| 冷却速率对Ti-V-Mo复合微合金钢组织转变及力学性能的影响 |
张可1,2( ), 李昭东3, 隋凤利1,2, 朱正海1,2, 章小峰1,2, 孙新军3, 黄贞益1,2, 雍岐龙3 |
1 安徽工业大学冶金减排与资源综合利用教育部重点实验室 马鞍山 243032 2 安徽工业大学冶金工程学院 马鞍山 243032 3 钢铁研究总院工程用钢所 北京 100081 |
|
| Effect of Cooling Rate on Microstructure Evolution and Mechanical Properties of Ti-V-Mo Complex Microalloyed Steel |
Ke ZHANG1,2( ), Zhaodong LI3, Fengli SUI1,2, Zhenghai ZHU1,2, Xiaofeng ZHANG1,2, Xinjun SUN3, Zhenyi HUANG1,2, Qilong YONG3 |
1 Key Laboratory of Metallurgical Emission Reduction & Resources Recycling (Anhui University of Technology), Ministry of Education, Maanshan 243032, China; 2 School of Metallurgical Engineering, Anhui University of Technology, Maanshan 243032, China 3 Institute of Structural Steels, Central Iron and Steel Research Institute, Beijing 100081, China |
引用本文:
张可, 李昭东, 隋凤利, 朱正海, 章小峰, 孙新军, 黄贞益, 雍岐龙. 冷却速率对Ti-V-Mo复合微合金钢组织转变及力学性能的影响[J]. 金属学报, 2018, 54(1): 31-38.
Ke ZHANG,
Zhaodong LI,
Fengli SUI,
Zhenghai ZHU,
Xiaofeng ZHANG,
Xinjun SUN,
Zhenyi HUANG,
Qilong YONG.
Effect of Cooling Rate on Microstructure Evolution and Mechanical Properties of Ti-V-Mo Complex Microalloyed Steel[J]. Acta Metall Sin, 2018, 54(1): 31-38.
| [1] | Jiao Z B, Liu J C.Research and development of advanced nano-precipitate strengthened ultra-high strength steels[J]. Mater. China, 2011, 30(12): 6(焦增宝, 刘锦川. 新型纳米强化超高强度钢的研究与进展[J]. 中国材料进展, 2011, 30(12): 6) | | [2] | Jiao Z B, Luan J H, Miller M K, et al.Co-precipitation of nanoscale particles in steels with ultra-high strength for a new era[J]. Mater. Today, 2017, 20: 142 | | [3] | Lv Z P, Jiang S H, He J Y, et al.Second phase strengthening in advanced metal materials[J]. Acta Metall. Sin., 2016, 52: 1183(吕昭平, 蒋虽合, 何骏阳等. 先进金属材料的第二相强化[J]. 金属学报, 2016, 52: 1183) | | [4] | Kim Y W, Kim J H, Hong S G, et al.Effects of rolling temperature on the microstructure and mechanical properties of Ti-Mo microalloyed hot-rolled high strength steel[J]. Mater. Sci. Eng., 2014, A605: 244 | | [5] | Chen J, Lv M Y, Tang S, et al.Microstructure, mechanical properties and interphase precipitation behaviors in V-Ti microalloyed steel[J]. Acta Metall. Sin., 2014, 50: 524(陈俊, 吕梦阳, 唐帅等. V-Ti微合金钢的组织性能及相间析出行为[J]. 金属学报, 2014, 50: 524) | | [6] | Mukherjee S, Timokhina I, Zhu C, et al.Clustering and precipitation processes in a ferritic titanium-molybdenum microalloyed steel[J]. J. Alloys Compd., 2017, 690: 621 | | [7] | Phaniraj M.P, Shin Y M, Lee J, et al.. Development of high strength hot rolled low carbon copper-bearing steel containing nanometer sized carbides[J]. Mater. Sci. Eng., 2015, A633: 1 | | [8] | Li X L, Wang Z D.Interphase precipitation behaviors of nanometer-sized carbides in a Nb-Ti-bearing low-carbon microalloyed steel[J]. Acta Metall. Sin., 2015, 51: 417(李小琳, 王昭东. 含Nb-Ti低碳微合金钢中纳米碳化物的相间析出行为[J]. 金属学报, 2015, 51: 417) | | [9] | Chen C Y, Chen C C, Yang J R.Microstructure characterization of nanometer carbides heterogeneous precipitation in Ti-Nb and Ti-Nb-Mo steel[J]. Mater. Charact., 2014, 88: 69 | | [10] | Yi H L, Du L X, Wang G D, et al.Development of Nb-V-Ti hot-rolled high strength steel with fine ferrite and precipitation strengthening[J]. J. Iron Steel Res. Int., 2009, 16(4): 72 | | [11] | Li X L, Wang Z D, Deng X T, et al.Effect of final temperature after ultra-fast cooling on microstructural evolution and precipitation behavior of Nb-V-Ti bearing low alloy steel[J]. Acta Metall. Sin., 2015, 51: 784(李小琳, 王昭东, 邓想涛等. 