Hi-B钢二次再结晶退火初期不同取向晶粒的三维形貌表征 |
徐洋,鲍思前( ),赵刚,黄祥斌,黄儒胜,刘兵兵,宋娜娜 |
武汉科技大学省部共建耐火材料与冶金国家重点实验室 武汉 430081 |
|
Three-Dimensional Morphologies of Different Oriented Grains in Hi-B Steel Formed During Early Stage of Secondary Recrystallization Annealing |
Yang XU,Siqian BAO( ),Gang ZHAO,Xiangbin HUANG,Rusheng HUANG,Bingbing LIU,Nana SONG |
The State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081, China |
引用本文:
徐洋,鲍思前,赵刚,黄祥斌,黄儒胜,刘兵兵,宋娜娜. Hi-B钢二次再结晶退火初期不同取向晶粒的三维形貌表征[J]. 金属学报, 2017, 53(5): 539-548.
Yang XU,
Siqian BAO,
Gang ZHAO,
Xiangbin HUANG,
Rusheng HUANG,
Bingbing LIU,
Nana SONG.
Three-Dimensional Morphologies of Different Oriented Grains in Hi-B Steel Formed During Early Stage of Secondary Recrystallization Annealing[J]. Acta Metall Sin, 2017, 53(5): 539-548.
[1] | Goss N P.Electrical sheet and method and apparatus for its manufacture and test [P]. US Pat., 1965559, 1934 | [2] | Littmann M F, Heek J E.Process of increasing the permeability of oriented silicon steels [P]. US Pat., 2599340, 1952 | [3] | Littmann M F.Structures and magnetic properties of grain-oriented 3.2% silicon-iron[J]. J. Appl. Phys., 1967, 38: 1104 | [4] | Hillert M.On the theory of normal and abnormal grain growth[J]. Acta Metall., 1965, 13: 227 | [5] | Harase J, Shimizu R.Distribution of {100}<001> oriented grains in the primary recrystallized 3%Si-Fe alloy[J]. Trans. Jpn. Inst. Met., 1988, 29: 388 | [6] | Shimizu R, Harase J.Coincidence grain boundary and texture evolution in Fe-3%Si[J]. Acta Metall., 1989, 37: 1241 | [7] | Hayakawa Y, Szpunar J A, Palumbo G, et al.The role of grain boundary character distribution in Goss texture development in electrical steels[J]. J. Magn. Magn. Mater., 1996, 160: 143 | [8] | Rajmohan N, Szpunar J A.An analytical method for characterizing grain boundaries around growing Goss grains during secondary recrystallization[J]. Scr. Mater., 2001, 44: 2387 | [9] | Hayakawa Y, Kurosawa M.Orientation relationship between primary and secondary recrystallized texture in electrical steel[J]. Acta Mater., 2002, 50: 4527 | [10] | Park H, Kim D Y, Hwang N M, et al.Microstructural evidence of abnormal grain growth by solid-state wetting in Fe-3%Si steel[J]. J. Appl. Phys., 2004, 95: 5515 | [11] | Wu K M, Enomoto M.Three-dimensional analysis of degenerate ferrite in an Fe-C-Mo alloy[J]. Chin. J. Stereol. Image Anal., 2004, 9: 134 | [11] | (吴开明, Enomoto M.Fe-C-Mo合金中退化铁素体的三维分析[J]. 中国体视学与图像分析, 2004, 9: 134) | [12] | Wu K M.3-D morphology observation of degenerate ferrite in steel Fe-0.28C-3.0Mo using serial sectioning and computer-aided reconstruction[J]. Acta Metall. Sin., 2005, 41: 1237 | [12] | (吴开明. 连续截面和计算机辅助重建法观察Fe-0.28C-3.0Mo合金钢退化铁素体的三维形貌[J]. 金属学报, 2005, 41: 1237) | [13] | Luan J H, Liu G Q, Wang H.Three-dimensional reconstruction of grains in pure iron specimen[J]. Acta Metall. Sin., 2011, 47: 69 | [13] | (栾军华, 刘国权, 王浩. 