| MgO改性HA对Mg-Zn-Zr/m-HA复合材料组织及性能的影响 |
郑浩然1, 陈民芳1,2( ), 李祯1, 由臣1, 刘德宝1 |
1 天津理工大学材料科学与工程学院 天津 300384 2 天津理工大学天津市光电显示材料与器件重点实验室 天津 300384 |
|
| Effects of MgO Modified HA Nanoparticles on the Microstructure and Properties of Mg-Zn-Zr/m-HA Composites |
Haoran ZHENG1, Minfang CHEN1,2( ), Zhen LI1, Chen YOU1, Debao LIU1 |
1 School of Materials Science and Engineering, Tianjin University of Technology, Tianjin 300384, China 2 Tianjin Key Lab for Photoelectric Materials & Devices, Tianjin University of Technology, Tianjin 300384, China |
引用本文:
郑浩然, 陈民芳, 李祯, 由臣, 刘德宝. MgO改性HA对Mg-Zn-Zr/m-HA复合材料组织及性能的影响[J]. 金属学报, 2017, 53(10): 1364-1376.
Haoran ZHENG,
Minfang CHEN,
Zhen LI,
Chen YOU,
Debao LIU.
Effects of MgO Modified HA Nanoparticles on the Microstructure and Properties of Mg-Zn-Zr/m-HA Composites[J]. Acta Metall Sin, 2017, 53(10): 1364-1376.
| [1] | Witte F, Fischer J, Nellesen J, et al.In vitro and in vivo corrosion measurements of magnesium alloys[J]. Biomaterials, 2006, 27: 1013 | | [2] | Zhao Y C, Huang G S, Wang G G, et al.Influence of grain orientation on the corrosion behavior of rolled AZ31 magnesium alloy[J]. Acta Metall. Sin.(Engl. Lett.), 2015, 28: 1387 | | [3] | Qin F X, Ji C, Dan Z H, et al.Corrosion behavior of MgZnCa bulk amorphous alloys fabricated by spark plasma sintering[J]. Acta Metall. Sin.(Engl. Lett.), 2016, 29: 793 | | [4] | Zheng Y F, Gu X N, Witte F.Biodegradable metals[J]. Mater. Sci. Eng., 2014, R77: 1 | | [5] | Chaubey A K, Jha B B, Mishra B K.Microstructure and mechanical properties of Mg-7.4% Al alloy matrix composites reinforced by nanocrystalline Al-Ca intermetallic particles[J]. Acta Metall. Sin.(Engl. Lett.), 2015, 28: 444 | | [6] | Wang Y, Wang H Y, Xiu K, et al.Fabrication of TiB2 particulate reinforced magnesium matrix composites by two-step processing method[J]. Mater. Lett., 2006, 60: 1533 | | [7] | Soon L L, Zuhailawati H, Suhaina I, et al.Prediction of compressive strength of biodegradable Mg-Zn/HA composite via response surface methodology and its biodegradation[J]. Acta Metall. Sin.(Engl. Lett.), 2016, 29: 464 | | [8] | Witte F, Feyerabend F, Maier P, et al.Biodegradable magnesium-hydroxyapatite metal matrix composites[J]. Biomaterials, 2007, 28: 2163 | | [9] | Gao J H, Guan S K, Ren Z W, et al.Homogeneous corrosion of high pressure torsion treated Mg-Zn-Ca alloy in simulated body fluid[J]. Mater. Lett., 2011, 65: 691 | | [10] | Zhao F Z, Feng X H, Yang Y S.Microstructure and mechanical properties of CNT-reinforced AZ91D composites fabricated by ultrasonic processing[J]. Acta Metall. Sin.(Engl. Lett.), 2016, 29: 652 | | [11] | Lei T, Tang W, Cai S H, et al.On the corrosion behaviour of newly developed biodegradable Mg-based metal matrix composites produced by in situ reaction[J]. Corros. Sci., 2012, 54: 270 | | [12] | Ratna Sunil B, Ganapathy C, Sampath Kumar T S, et al. Processing and mechanical behavior of lamellar structured degradable magnesium-hydroxyapatite implants[J]. J. Mech. Behav. Biomed. Mater., 2014, 40: 178 | | [13] | Zhou D S, Qiu F, Wang H Y, et al.Manufacture of nano-sized particle-reinforced metal matrix composites: A review[J]. Acta Metall. Sin.