| Sn的加入对MnFe(P, Si)合金显微组织和磁性的影响 |
耿遥祥1( ),特古斯2,汪海斌1,董闯3,王宇鑫1 |
1 江苏科技大学材料科学与工程学院 镇江 212003 2 内蒙古师范大学内蒙古自治区功能材料物理与化学重点实验室 呼和浩特 010022 3 大连理工大学三束材料改性教育部重点实验室 大连 116024 |
|
| Effect of Sn Addition on Microstructure and Magnetism of MnFe(P, Si) Alloy |
Yaoxiang GENG1( ),Ojied TEGUS2,Haibin WANG1,Chuang DONG3,Yuxin WANG1 |
1 School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China 2 Inner Mongolia Key Laboratory for Physics and Chemistry of Functional Materials, Inner Mongolia Normal University, Hohhot 010022, China 3 Key Lab of Materials Modification by Laser, Ion and Electron Beams, Ministry of Education, Dalian University of Technology, Dalian 116024, China |
引用本文:
耿遥祥,特古斯,汪海斌,董闯,王宇鑫. Sn的加入对MnFe(P, Si)合金显微组织和磁性的影响[J]. 金属学报, 2017, 53(1): 77-82.
Yaoxiang GENG,
Ojied TEGUS,
Haibin WANG,
Chuang DONG,
Yuxin WANG.
Effect of Sn Addition on Microstructure and Magnetism of MnFe(P, Si) Alloy[J]. Acta Metall Sin, 2017, 53(1): 77-82.
| [1] | Chen P, Wang D H, Du Y W.Progress on working material of magnetic cooling[J]. Prog. Phys., 1999, 19: 371 | | [1] | (陈鹏, 王敦辉, 都有为. 磁制冷工质材料的研究进展[J]. 物理学进展, 1999, 19: 371) | | [2] | Brück E.Developments in magnetocaloric refrigeration[J]. J. Phys., 2005, 38D: R381 | | [3] | Brück E, Tegus O, Li X W, et al.Magnetic refrigeration-towards room-temperature applications[J]. Physica, 2003, 327B: 431 | | [4] | Bednarz G, Geldart D J W, White M A. Heat capacity of gadolinium near the Curie temperature[J]. Phys. Rev., 1993, 47B: 14247 | | [5] | Li J W, Huo J T, Law J Y, et al.Magnetocaloric effect in heavy rare-earth elements doped Fe-based bulk metallic glasses with tunable Curie temperature[J]. J. Appl. Phys., 2014, 116: 063902 | | [6] | Pecharsky V K, Gschneidner K A Jr. Giant magnetocaloric effect in Gd5(Si2Ge2)[J]. Phys. Rev. Lett., 1997, 78: 4494 | | [7] | Hu F X, Shen B G, Sun J R, et al.Influence of negative lattice expansion and metamagnetic transition on magnetic entropy change in the compound LaFe11.4Si1.6[J]. Appl. Phys. Lett., 2001, 78: 3675 | | [8] | Wada H, Tanabe Y.Giant magnetocaloric effect of MnAs1-xSbx[J]. Appl. Phys. Lett., 2001, 79: 3302 | | [9] | Tegus O, Brück E, Buschow K H J, et al. Transition-metal-based magnetic refrigerants for room-temperature applications[J]. Nature, 2002, 415: 150 | | [10] | Trung N T, Zhang L, Caron L, et al.Giant magnetocaloric effects by tailoring the phase transitions[J]. Appl. Phys. Lett., 2010, 96: 172504 | | [11] | Tegus O, Fuquan B, Dagula W, et al.Magnetic-entropy change in Mn1.1Fe0.9P0.7As0.3-xGex[J]. J. Alloys Compd., 2005, 396: 6 | | [12] | Dagula W, Tegus O, Li X W, et al. Magnetic properties and magnetic-entropy change of MnFeP0.5As0.5–xSix(x=0~0.3) compounds [J]. J. Appl. Phys., 