| Hi-B钢二次再结晶退火中异常长大Goss取向晶粒的三维形貌表征 |
鲍思前( ), 刘兵兵, 赵刚, 徐洋, 柯珊珊, 胡晓, 刘磊 |
| 武汉科技大学省部共建耐火材料与冶金国家重点实验室 武汉 430081 |
|
| Three-Dimensional Morphologies of Abnormally Grown Goss Oriented Grains in Hi-B Steel During Secondary Recrystallization Annealing |
Siqian BAO( ), Bingbing LIU, Gang ZHAO, Yang XU, Shanshan KE, Xiao HU, Lei LIU |
| The State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081,China |
引用本文:
鲍思前, 刘兵兵, 赵刚, 徐洋, 柯珊珊, 胡晓, 刘磊. Hi-B钢二次再结晶退火中异常长大Goss取向晶粒的三维形貌表征[J]. 金属学报, 2018, 54(6): 877-885.
Siqian BAO,
Bingbing LIU,
Gang ZHAO,
Yang XU,
Shanshan KE,
Xiao HU,
Lei LIU.
Three-Dimensional Morphologies of Abnormally Grown Goss Oriented Grains in Hi-B Steel During Secondary Recrystallization Annealing[J]. Acta Metall Sin, 2018, 54(6): 877-885.
| [1] | He Z Z, Zhao Y, Luo H W.Electrical Steel [M]. Beijing: Metallurgical Industry Press, 2012: 102(何忠治, 赵宇, 罗海文. 电工钢[M]. 北京: 冶金工业出版社, 2012: 102) | | [2] | Dunn C G, Lionetti F.The effect of orientation difference on grain boundary energies[J]. Trans. AIME, 1949, 185: 125 | | [3] | Dunn C G, Daniels F W, Bolton M J.Measurement of relative interface energies in twin related crystals[J]. Trans. AIME, 1950, 188: 368 | | [4] | Hillert M.On the theory of normal and abnormal grain growth[J]. Acta Metall., 1965, 13: 227 | | [5] | Shimizu R, Harase J.Coincidence grain boundary and texture evolution in Fe-3%Si[J]. Acta Metall., 1989, 37: 1241 | | [6] | Harase J, Shimizu R.Distribution of {100}<001> oriented grains in the primary recrystallized 3%Si-Fe alloy[J]. Trans. Jpn. Inst. Met., 1988, 29: 388 | | [7] | Harase J, Shimizu R, Dingley D J.Texture evolution in the presence of precipitates in Fe-3%Si alloy[J]. Acta Metall. Mater., 1991, 39: 763 | | [8] | Hayakawa Y, Szpunar J A.The role of grain boundary character distribution in secondary recrystallization of electrical steels[J]. Acta Mater., 1997, 45: 1285 | | [9] | Rajmohan N, Szpunar J A, Hayakawa Y.A role of fractions of mobile grain boundaries in secondary recrystallization of Fe-Si steels[J]. Acta Mater., 1999, 47: 2999 | | [10] | Komatsubara M, Hayakawa Y, Takamiya T, et al. Newly developed grain-oriented Si-steel with thinner gauges[J]. J. Phys. IV France, 1998, 8(PR2): Pr2-467 | | [11] | Park H, Kim D Y, Hwang N M, et al.Microstructural evidence of abnormal grain growth by solid-state wetting in Fe-3%Si steel[J]. J. Appl. Phys., 2004, 95: 5515 | | [12] | Lee D K, Ko K J, Lee B J, et al.Monte Carlo simulations of abnormal grain growth by sub-boundary-enhanced solid-state wetting[J]. Scr. Mater., 2008, 58: 683 | | [13] | Ko K J, Park J T, Kim J K, et al.Morphological evidence that Goss abnormally growing grains grow by triple junction wetting during secondary recrystallization of Fe-3%Si steel[J]. Scr. Mater., 2008, 59: 764 | | [14] | Fan X M, Lin Y, Huang J W, et al.The three-dimensional morphology reconstruction of boride layer on armco iron based on serial sectioning[J]. Mater. Sci. Technol., 2013, 21(6): 17(樊新民, 林银, 黄洁雯等. 