(Engl. Lett.), 2014, 27: 798 | | [14] | Gu X N, Wang X, Li N, et al.Microstructure and characteristics of the metal-ceramic composite (MgCa-HA/TCP) fabricated by liquid metal infiltration[J]. J. Biomed. Mater. Res., 2011, 99B: 127 | | [15] | Ye X Y, Chen M F, Yang M, et al.In vitro corrosion resistance and cytocompatibility of nano-hydroxyapatite reinforced Mg-Zn-Zr composites[J]. J. Mater. Sci. Mater. Med., 2010, 21: 1321 | | [16] | Liu D B, Zuo Y B, Meng W Y, et al.Fabrication of biodegradable nano-sized β-TCP/Mg composite by a novel melt shearing technology[J]. Mater. Sci. Eng., 2012, C32: 1253 | | [17] | Li Z, Chen M F, Li W, et al.The synergistic effect of trace Sr and Zr on the microstructure and properties of a biodegradable Mg-Zn-Zr-Sr alloy[J]. J. Alloys Compd., 2017, 702: 290 | | [18] | Li Z, Sun S Z, Chen M F, et al.In vitro and in vivo corrosion, mechanical properties and biocompatibility evaluation of MgF2-coated Mg-Zn-Zr alloy as cancellous screws[J]. Mater. Sci. Eng., 2017, C75: 1268 | | [19] | He S Y, Sun Y, Chen M F, et al.Microstructure and properties of biodegradable β-TCP reinforced Mg-Zn-Zr composites[J]. Trans. Nonferrous Met. Soc. China, 2011, 21: 814 | | [20] | Jin X Y, Zhuang J Z, Zhi Z, et al.Hydrothermal synthesis of hydroxyapatite nanorods in the presence of sodium citrate and its aqueous colloidal stability evaluation in neutral pH[J]. J. Colloid Interface Sci., 2015, 443: 125 | | [21] | Huang Y, Liu D B, Anguilano L, et al.Fabrication and characterization of a biodegradable Mg-2Zn-0.5Ca/1β-TCP composite[J]. Mater. Sci. Eng., 2015, C54: 120 | | [22] | Humphreys F J, Hatherly M.Recrystallization and Related Annealing Phenomena[M]. 2nd Ed., Oxford: Elsevier, 2004: 20 | | [23] | Song G L.Corrosion and Protection of Magnesium Alloys [M]. Beijing: Chemical Industry Press, 2006: 94(宋光铃. 镁合金腐蚀与防护 [M]. 北京: 化学工业出版社, 2006: 94) | | [24] | Bakhsheshi-Rad H R, Abdul-Kadir M R, Idris M H, et al. Relationship between the corrosion behavior and the thermal characteristics and microstructure of Mg-0.5Ca-xZn alloys[J]. Corros. Sci., 2012, 64: 184 | | [25] | Argade G R, Kandasamy K, Panigrahi S K, et al.Corrosion behavior of a friction stir processed rare-earth added magnesium alloy[J]. Corros. Sci., 2012, 58: 321 | | [26] | Shi Z M, Atrens A.An innovative specimen configuration for the study of Mg corrosion[J]. Corros. Sci., 2011, 53: 226 | | [27] | King A D, Birbilis N, Scully J R.Accurate electrochemical measurement of magnesium corrosion rates; a combined impedance, mass-loss and hydrogen collection study[J]. Electrochim. Acta, 2014, 121: 394 | | [28] | Wang Y, Fan Z, Zhou X, et al.Characterisation of magnesium oxide and its interface with α-Mg in Mg-Al-based alloys[J]. Phil. Mag. Lett., 2011, 91: 516 | | [29] | Splinter S J, Rofagha R, McIntyre N S, et al. XPS characterization of the corrosion films formed on nanocrystalline Ni-P alloys in sulphuric acid[J]. Surf. Interface Anal., 1996, 24: 181 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|