| Cu的析出及其对FeCrMoCu合金阻尼性能和力学性能的影响 |
胡小锋1( ),杜瑜宾1,2,闫德胜1,戎利建1 |
1 中国科学院金属研究所中国科学院核用材料与安全评价重点实验室 沈阳 110016 2 中国科学技术大学材料科学与工程学院 沈阳 110016 |
|
| Cu Precipitation and Its Effect on Damping Capacity and Mechanical Properties of FeCrMoCu Alloy |
Xiaofeng HU1( ),Yubin DU1,2,Desheng YAN1,Lijian RONG1 |
1 CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China |
引用本文:
胡小锋,杜瑜宾,闫德胜,戎利建. Cu的析出及其对FeCrMoCu合金阻尼性能和力学性能的影响[J]. 金属学报, 2017, 53(5): 601-608.
Xiaofeng HU,
Yubin DU,
Desheng YAN,
Lijian RONG.
Cu Precipitation and Its Effect on Damping Capacity and Mechanical Properties of FeCrMoCu Alloy[J]. Acta Metall Sin, 2017, 53(5): 601-608.
| [1] | Hu X F, Li X Y, Zhang B, et al.Magnetic domain structure and damping capacity of Fe-13Cr-2.5Mo alloy[J]. Mater. Sci. Eng., 2010, B171: 40 | | [2] | Pulino-Sagradi D, Sagradi M, Karimi A, et al.Damping capacity of Fe-Cr-X high-damping alloys and its dependence on magnetic domain structure[J]. Scr. Mater., 1998, 39: 131 | | [3] | Zhou Z C, Wei J N, Han F S.Influences of heat treatment and grain size on the damping capacity of an Fe-Cr-Al alloy[J]. Phys. Status Solidi, 2002, 191A: 89 | | [4] | Wang H, Wang F, Xiao J, et al.Effect of cooling rate on damping capacity of Fe-Cr based ferromagnetic metal alloy[J]. Mater. Sci. Eng., 2016, A650: 382 | | [5] | Hu X F, Li X Y, Zhang B, et al.Influences of additions of Nb, Ti and Cu on damping capacity and corrosion resistance of Fe-13Cr-2.5Mo alloy[J]. Acta Metall. Sin., 2009, 45: 717 | | [5] | (胡小锋, 李秀艳, 张波等. Nb, Ti和Cu对Fe-13Cr-2.5Mo合金阻尼与腐蚀性能的影响[J]. 金属学报, 2009, 45: 717) | | [6] | Wang H, Wang F, Liu H T, et al.Influence of alloy elements (Mo, Nb, Ti) on the strength and damping capacity of Fe-Cr based alloy[J]. Mater. Sci. Eng., 2016, A667: 326 | | [7] | Hu X F, Liu S W, Li X Y, et al.Influence of static stress on damping behavior in Fe-15Cr and Fe-8Al ferromagnetic alloys[J]. Mater. Sci. Eng., 2011, A528: 5491 | | [8] | Karimi A, Giauque P H, Martin J L.Magnetomechanical damping in plasma sprayed iron-chromium based coatings[J]. J. Appl. Phys., 1996, 79: 1670 | | [9] | Azco?tia C, Karimi A.Magnetomechanical damping in Fe-Cr alloys and effect of Al and Mo addition[J]. J. Alloys Compd., 2000, 310: 160 | | [10] | Karimi A, Azcoitia C, Degauque J.Relationships between magnetomechanical damping and magnetic properties of Fe-Cr(Al, Mo) | | [10] | alloys [J]. J. Magn. Magn. Mater., 2000, 215-216: 601 | | [11] | Karimi A, Giauque P H, Martin J L. Magneto-mechanical damping in plasma sprayed Fe-Cr-X alloys [J]. Mater. Sci. Forum, 1995, 179-181: 679 | | [12] | Xu Y G, Chen X G.On relationship between annealing treatment and magnetostriction behavior of Fe-16Cr-2.5Mo damping alloy[J]. J. Alloys Compd., 2014, 582: 364 | | [13] | Lin R R, Liu F, Cao M Z, et al.Influence of annealing and substitution elements on damping capacity and strength of Fe-Cr-Al based alloys[J]. Acta Metall. Sin., 2005, 41: 958 | | [13] | (林仁荣, 刘芳, 曹名洲等. 