| TiN析出相对中碳Cr-Mo耐磨钢凝固组织的影响* |
郭文营1,2,胡小强2( ),马晓平2,李殿中2 |
1 中国科学技术大学化学与材料科学学院, 合肥 230022。 2 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016。 |
|
| EFFECT OF TiN PRECIPITATES ON SOLIDIFICATION MICROSTRUCTURE OF MEDIUM CARBON Cr-Mo WEAR RESISTANT STEEL |
Wenying GUO1,2,Xiaoqiang HU2( ),Xiaoping MA2,Dianzhong LI2 |
1 School of Chemistry and Materials Science, University of Science and Technology of China, Hefei 230022, China 2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
郭文营,胡小强,马晓平,李殿中. TiN析出相对中碳Cr-Mo耐磨钢凝固组织的影响*[J]. 金属学报, 2016, 52(7): 769-777.
Wenying GUO,
Xiaoqiang HU,
Xiaoping MA,
Dianzhong LI.
EFFECT OF TiN PRECIPITATES ON SOLIDIFICATION MICROSTRUCTURE OF MEDIUM CARBON Cr-Mo WEAR RESISTANT STEEL[J]. Acta Metall Sin, 2016, 52(7): 769-777.
| [1] | Deng X T, Wang Z D, Han Y, Zhao H, Wang G D.J Iron Steel Res Int, 2014; 21(1): 98 | | [2] | Gahr K H Z.Tribol Int, 1998; 31: 587 | | [3] | Melloy G F, Summon P R, Podgursky P P.Mater Trans, 1973; 4: 2279 | | [4] | Kapadia B M, Brown R M, Murphy W J.Trans Met Soc AIME, 1968; 242: 1689 | | [5] | Shen Y L, Hansen S S.Metall Mater Trans, 1997; 28A: 2027 | | [6] | Wang C, Gao H Y, Dai Y B, Ruan X M, Wang J, Sun B D.Metall Mater Trans, 2010; 41A: 1616 | | [7] | Bramfitt B L.Metall Trans, 1970; 1: 1987 | | [8] | Shi C X, Cheng G G, Li Z J, Zhao P.J Iron Steel Res Int, 2008; 15(3): 57 | | [9] | Poole W, Mitchell A, Weinberg F.High Temp Mater Proc, 1997; 16: 173 | | [10] | Pan N, Song B, Zhai Q J, Wen B.J Univ Sci Technol Beijing, 2010; 32: 179 | | [10] | (潘宁, 宋波, 翟启杰, 文彬. 北京科技大学学报, 2010; 32: 179) | | [11] | Sasaki M, Ohsasa K, Kudoh M, Matsuura K.ISIJ Int, 2008; 48: 340 | | [12] | Ohno M, Matsuura K.ISIJ Int, 2008; 48: 1373 | | [13] | Sasaki M, Matsuura K, Ohsasa K, Ohno M.ISIJ Int, 2009; 49: 1367 | | [14] | Sasaki M, Matsuura K, Ohsasa K, Ohno M.ISIJ Int, 2009; 49: 1362 | | [15] | Fu J, Zhu J, Di L, Tong F S, Liu D L, Wang Y L.Acta Metall Sin, 2000; 36: 801 | | [15] | (傅杰, 朱剑, 迪林, 佟福生, 柳得橹, 王元立. 金属学报, 2000; 36: 801) | | [16] | Yang X, Cheng G G, Wang M L, Li Y L, Wang Y G, Zhao P. J Univ Sci Technol Beijing (Engl Lett), 2003; 10: 24 | | [17] | Nagata M T, Speer J G, Matlock D K.Metall Mater Trans, 2002; 33A: 3099 | | [18] | Cheng G G, Zhu X X, Peng Y F, Wang Y G, Zhao P.J Univ Sci Technol Beijing, 2002; 24: 273 | | [18] | (成国光, 朱晓霞, 彭岩峰, 王玉钢, 赵沛. 北京科技大学学报, 2002; 24: 273) | | [19] | Shi X F, Cheng G G.Steel Making, 2008; 24(4): 36 | | [19] | (施晓芳, 成国光. 炼钢, 2008; 24(4): 36) | | [20] | Pagounis E, Lindroos V K.Mater Sci Eng, 1998; A246: 221 | | [21] | Yan W, Shan Y Y, Yang K.Metall Mater Trans, 2006; 37A: 2147 | | [22] | Du J, Strangwood M, Davis C L. J Mater Sci Technol, 2012; 28: 878 | | [23] | Yong Q L.Secondary Phases in Steel. Beijing: Metallurgical Industry Press, 2006: 28 | | [23] | (雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 28) | | [24] | Cui Z Q, Tan Y C.Metallographic and Thermal Treatment. 2nd Ed., Beijing: China Machine Press, 2007: 37 | | [24] | (崔忠圻, 覃耀春. 金属学与热处理. 第二版, 北京: 机械工业出版社, 2007: 37) | | [25] | Kurz W, Fisher D J.Fundamentals of Solidification. 4th Ed., Aedermannsdorf: Trans Tech Publications Ltd, 1998: 85 | | [26] | Han Q Y, Hu H Q. J Univ Sci Technol Beijing, 1985; (1): 1 | | [26] | (韩青有, 胡汉起. 北京科技大学学报, 1985; (1): 1) | | [27] | Pierer R, Bernhard C. J Mater Sci, 2008; 43: 6938 | | [28] | Paliwal M, Kang D H, Essadiqi E, Jung I H.Adv Mater Res, 2012; 409: 362 |
|
|