基于系列磨片的纯铁渗硼层形貌三维重建[J]. 材料科学与工艺, 2013, 21(6): 17) | | [15] | Morito S, Edamatsu Y, Ichinotani K, et al.Quantitative analysis of three-dimensional morphology of martensite packets and blocks in iron-carbon-manganese steels[J]. J. Alloys Compd., 2013, 577(suppl.1): S587 | | [16] | Wu K M, Enomoto M.Three-dimensional analysis of degenerate ferrite in an Fe-C-Mo alloy[J]. Chin. J. Stereol. Image Anal., 2004, 9: 134(吴开明, Enomoto M.Fe-C-Mo合金中退化铁素体的三维分析[J]. 中国体视学与图像分析, 2004, 9: 134) | | [17] | Wu K M.3-D morphology observation of degenerate ferrite in steel Fe-0.28C-3.0Mo using serial sectioning and computer-aided reconstruction[J]. Acta Metall. Sin., 2005, 41: 1237(吴开明. 连续截面和计算机辅助重建法观察Fe-0.28C-3.0Mo合金钢退化铁素体的三维形貌[J]. 金属学报, 2005, 41: 1237) | | [18] | Li Y, Xu L, Li S M, et al.Three-dimensional microstructure morphology of ZL102 Al-Si alloy[J]. Foundry, 2015, 64: 814(李英, 徐磊, 李双明等. ZL102铝硅合金的三维显微组织形态研究[J]. 铸造, 2015, 64: 814) | | [19] | Luan J H, Liu G Q, Wang H.Three-dimensional reconstruction of grains in pure iron specimen[J]. Acta Metall. Sin., 2011, 47: 69(栾军华, 刘国权, 王浩. 纯Fe试样中晶粒的三维可视化重建[J]. 金属学报, 2011, 47: 69) | | [20] | Bao S Q, Xu Y, Zhao G, et al.Microstructure, texture and precipitates of grain-oriented silicon steel produced by thin slab casting and rolling process[J]. J. Iron Steel Res., Int., 2017, 24: 91 | | [21] | Huang X B, Bao S Q, Zhao G, et al.Primary recrystallization kinetics and texture evolution during annealing of low temperature grain-oriented silicon steel[J]. J. Iron Steel Res., 2017, 29: 577(黄祥斌, 鲍思前, 赵刚等. 低温取向硅钢初次再结晶动力学模型及织构演变[J]. 钢铁研究学报, 2017, 29: 577) | | [22] | Xu Y, Bao S Q, Zhao G, et al.Three-dimensional morphologies of different oriented grains in Hi-B steel formed during early stage of secondary recrystallization annealing[J]. Acta Metall. Sin., 2017, 53: 539(徐洋, 鲍思前, 赵刚等. Hi-B钢二次再结晶退火初期不同取向晶粒的三维形貌表征[J]. 金属学报, 2017, 53: 539) | | [23] | Shirdel M, Mirzadeh H, Parsa M H.Abnormal grain growth in AISI 304L stainless steel[J]. Mater. Charact., 2014, 97: 11 | | [24] | Chen N, Zaefferer S, Lahn L, et al.Effects of topology on abnormal grain growth in silicon steel[J]. Acta Mater., 2003, 51: 1755 | | [25] | Hwang N M.Simulation of the effect of anisotropic grain boundary mobility and energy on abnormal grain growth[J]. J. Mater. Sci., 1998, 33: 5625 | | [26] | Yan M Q, Qian H, Yang P, et al.Analysis of micro-texture during secondary recrystallization in a Hi-B electrical steel[J]. J. Mater. Sci. Technol., 2011, 27: 1065 |
|
|