2006, 99: 08Q105 | | [13] | Thanh D T C, Brück E, Tegus O, et al. Magnetocaloric effect in MnFe(P, Si, Ge) compounds [J]. J. Appl. Phys., 2006, 99: 08Q107 | | [14] | Song L, Wang G F, Ou Z Q, et al.Magnetic properties and magnetocaloric effect of MnFeP0.5Ge0.5-xSix compounds[J]. J. Alloys Compd., 2009, 474: 388 | | [15] | Trung N T, Ou Z Q, Gortenmulder T J, et al.Tunable thermal hysteresis in MnFe(P, Ge) compounds[J]. Appl. Phys. Lett., 2009, 94: 102513 | | [16] | Dung N H, Zhang L, Ou Z Q, et al.From first-order magneto-elastic to magneto-structural transition in (Mn, Fe)1.95P0.50Si0.50 compounds[J]. Appl. Phys. Lett., 2011, 99: 092511 | | [17] | Geng Y X, Tegus O, Bi L G.Magnetocaloric effects in Mn1.35Fe0.65P1-xSix compounds[J] Chin. Phys., 2012, 21B: 037504 | | [18] | Tegus O, Bao L H, Song L.Phase transitions and magnetocaloric effects in intermetallic compounds MnFeX (X=P, As, Si, Ge)[J]. Chin. Phys., 2013, 22B: 037506 | | [19] | Dung N H, Ou Z Q, Caron L, et al.Mixed magnetism for refrigeration and energy conversion[J]. Adv. Energy Mater., 2011, 1: 1215 | | [20] | Yibole H, Guillou F, Zhang L, et al.Direct measurement of the magnetocaloric effect in MnFe (P, X) (X = As, Ge, Si) materials[J]. J. Phys., 2014, 47D: 075002 | | [21] | Geng Y X, Tegus O.Experimental study on the magnetocaloric effect in Mn1.2Fe0.8-xCoxP0.48Si0.52 compounds[J]. J. Magn. Mater. Dev., 2011, 42(5): 17 | | [21] | (耿遥祥, 特古斯. Mn1.2Fe0.8-xCoxP0.48Si0.52化合物磁热效应研究[J]. 磁性材料及器件, 2011, 42(5): 17) | | [22] | Geng Y X, Tegus O, Bi L G, et al.Influence of different preparation techniques and raw materials on magnetocaloric effect in Mn1.2Fe0.8P0.48Si0.52 compound[J]. J. Chin. Rare Earth Soc., 2011, 29: 266 | | [22] | (耿遥祥, 特古斯, 毕力格等. 不同工艺和原料对Mn1.2Fe0.8P0.48Si0.52化合物磁热效应的影响[J]. 中国稀土学报, 2011, 29: 266) | | [23] | Hashimoto T, Numasawa T, Shino M, et al.Magnetic refrigeration in the temperature range from 10 K to room temperature: The ferromagnetic refrigerants[J]. Cryogenics, 1981, 21: 647 | | [24] | Chirkova A, Skokov K P, Schultz L, et al.Giant adiabatic temperature change in FeRh alloys evidenced by direct measurements under cyclic conditions[J]. Acta Mater., 2016, 106: 15 | | [25] | Duan T F, Ren W J, Liu W, et al.Magnetization processes and transitions between two antiferromagnetic spin configurations in single-crystalline MnSn2[J]. Physica, 2016, 495B: 94 | | [26] | Huliyageqi B, Geng Y X, Li Y J, et al.A significant reduction of hysteresis in MnFe(P, Si) compounds[J]. J. Korean Phys. Soc., 2013, 63: 525 | | [27] | Zheng Z G, Tan Z C, Yu H Y, et al.Structural, magnetic properties and magnetocaloric effect of Mn1.2Fe0.8P1-xSixB0.03 compounds[J]. Mater. Res. Bull., 2016, 77: 29 |
|
|