退火及置换元素对Fe-Cr-Al基合金阻尼性能及强度的影响[J]. 金属学报, 2005, 41: 958) | | [14] | Lin R R, Cao M Z, Yang R. Damping capacity of the Fe-Cr-Al based alloys [J]. Mater. Sci. Forum, 2005, 475-479: 261 | | [15] | Hu X F, Du Y B, Yan D S, et al.Effect of Cu content on microstructure and properties of Fe-16Cr-2.5Mo damping alloy[J]. J. Mater. Sci. Technol., in press | | [16] | Nakashima K, Futamura Y, Tsuchiyama T, et al.Interaction between dislocation and copper particles in Fe-Cu alloys[J]. ISIJ Int., 2002, 42: 1541 | | [17] | Kimura Y, Takaki S.Phase transformation mechanism of Fe-Cu alloys[J]. ISIJ Int., 1997, 37: 290 | | [18] | Zhang Z W.Research development of high strength low alloy (HSLA) steels[J]. Mater. China, 2016, 35: 141 | | [18] | (张中武. 高强度低合金钢(HSLA)的研究进展[J]. 中国材料进展, 2016, 35: 141) | | [19] | Xu Z, Zhao L C.Principle of Solid Phase Transformation of Metals [M]. Beijing: Science Press, 2004: 150 | | [19] | (徐洲, 赵连城. 金属固态相变原理 [M]. 北京: 科学出版社, 2004: 150) | | [20] | Deschamps A, Militzer M, Poole W J.Precipitation kinetics and strengthening of a Fe-0.8wt%Cu alloy[J]. ISIJ Int., 2001, 41: 196 | | [21] | Takaki S, Fujioka M, Aihara S, et al.Effect of copper on tensile properties and grain-refinement of steel and its relation to precipitation behavior[J]. Mater. Trans., 2004, 45: 2239 | | [22] | Xiao J M.Alloy Phase and Phase Transformation [M]. 2nd Ed., Beijing: Metallurgical Industry Press, 2004: 307 | | [22] | (肖纪美. 合金相与相变 [M]. 第2版, 北京: 冶金工业出版社, 2004: 307) | | [23] | Wang W G, Zhou B X.The correlation of damping capacity with grain-boundary precipitates in Fe-Cr-based damping alloys annealed at high temperature[J]. Mater. Sci. Eng., 2004, A366: 45 | | [24] | Smith G W, Birchak J R.Internal stress distribution theory of magnetomechanical hysteresis-an extension to include effects of magnetic field and applied stress[J]. J. Appl. Phys., 1969, 40: 5174 | | [25] | Smith G W, Birchak J R.Effect of internal stress distribution on magnetomechanical damping[J]. J. Appl. Phys., 1968, 39: 2311 | | [26] | Goodman S R, Brenner S S, Low J R.An FIM-atom probe study of the precipitation of copper from lron-1.4 at. pct copper. Part II: Atom probe analyses[J]. Metall. Trans., 1973, 4: 2371 | | [27] | Goodman S R, Brenner S S, Low J R.An FIM-atom probe study of the precipitation of copper from lron-1.4 at. pct copper. Part I: Field-ion microscopy[J]. Metall. Trans., 1973, 4: 2363 | | [28] | Li Z, He Z Q, Jin J J, et al.Development of Aeronautical Ultra Strength Steels [M]. Beijing: National Defense Industry Press, 2012: 45 | | [28] | (李志, 贺自强, 金建军等. 航空超高强度钢的发展 [M]. 北京: 国防工业出版社, 2012: 45) |
|
|