Zr含量对Nb-Ti-Si基超高温合金组织及抗氧化性能的影响 |
曾宇翔1,郭喜平1(),乔彦强1,聂仲毅2 |
2 中钢集团西安重机有限公司, 西安 710077 |
|
EFFECT OF Zr ADDITION ON MICROSTRUCTURE AND OXIDATION RESISTANCE OF Nb-Ti-Si BASE ULTRAHIGH-TEMPERATURE ALLOYS |
Yuxiang ZENG1,Xiping GUO1(),Yanqiang QIAO1,Zhongyi NIE2 |
1 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi′an 710072 2 Sinosteel Xi′an Heavy Machinery Co. Ltd., Xi′an 710077 |
引用本文:
曾宇翔,郭喜平,乔彦强,聂仲毅. Zr含量对Nb-Ti-Si基超高温合金组织及抗氧化性能的影响[J]. 金属学报, 2015, 51(9): 1049-1058.
Yuxiang ZENG,
Xiping GUO,
Yanqiang QIAO,
Zhongyi NIE.
EFFECT OF Zr ADDITION ON MICROSTRUCTURE AND OXIDATION RESISTANCE OF Nb-Ti-Si BASE ULTRAHIGH-TEMPERATURE ALLOYS[J]. Acta Metall Sin, 2015, 51(9): 1049-1058.
[1] | Bewlay B P, Jackson M R, Lipsitt H A. Metall Mater Trans, 1996; 27A: 3801 | [2] | Grammenos I, Tsakiropoulos P. Intermetallics, 2010; 18: 242 | [3] | Bewlay B P, Jackson M R, Zhao J C, Subramanian P R. Metall Mater Trans, 2003; 34A: 2043 | [4] | Wu C L, Zhou L Z, Guo J T. Acta Metall Sin, 2006; 42: 1061 (伍春兰, 周兰章, 郭建亭. 金属学报, 2006; 42: 1061) | [5] | Kang Y W, Qu S Y, Song J X, Han Y F. Acta Metall Sin, 2008; 44: 593 (康永旺, 曲士昱, 宋尽霞, 韩雅芳. 金属学报, 2008; 44: 593) | [6] | Jia L N, Gao M, Ge J R, Zheng L J, Sha J B, Zhang H. Acta Metall Sin, 2011; 47: 88 (贾丽娜, 高 明, 盖京茹, 郑立静, 沙江波, 张 虎. 金属学报, 2011; 47: 88) | [7] | Wang J, Guo X P, Guo J M. Chin J Aeronaut, 2009; 22: 544 | [8] | Zhang S, Guo X P. Intermetallics, 2015; 57: 83 | [9] | Xiong B W, Cai C C, Wan H, Zheng Y H. J Alloys Compd, 2009; 486: 330 | [10] | Guo J M, Guo X P, Song S G. Acta Metall Sin, 2008; 44: 574 (郭金明, 郭喜平, 宋曙光. 金属学报, 2008; 44: 574) | [11] | Zelenitsas K, Tsakiropoulos P. Mater Sci Eng, 2006; A416: 269 | [12] | Geng J, Tsakiropoulos P, Shao G S. Mater Sci Eng, 2006; A441: 26 | [13] | Li Z F, Tsakiropoulos P. Intermetallics, 2012; 26: 18 | [14] | Wang L G, Jia L N, Cui R J, Zheng L J, Zhang H. Chin J Aeronaut, 2012; 25: 292 | [15] | Grammenos I, Tsakiropoulos P. Intermetallics, 2011; 19: 1612 | [16] | Geng J, Tsakiropoulos P. Intermetallics, 2007; 15: 382 | [17] | Behrani V, Thom A J, Kramer M J, Akinc M. Intermetallics, 2006; 14: 24 | [18] | Vellios N, Tsakiropoulos P. Intermetallics, 2010; 18: 1729 | [19] | Vellios N, Tsakiropoulos P. Intermetallics, 2007; 15: 1518 | [20] | Yuan W H, Liang Z Y. Mater Des, 2011; 32: 4195 | [21] | Mousa M, Wanderka N, Timpel M, Singh S, Krüger M, Heilmaier M, Banhart J. Ultramicroscopy, 2011; 111: 706 | [22] | Gorr B, Wang L, Burk S, Azim M, Majumdar S, Christ H J, Mukherji D, R?sler J, Schliephake D, Heilmaier M. Intermetallics, 2014; 48: 34 | [23] | Yu Q H, Zhou C G, Zhang H Y, Zhao F. J Eur Ceram Soc, 2010; 30: 889 | [24] | Li X, Guo X P, Qiao Y Q. Oxid Met, 2015; 83: 253 | [25] | Li X, Guo X P. Acta Metall Sin, 2012; 48: 1394 (李 轩, 郭喜平. 金属学报, 2012; 48: 1394) | [26] | Tian Y X, Guo J T, Sheng L Y, Cheng G M, Zhou L Z, He L L, Ye H Q. Intermetallics, 2008; 16: 807 | [27] | Li X F, Guo X P. Acta Metall Sin, 2013; 49: 853 (李小飞, 郭喜平. 金属学报, 2013; 49: 853) | [28] | Liu A Q, Sun L, Li S S, Han Y F. J Rare Earth, 2007; 25: 474 | [29] | Lee D B, Woo S W. Intermetallics, 2005; 13: 169 |
|
|