2019, 55(8): 1049-1057.
| [1] | Uematsu Y, Kakiuchi T, Tokaji K, et al. Effects of shot peening on fatigue behavior in high speed steel and cast iron with spheroidal vanadium carbides dispersed within martensitic-matrix microstructure [J]. Mater. Sci. Eng., 2013, A561: 386 | | [2] | Cao Y B, Zhi S X, Gao Q, et al. Formation behavior of in-situ NbC in Fe-based laser cladding coatings [J]. Mater. Charact., 2016, 119: 159 | | [3] | Zhao N N, Xu Y H, Wang J F, et al. Microstructure and kinetics study on tantalum carbide coating produced on gray cast iron in situ [J]. Surf. Coat. Technol., 2016, 286: 347 | | [4] | Zhong L S, Zhang X, Chen S L, et al. Fe-W-C thermodynamics and in situ preparation of tungsten carbide-reinforced iron-based surface composites by solid-phase diffusion [J]. Int. J. Refract. Met. Hard Mater., 2016, 57: 42 | | [5] | Song Q S, Xu Q, Xu L, et al. Synthesis of Ni-TiC composite powder electrochemically in molten chlorides [J]. J. Alloys Compd., 2017, 690: 116 | | [6] | Zhao X B, Zhuo Y G, Liu S, et al. Investigation on WC/TiC interface relationship in wear-resistant coating by first-principles [J]. Surf. Coat. Technol., 2016, 305: 200 | | [7] | Chen L Q, Guo J H, Wang J J, et al. Tensile deformation and fracture behavior of AZ91D magnesium alloy and TiC/Mg magnesium matrix composites synthesized by in situ reactive infiltration technique [J]. Rare Met. Mater. Eng., 2006, 35: 29 | | [7] | (陈礼清, 郭金花, 王继杰等. 原位反应自发渗透法TiC/AZ91D镁基复合材料及AZ91D镁合金的拉伸变形与断裂行为 [J]. 稀有金属材料与工程, 2006, 35: 29) | | [8] | Andrieux J, Gardiola B, Dezellus O. Synthesis of Ti matrix composites reinforced with TiC particles: in situ synchrotron X-ray diffraction and modeling [J]. J. Mater. Sci., 2018, 53: 9533 | | [9] | Sun X L, Han Y F, Cao S H, et al. Rapid in-situ reaction synthesis of novel TiC and carbon nanotubes reinforced titanium matrix composites [J]. J. Mater. Sci. Technol., 2017, 33: 1165 | | [10] | Song M S, Zhang J, Li Y, et al. Investigation of Al-matrix composites reinforced by TiC particulates synthesized from melt and corresponding properties [J]. Hot Working Technol., 2017, 46(20): 116 | | [10] | (宋谋胜, 张 杰, 李 勇等. 熔体内合成TiC颗粒增强Al基复合材料及其性能研究 [J]. 热加工工艺, 2017, 46(20): 116) | | [11] | Li Y Y, Ni K Y, Zhu F W. Study of TiC particle-reinforced Cu matrix composites [J]. Powder Metall. Technol., 2018, 36: 106 | | [11] | (李月英, 倪慨宇, 祝夫文. TiC颗粒增强铜基复合材料的研究 [J]. 粉末冶金技术, 2018, 36: 106) | | [12] | Ma S B, Xia Z W, Xu Y, et al. Microstructure and abrasion resistance of in-situ TiC particles reinforced Ni-based composite coatings by laser cladding [J]. J. Mater. Eng., 2017, 45(6): 24 | | [12] | (马世榜, 夏振伟, 徐 杨等. 激光熔覆原位自生TiC颗粒增强镍基复合涂层的组织与耐磨性 [J]. 材料工程, 2017, 45(6): 24) | | [13] | Ni Z F, Sun Y S, Xue F, et al. Microstructure and properties of austenitic stainless steel reinforced with in situ TiC particulate [J]. Mater. Des., 2011, 32: 1462 | | [14] | Akhtar F, Guo S J. Microstructure, mechanical and fretting wear properties of TiC-stainless steel composites [J]. Mater. Charact., 2008, 59: 84 | | [15] | Almangour B, Grzesiak D, Yang J M. In situ formation of TiC-particle-reinforced stainless steel matrix nanocomposites during ball milling: Feedstock powder preparation for selective laser melting at various energy densities [J]. Powder Technol., 2018, 326: 467 | | [16] | Ni Z F, Sun Y S, Xue F, et al. Evaluation of electroslag remelting in TiC particle reinforced 304 stainless steel [J]. Mater. Sci. Eng., 2011, A528: 5664 | | [17] | Tang H Q, Su G C, Zhan Y Z, et al. Microstructure characterisation of insitu TiC particulates reinforced Fe-based composites [J]. Mater. Res. Innovations, 2015, 19(Suppl.): S5-152 | | [18] | Zhong L S, Xu Y H, Hojamberdiev M, et al. In situ fabrication of titanium carbide particulates-reinforced iron matrix composites [J]. Mater. Des., 2011, 32: 3790 | | [19] | Sharifitabar M, Khaki J V, Sabzevar M H. Microstructure and wear resistance of in-situ TiC-Al2O3 particles reinforced Fe-based coatings produced by gas tungsten arc cladding [J]. Surf. Coat. Technol., 2016, 285: 47 | | [20] | Liu X Y, Zheng K H, Luo T G, et al. Three body abrasive wear properties of in-situ TiC iron matrix composites [J]. Foundry Technol., 2018, 39: 976 | | [20] | (刘相熠, 郑开宏, 罗铁钢等. 自生TiC铁基复合材料的三体磨料磨损性能的工艺探究 [J]. 铸造技术, 2018, 39: 976) | | [21] | Zhong L S, Ye F X, Xu Y H, et al. Microstructure and abrasive wear characteristics of in situ vanadium carbide particulate-reinforced iron matrix composites [J]. Mater. Des., 2014, 54: 564 | | [22] | Peng J H, Dong H L, Hojamberdiev M, et al. Improving the mechanical properties of tantalum carbide particle-reinforced iron-based composite by varying the TaC contents [J]. J. Alloys Compd., 2017, 726: 896 | | [23] | Ding Y C, Wang Y S, Wang J, et al. Structure and properties of V8C7 matrix composite fabricated in-situ [J]. J. Sichuan Univ. (Eng. Sci. Ed.), 2007, 39(4): 113 | | [23] | (丁义超, 王一三, 王静等. 原位合成V8C7颗粒增强铁基复合材料的结构和性能 [J]. 四川大学学报(工程科学版), 2007, 39(4): 113) | | [24] | Wang Z, Lin T, He X B, et al. Microstructure and properties of TiC-high manganese steel cermet prepared by different sintering processes [J]. J. Alloys Compd., 2015, 650: 918 | | [25] | Bikerman J J. Ploughing and adhesion of sliding metals [J]. J. Appl. Phys., 1943, 14: 436 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|