纯Fe试样中晶粒的三维可视化重建[J]. 金属学报, 2011, 47: 69) | [14] | Zhang Q.Curvature-driven grain growth by cellular automaton simulation in isothermal process [D]. Shenyang: Northeastern University, 2012 | [14] | (张倩. 等温过程曲率驱动晶粒长大的元胞自动机模拟 [D]. 沈阳: 东北大学, 2012) | [15] | He Z Z, Zhao Y, Luo H W.Electrical Steel [M]. Beijing: Metallurgical Industry Press, 2012: 102 | [15] | (何忠治, 赵宇, 罗海文. 电工钢[M]. 北京: 冶金工业出版社, 2012: 102) | [16] | Gottstein G, Molodov D A, Shvindlerman L S.Grain boundary migration in metals: Recent developments[J]. Interf. Sci., 1998, 6: 7 | [17] | Burke J E, Turnbull D.Recrystallization and grain growth[J]. Prog. Metal Phys., 1952, 3: 220 | [18] | Lin P, Palumbo G, Harase J, et al.Coincidence site lattice (CSL) grain boundaries and Goss texture development in Fe-3%Si alloy[J]. Acta Mater., 1996, 44: 4677 | [19] | Takamiya T, Kurosawa M, Komatsubara M. Effect of hydrogen content in the final annealing atmosphere on secondary recrystallization of grain-oriented Si steel [J]. J. Magn. Magn. Mater., 2003, 254-255: 334 | [20] | Yan M Q, Qian H, Yang P, et al.Analysis of micro-texture during secondary recrystallization in a Hi-B electrical steel[J]. J. Mater. Sci. Technol., 2011, 27: 1065 | [21] | Wang H, Luo L J, Wang J A.Formation and growth of cubic grains during rolling-annealing process in Fe-3.2%Si alloy[J]. Trans. Mater. Heat Treat., 2012, 33(5): 70 | [21] | (王辉, 骆靓鉴, 王均安. 铁硅合金轧制-退火过程中立方取向晶粒的形核与长大[J]. 材料热处理学报, 2012, 33(5): 70) | [22] | Zhou B X.Issues concerning the formation of cube texture of silicon-iron alloy[J]. Baosteel Technol., 2000, (5): 52 | [22] | (周邦新. 铁硅合金中形成立方织构的有关问题[J]. 宝钢技术, 2000, (5): 52) | [23] | Park H K, Park C S, Na T W, et al.Irregular or smooth grain boundaries evolved after secondary recyrstallization of Fe-3%Si steel[J]. Mater. Trans., 2012, 53: 658 | [24] | Park J Y, Szpunar J A. Influence of the primary recrystallization texture on abnormal grain growth of Goss grains in grain oriented electrical steels [J]. Mater. Sci. Forum, 2002, 408-412: 821 | [25] | Nakashima S, Takashima K, Harase J.Effect of silicon content on secondary recrystallization in grain-oriented electrical steel produced by single-stage cold rolling process[J]. ISIJ Int., 1991, 31: 1007 | [26] | Jiang S H, Mao W M, Yang P, et al.Recrystallization behavior of warm rolled Fe-6.5%Si alloy sheet[J]. J. Univ. Sci. Technol. Beijing, 2014, 36: 1643 | [26] | (蒋虽合, 毛卫民, 杨平等. Fe-6.5%Si合金温轧后退火过程中再结晶行为[J]. 北京科技大学学报, 2014, 36: 1643) | [27] | Liu Z Q, Yang P, Mao W M, et al.Effect of {114}<418> texture on abnormal growth during secondary recrystallization in grain-oriented steel[J]. Acta Metall. Sin., 2015, 51: 769 | [27] | (刘志桥, 杨平, 毛卫民等. 取向硅钢中{114}<418>织构对二次再结晶时晶粒异常长大的影响[J]. 金属学报, 2015, 51: 769) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|