超快冷终冷温度对含Nb-V-Ti微合金钢组织转变及析出行为的影响[J]. 金属学报, 2015, 51: 784) | | [12] | Zhang K, Yong Q L, Sun X J, et al.Effect of coiling temperature on microstructure and mechanical properties of Ti-V-Mo complex microalloyed ultra-high strength steel[J]. Acta Metall. Sin., 2016, 52: 529(张可, 雍岐龙, 孙新军等. 卷取温度对Ti-V-Mo复合微合金化超高强度钢组织及力学性能的影响[J]. 金属学报, 2016, 52: 529) | | [13] | Olasolo M, Uranga P, Rodriguez-Ibabe J M, et al.. Effect of austenite microstructure and cooling rate on transformation characteristics in a low carbon Nb-V microalloyed steel[J]. Mater. Sci. Eng., 2011, A528: 2559 | | [14] | Wang Q, Sun T T, Bai Y Q.Effect of cooling rate on microstructure and mechanical properties of ultra-low carbon micro-alloyed steel[J]. Heat Treat. Met., 2015, 40(2): 148(王权, 孙婷婷, 白雅琼. 冷却速度对超低碳微合金钢组织和性能的影响[J]. 金属热处理, 2015, 40(2): 148) | | [15] | Ma F J, Wen G H, Tang P, et al.Effect of cooling rate on the precipitation behavior of carbonitride in microalloyed steel slab[J]. Metall. Mater. Trans., 2011, 42B: 81 | | [16] | Xu Y, Sun M X, Zhou Y L, et al.Precipitation behavior of (Nb, Ti)C in coiling process and its effect on micro-mechanical characteristics of ferrite[J]. Acta Metall. Sin., 2015, 51: 31(徐洋, 孙明雪, 周砚磊等. (Nb, Ti)C在轧后卷取中的析出及对铁素体相微观力学特征的影响[J]. 金属学报, 2015, 51: 31) | | [17] | Sha Q Y, Li G Y, Yan P Y, et al.Effect of cooling rate and coiling temperature on the precipitates in ferrite of Nb-V-Ti microalloyed complex strip steel[J]. Mater. China, 2011, 30(12): 23(沙庆云, 李桂艳, 严平沅等. 冷却速度和卷取温度对Nb-V-Ti复合微合金带钢铁素体中析出的影响[J]. 中国材料进展, 2011, 30(12): 23) | | [18] | Zajac S, Siwecki T, Hutchinson B, et al.Recrystallization controlled rolling and accelerated cooling for high strength and toughness in V-Ti-N steels[J]. Metall. Mater. Trans., 1991, 22A: 2681 | | [19] | Manohar P A, Chandra T.Continuous cooling transformation behaviour of high strength microalloyed steels for linepipe applications[J]. ISIJ Int., 1998, 38: 766 | | [20] | Zhang K, Li Z D, Wang Z Q, et al.Precipitation behavior and mechanical properties of hot-rolled high strength Ti-Mo-bearing ferritic sheet steel: The great potential of nanometer-sized (Ti, Mo)C carbide[J]. J. Mater. Res., 2016, 31: 1254 | | [21] | Yong Q L, Ma M T, Wu B R.Microalloyed Steel─Physical and Mechanical Metallurgy [M]. Beijing: China Machine Press, 1989: 65(雍岐龙, 马鸣图, 吴宝榕. 微合金钢─物理和力学冶金 [M]. 北京: 机械工业出版社, 1989: 65) | | [22] | Gladman T, McIvor I D, Pickering F B. Some aspects of the structure-property relationships in high-carbon ferrite-pearlite steels[J]. J. Iron Steel Inst., 1972, 210: 916 | | [23] | Kim Y W, Song S W, Seo S J, et al.Development of Ti and Mo micro-alloyed hot-rolled high strength sheet steel by controlling thermomechanical controlled processing schedule[J]. Mater. Sci. Eng., 2013, A565: 430 | | [24] | Zhang K, Li Z D, Sun X J, et al.Development of Ti-V-Mo complex microalloyed hot-rolled 900-MPa-Grade high-strength steel[J]. Acta Metall. Sin.(Engl. Lett.), 2015, 28: 641 | | [25] | Pavlina E J, Van Tyne C J. Correlation of yield strength and tensile strength with hardness for steels[J]. J. Mater. Eng. Perform., 2008, 17: 888 | | [26] | Xu Y.Study on ferrite transformation and nano-precipitation behaviors and mechanism of Ti micro-alloyed steel [D]. Shenyang: Northeastern University, 2015(徐洋. 钛微合金化钢中铁素体相变及纳米相析出行为与机理研究 [D]. 沈阳: 东北大学, 2015) |
|
|