| Fe-C-Cu粉末锻造汽车发动机连杆的组织与力学性能* |
柏琳娜1,刘福平1,2,王邃1,江峰1( ),孙军1,陈良斌1,王丰元2 |
1 西安交通大学金属材料强度国家重点实验室, 西安 710049 2 青岛理工大学汽车与交通学院, 青岛 266520 |
|
| MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Fe-C-Cu POWDER-FORGED CONNECTING ROD |
Linna BAI1,Fuping LIU1,2,Sui WANG1,Feng JIANG1( ),Jun SUN1,Liangbin CHEN1,WANG,Fengyuan2 |
1 State Key Laboratory for Mechanical Behavior of Materials, Xi'an Jiaotong University, Xi'an 710049, China 2 School of Automobile and Transportation, Qingdao Technological University, Qingdao 266520, China |
引用本文:
柏琳娜,刘福平,王邃,江峰,孙军,陈良斌,王丰元. Fe-C-Cu粉末锻造汽车发动机连杆的组织与力学性能*[J]. 金属学报, 2016, 52(1): 41-50.
Linna BAI,
Fuping LIU,
Sui WANG,
Feng JIANG,
Jun SUN,
Liangbin CHEN,
,
Fengyuan.
MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Fe-C-Cu POWDER-FORGED CONNECTING ROD[J]. Acta Metall Sin, 2016, 52(1): 41-50.
| [1] | Capus J. Met Powder Rep, 2014; 69: 31 | | [2] | Ilia E, Tutton K O, Neill M. Met Powder Rep, 2005; 60: 38 | | [3] | Guo B, Ge C C, Zhang S C, Zhang Y. Powder Metall Ind, 2011; 21(3): 45 | | [3] | (郭 彪, 葛昌纯, 张随财, 张 宇. 粉末冶金工业, 2011; 21(3): 45) | | [4] | Afzal A. Master Thesis, University of Toledo, USA, 2004 | | [5] | Dinu D, Lapp M T. SAE Tech Paper, 2006; 01: 0894 | | [6] | Hanke W, Buschbeck R, Letourneau S, Sinclair D, Skiadas A, Urabe M, Takiguchi M. SAE Tech Paper, 2009; 01: 1958 | | [7] | Bao X P, Tan X Y, Liu S D, Le P. Light Vehicles, 2009; 236: 20 | | [7] | (包雪鹏, 谭晓园, 刘善德, 乐 萍. 轻型汽车技术, 2009; 236: 20) | | [8] | Ilia E, Lanni G, Xin J, Yan R, Zung E. Trans Csice, 2008; 26: 463 | | [8] | (Ilia E, Lanni G, 辛 军, Yan R, Zung E. 内燃机学报, 2008; 26: 463) | | [9] | Williams B. Met Powder Rep, 2004; 59: 14 | | [10] | Guo B, Ge C C, Yan Y N, Zhang S C, Yu B J. Mater Rev, 2012; 26(7)B: 141 | | [10] | (郭 彪, 葛昌纯, 颜永年, 张随财, 余本军. 材料导报, 2012; 26(7)B: 141) | | [11] | Guo B, Ge C C, Yan Y N, Zhang S C, Yu B J. Hot Work Technol, 2012; 41(18): 64 | | [11] | (郭 彪, 葛昌纯, 颜永年, 张随财, 余本军. 热加工工艺, 2012; 41(18): 64) | | [12] | Wang J L, Chen Z, Chen H. J Changchun Univ Technol, 2005; 26(1): 61 | | [12] | (王佳玲, 陈 卓, 陈 华. 长春工业大学学报, 2005; 26(1): 61) | | [13] | Wang J X, Guo C M, Zhu Z Y, Yin Z M, Zhou K Z, Li Z Y. Mater Sci Eng Powder Metall, 2006; 11(1): 19 | | [13] | (王继新, 郭昌明, 朱志远, 尹志民, 周科朝, 李智友. 粉末冶金材料科学与工程, 2006; 11(1): 19) | | [14] | Zhou M Z, Li P, Xue K M. J Plast Eng, 2005; 12(6): 11 | | [14] | (周明智, 李 萍, 薛克敏. 塑性工程学报, 2005; 12(6): 11) | | [15] | Tu T S, Lin D W. Met Forming Technol, 2001; 19(2): 4 | | [15] | (屠挺生, 林大为. 金属成形工艺, 2001; 19(2): 4) | | [16] | Zhao W B. PhD Dissertation, South China University of Technology, Guangzhou, 2005 | | [16] | (赵伟斌. 华南理工大学博士学位论文, 广州, 2005) | | [17] | Wang C L. In: PM Branch of SCS Ed., The 20th Anniversary Corpus of PM Branch of SCS, Beijing: CMPMA, 2010: 104 | | [17] | (王崇琳. 中国钢结构协会粉末冶金分会 编. 粉末冶金产业技术创新战略联盟论坛暨中国钢协机协粉末冶金协会二十周年纪念文集, 北京: 中国机械通用零部件工业协会粉末冶金专业协会, 2010: 104) | | [18] | Guo B. PhD Dissertation, Southwest Jiaotong University, Chengdu, 2008 | | [18] | (郭 彪. 西南交通大学博士学位论文, 成都, 2008) | | [19] | Li P. Auto Technol Mater, 2010; (1): 42 | | [19] | (李 鹏. 汽车工艺与材料, 2010; (1): 42) | | [20] | Han F L. Adv Mater Ind, 2005; (11): 55 | | [20] | (韩凤麟. 新材料产业, 2005; (11): 55) | | [21] | Hong S Z. J Netshape Forming Eng, 2011; (3): 47 | | [21] | (洪慎章. 精密成形工程, 2011; (3): 47) | | [22] | Wang Y K, Peng M G. Met Mater Metall Eng, 2007; 35(5): 57 | | [22] | (王云坤, 彭茂公. 金属材料与冶金工程, 2007; 35(5): 57) | | [23] | Han F L. Powder Metall Ind, 2011; 21(4): 1 | | [23] | (韩凤麟. 粉末冶金工业, 2011; 21(4): 1) | | [24] | Engstrom U. Int J Powder Metall, 2003; 39: 29 | | [25] | Han F L. Powder Metall Ind, 2014; 24(4): 1 | | [25] | (韩凤麟. 粉末冶金工业, 2014; 24(4): 1) | | [26] | Haerian A H, Khaki J V, Mashhadi H A. IJE Trans, 2004; 6B: 81 | | [27] | Tang R Z,Tian R Z. Binary Alloy Phase Diagrams and Crystal Structure of Intermediate Phase. Changsha: Central South University Press, 2009: 126 | | [27] | (唐仁政,田荣璋. 二元合金相图及中间相晶体结构. 长沙: 中南大学出版社, 2009: 126) | | [28] | Jang X D, Liu Z L, Zou D H, Liu B L. Mater Mech Eng, 2012; 36(4): 46 | | [28] | (蒋晓冬, 刘子利, 邹德华, 刘伯路. 机械工程材料, 2012; 36(4): 46) |
|
|